Your search resulted in 1074 documents. Displaying 25 entries per page.
Simulation test of subchronic inhalation toxicity of TBTO vapours in the air
1987 - IRG/WP 3454
The test was carried out in a wainscotted room of a normal size. Wooden panelling had been treated with one coat of basic preserving agent and, after the installation, with 2 coats of stain. Laboratory animals (rats) were kept in this room for 90 days. For the same period a control group of test animals was kept in a room of equal size where there was no panelling. During the test, concentration o...
V Skubic, S Kobal, J Stupar, R Ajlec, J Korošin, G R Pecenko
A report on the development of "Technical Recommendations Document for the Canadian wood preservation and protection facilities"
1987 - IRG/WP 3447
The wood preservation and wood protection industry uses chemicals which are similar. However, because the methods of applications of preservatives are different in wood preservation (pressure treatment) and wood protection (surface treatment) plants, their problems need to be resolved separately. As a part of a federal strategy to protect the environment and human health from potentially toxic com...
G Das, V N P Mathur
Marine wood-borer test with preservatives on the coasts of Turkey
1995 - IRG/WP 95-10091
Marine wood-borer tests were carried out on the coasts of Turkey (Marmara, Mediterranean Sea and Black Sea). Sapwood blocks of 8 x 15 x 30 cm³ in size from Scots pine, Bornmüller's fir oriental beech and sessile oak were used. The test blocks were treated with CCB-salts by full cell process and coal tar creosote by empty cell process. The test blocks were installed on exposure sites bef...
A Bobat
Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals
Leaching of Boron - more than 3 years of field exposure
1997 - IRG/WP 97-30143
The diffusibility of Boron in wood and thus the ability of its leaching is known since long. Nevertheless quantitative data on this process are only rarely available. To overcome this lack of information field exposure tests were started with beam-segments treated with pure boric acid and poles treated with CCB. In addition some of the beam-segments were surface-treated with a varnish to investiga...
A Peylo, H Willeitner
Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler
Penetration as Key Factor for Determining the Performance of Wood Preservatives
2004 - IRG/WP 04-20293
Stakes of Scots pine sapwood with a dimension of 4 x 4 x 75 cm³ were impregnated with preservatives containing 2 % of propiconazole which had passed the EN 113 test criteria without any problems. The
penetration of the colourless preservative was determined successfully by a fungal screening test described by Sutter (1978). The test revealed the insufficient penetration behaviour within the gi...
H Leithoff, I Stephan, R-D Peek
Variations in the virulence of test strains of Coniophora puteana (Schum ex Fr) Karst
1982 - IRG/WP 2185
In laboratory experiments using petri-dishes and small wood blocks (30 x 10 x 5 mm³) 6 different isolates of Coniophora puteana strain BAM 15 were compared with strain FPRL 11E for growth rate and decay capability. Only the recently received strain from EMPA was suitably active giving 24% weight loss after 6 weeks compared with 38.1% for 11E. Collation of data from standard test records revealed ...
A F Bravery, J K Carey, W Worley
Effectiveness of wood preservatives by IUFRO's method
1984 - IRG/WP 3305
Pinus elliottii and Eucalyptus saligna stakes treated with 4.9; 6.9; 9.6 and 13.5 kg/m³ of CCA-A, CCA-C and CCB and with 30-50; 60-80; 90-110 and 120-140 kg/m³ of Benzotar and CNSL (cashew-nut shell liquid) were exposed in seven test sites in Sao Paulo State, Brazil. After 4 years it was concluded that the mean useful life of untreated Pinus elliottii stakes was 8 months and of untreated Eucalyp...
G A C Lopez, E S Lepage, O B Neto
Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver
Use of compression strength loss for measuring decay in the soil block test
1996 - IRG/WP 96-20083
The possibility of using radial direction compression strength of wood, rather than mass loss, was evaluated for both a brown-rot fungus (Gloeophyllum trabeum) and white-rot fungus (Trametes versicolor). With untreated pine wafers (5 x 19 x 19 mm³ - l x r x t) exposed to Gloeophyllum trabeum in a soil block test for five days, the compression strength loss was nearly 50% compared to a 5% mass los...
D D Nicholas, Zhongwei Jin
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 19: Report on the condition of specimens at Sekondi, Ghana after 42 months
1984 - IRG/WP 4109
The results of the first formal inspeation of CCA- and CCB- treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. All untreated control panels of both reference and local species have been destroyed. Of the% CCA- treated specimens, only those of Pinus sylvestris (reference species) and Mitragyna stipulosa (local species) have not been attacked. 3% CCB-treated local species ha...
