The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Inspection method of surface checking of Sugi posts
2003 - IRG/WP 03-20272
In order to establish the method for evaluating the checking of Sugi posts, checks on exposed posts were examined. Checks on Sugi posts exposed for 18 months were superficially inspected, that is, the length, width, and depth of the checks were measured from the outside with a ruler and 0.1 mm thick feeler gauge. Then, each post was cut into cross sections of the 30 mm width, and the check depth w...
H Kurisaki, H Nakatani, K Mizumoto


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


The efficacy of polyurethane coatings on wood samples exposed in the marine environment. Final Report -10 Year Assessment
1996 - IRG/WP 96-10170
The results of an IRG collaborative marine trial to investigate the long-term permanence and efficacy of polyurethane coatings against marine borers are reported. PU-coated wood samples were exposed at a range of sites from tropical to cold temperate locations. The marine borer species present at the sites included teredinids, pholads, limnoriids and sphaeromatids so that each site offered its own...
R A Eaton


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Evaluation of Barrier Wrap Systems after 71 Months of Exposure
2013 - IRG/WP 13-40631
A 71 month study of the performance of booted samples in ground contact was conducted in AWPA hazard zone 4. Data indicated that excellent performance of wrapped systems, even over untreated wood, could be obtained. Instances of decay colonization or termite attack could all be attributed to some breaking of the integrity of the barrier system. Good performance for treatment below ground contact...
H M Barnes, M G Sanders, G B Lindsey, C McIntyre


How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort


Influence of a dipping preservative treatment on the performance of wood finished with waterborne coatings
1998 - IRG/WP 98-40121
Within a larger European research project on the performance of joinery finished with waterborne coatings, the influence of a water based dipping preservative treatment was studied in several ways. Six different waterborne coatings were tested with and without a preservative underneath the coating. The performance was tested on pine sapwood and spruce panels in a 2-year outdoor weathering trial on...
M De Meijer, J Creemers, W Cobben, P Ahola


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


Exploring the potential for plasma-assisted coating at atmospheric pressure for wood protection
2023 - IRG/WP 23-40982
J Profili, G Laroche


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


Enzyme systems of bacterial isolates from ponded logs - Potentials of pectin and/or starch degradation
2000 - IRG/WP 00-10378
This paper deals with the degradation potentials of wood constituents by the bacterial isolates from ponded logs. The potentials to degrade pectin as a constituent of pit-tori as well as starch existing in ray parenchyma cells in the areas of sap- and transition wood with the isolates were examined. The pectinase activity was investigated by means of the degradation degree of a carrot strip used a...
S Doi, S Ohta


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


Improving the weather resistance of glue-laminated jarrah and karri
1994 - IRG/WP 94-40017
Surface modification and dimensional stabilisation significantly increased the dry and wet shear strength of karri and jarrah lap-shear specimens (laminates) bonded with resorcinol formaldehyde. The combination of surface modification (sanding/sodium hydroxide treatment), and furfurylation produced the highest dry and wet shear strengths. Acetylated laminates had the lowest dry bond strength, but ...
J Balfas, P D Evans


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 2nd Interim Report
1990 - IRG/WP 4161
The results of a collaborative international test to evaluate the performance of elastomeric polyurethane coatings of wooden test samples exposed in seawater at 13 sites around the world are reported. The samples have been exposed at sites with known infestations by molluscan and/or crustacean wood borers. Performance data for up to 4 years exposure at some sites is presented providing information...
R A Eaton


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Evaluating the performance of preservative/water repellent emulsion systems
1997 - IRG/WP 97-20127
Water repellent emulsions are being combined with wood preservatives to improve the weathering properties of treated wood in service. Unfortunately, few standard procedures are available to objectively compare the performance of these systems and as a result quality issues are almost completely neglected. The value of swellometer tests, water immersion tests and accelerated weathering regimes in t...
K J Archer, F Cui


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


The environment and the timber preservation in the Benelux countries
1990 - IRG/WP 3580
The environment has become a major issue in all industries. To focus on the timber preservation industry an analysis is made of the production chain. Suggestions are made for diminishing or excluding emissions of agents of pollution. After a review of the legislation in Holland, some important statements are made on the production process, the products involved and the waste materials. Finally raw...
C De Mey, R Leegwater