IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 181 documents. Displaying 25 entries per page.


Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Effects of alkali treatment on some mechanical and chemical properties of creosote treated oaks
1991 - IRG/WP 2366
To date, there is a lack of information on the effects of chemical treatment on the performance of creosote preservative treated oak sleepers. This factorial experiment was designed to analyze three main effects: species (Quercus alba and Quercus rubra) creosote treatment (treated and untreated), and alkali (NaOH) soaking (0, 1, and 10 percent). The modulus of elasticity (MOE) and fiber stress at ...
P Chow, A J Reinschmidt, E J Barenberg, L C Chang


Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


The effect of primary blue-staining fungi on the strength properties of Scots pine sapwood
2004 - IRG/WP 04-10515
The fungi action may have influence on wood properties especially Basidiomycotina fungi causing wood decay. The investigation of influence of fungi causing mainly wood discoloration and disfigurement on wood properties is still in development process. There were determined the differences between the bending strength, the compression along the grains and impact strength of control and blue stained...
A Fojutowski


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


The use of spruce for transmission poles
1973 - IRG/WP 326
A series of preservative treatments with creosote using Lowry and Rueping schedules was undertaken. From these treatments the most suitable impregnation conditions for water stored Sitka spruce (Picea sitchensis) and Norway spruce (Picea abies) transmission poles were determined. Preservative distribution and permeability values for poles of both species were used to decide the optimum season and ...
J A Dunleavy, D J Balfe, J P Prendergast


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Evaluation of a utility pole inspection procedure
1996 - IRG/WP 96-20084
Methods were developed and are currently being utilized to appraise residual strength of utility poles based on visual assessment of increment cores. Strength tests, mycological descriptions and anatomical analyses were performed on eight utility poles taken out of service and one new (never in service) pole. Samples were obtained from increment cores removed from 6 levels in the pole: 2 feet, gro...
S E Anagnost, C J K Wang


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Preservative treatment of common timbers and bamboos of Bangladesh for rural electrification infrastructure
1998 - IRG/WP 98-40104
Researches revealed new treatment grades, treatment groups, grading groups, natural durability grades, strength groups and a new preservative combination for remedial treatment and sterilization of most common timbers and bamboos of Bangladesh. The obtained findings are applicable for equivalent timber species having equivalent climatic condition. Sapwoods are always perishable and timbers with wh...
A K Lahiry


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


Reduction of preservatives leaching from wood by the application of animal proteins
2005 - IRG/WP 05-30387
The investigations consisted in the estimation of the effectiveness of protein borates and protein propionates in wood preservation against Coniophora puteana. The estimation was made on the basis of mass losses caused by the test fungus action against treated wood which was subjected to leaching with water. The investigations were performed for Scots pine wood (Pinus sylvestris L.) treated with p...
B Mazela, I Ratajczak, M Bartkowiak


Applicability of supercritical carbon dioxide to the preservative treatment of wood-based composites
2001 - IRG/WP 01-40199
Treatability of five structural-use wood-based composites (medium density fiberboard, hardwood plywood, softwood plywood, particleboard and oriented strand board) was evaluated when supercritical (SC) carbon dioxide (CO2) was used as a carrier solvent. Treatments were conducted at three temperature 32 levels (25, 35 and 45°C) and two pressure levels [80 kgf/cm2 (7,845 kPa) and 120 kgf/cm2 (11,768...
M Muin, A Adachi, K Tsunoda


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Dutch national environmental policy strategy (NMP): Implications throughout the life cycle of treated timber and for the Dutch preservation industry
1993 - IRG/WP 93-50001-31
All overview of relevant environmental legislation and instruments for control is given for each stage of the life cycle of treated timber. Recent policy in the Netherlands has been focused around the "National Environmental Policy Strategy", in which a general policy with regard to reduction of pollution to the air, soil and water is described. The principle is one of an "Integrated Chain of Cont...
P Esser, D A Lewis, A J Pendlebury


Previous Page | Next Page