F F K Ampong
Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher
Fungicidal effectiveness of amended alkylammonium compound
1987 - IRG/WP 3421
Amendment of didecyldimethylammonium chloride was attempted to improve its fungicidal effectiveness and properties of treating solutions. Addition of copper definitely increased effectiveness in controlling wood decay fungi, although metal corrosiveness and stability of treating solutions was unsatisfactory. Further amendment with stabilizer(s), anticorrosive agent(s) and sequestering agent(s) res...
K Tsunoda, K Nishimoto
New experiences with Dry Rot in Danish buildings, heat treatment and viability tests
1989 - IRG/WP 1423
An increasing number of concealed dry rot attacks, especially in older multi-storey houses under renovation, have been detected during the last few years. A necessary consequence is a demand for cheaper methods of repair, compared to the standard method used in Denmark for many years otherwise severely attacked houses will by pulled down. A heat-treatment has been developed and tested in practice....
A P Koch, C Kjerulf-Jensen, B Madsen
Termite resistance classification of some tropical and temperate species based on the laboratory choice test results against formosan termite, Coptotermes formosanu
2004 - IRG/WP 04-20291
The results of classification of termite durability were varied. We carried out
laboratory evaluation of the classification of termite durability on various species by
the choice test against formosan termite, Coptotermes formosanus. We classified five
grades (very sensitive to very resistant). According to our results, azobe, ipe, keruing,
intsia, kapur, yellow meranti, jarraah, malas, cypres...
K Suzuki
Effects of air-seasoning on fungal colonization and wood strength of Douglas fir poles
1987 - IRG/WP 1315
Air seasoning economically reduces the moisture content of Douglas fir poles before pressure treatment with preservatives. Advanced decay in poles in service has resulted when decay fungi (Basidiomycetes) colonized poles during air-seasoning and survived the treatment process. These problems have led to recommendations to severely limit this practice. To determine the role of these fungi in peeled...
J J Morrell, M E Corden, R D Graham, B L Kropp, P Przybylowicz, S M Smith, C A Sexton
Resistance of borate-treated lumber to subterranean termites under protected, above-ground conditions
2000 - IRG/WP 00-30239
An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT(disodium octaborate tetrahydrate)-treated hem-fir samples [Tsuga heterophylla (Raf.)...
K Tsunoda, A Adachi, T Yoshimura, A Byrne, P I Morris, J K Grace
Anti-bluestain treatment developed for log cargoes stacked in subtropical conditions for export on logging ships
1995 - IRG/WP 95-30081
Subtropical environments impose conditions of temperature, humidity and rainfall which are optimal for growth of bluestain fungi. Unprotected softwoods under such conditions become bluestained three days after felling. Furthermore, intervals between harvesting and delivery to export marketplaces exceed the 30-day protection periods attributed to anti-bluestain formulations in such conditions. Thes...
A A W Baecker, M Behr, G D Shelver
The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech.
After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens
Aureobasidium or Hormonema? A Genetic Approach.
2004 - IRG/WP 04-10529
Aureobasidium pullulans is the main organism causing disfigurement of coatings on wood and the surface of exposed timber. This disfigurement of timber in-service is referred to as “bluestain in-service”. A. pullulans is also associated with the sapstaining of dead wood in the forest and in-service. A. pullulans is noted for its highly variable growth forms (polymorphisms). This variability pre...
M J Ray, D J Dickinson, M Buck
Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda
The ecotoxicology assessment of wood preservatives and their active ingredients by means of germination tests using cress - A critical consideration
1999 - IRG/WP 99-50125
With putting the Biocidal Products Directive 98/08/EC (BPD) in place an environmental risk assessment for wood preservatives and impregnated timber is requested. To assess possible risks, suitable test methods are required, which reveal the ecotoxicological profile including environmental fate and behaviour of treated commodities. Germination and growth tests could contribute to the determination ...
P Jüngel, A O Rapp, E Melcher
Studies on the determination of the durability of wooden poles and fence posts
1982 - IRG/WP 3195
This study was carried out by the Forestry Research Institute. 5 Turkish main tree species, Oak (Quercus), pine (Pinus sylvestris), beech (Fagus orientalis) and Fir (Abies bornmülleriana) wooden poles and fence posts, were treated with Tanalith-U and creosote applying pressure process. Tanalith-U was applied by full-cell process and creosote was applied by empty cell process. Treated and untreate...
R Ilhan, O Taskin, A P Erten
The influence of staining fungi on the decay resistance of wood treated with alkylammonium compounds
1984 - IRG/WP 3308
Although found to be very effective in laboratory tests, alkylammonium compounds (AAC's) have failed to perform as well in field stake tests. Examination of leachability showed that this was not the cause. The present study investigated the possibility that staining fungi, (which have been observed to rapidly infect the field stakes), degrade the AAC wood preservative. Soil-blocks were tr...
J N R Ruddick