Anti-feedant activity of stilbenic components from bark of Picea glehnii against a subterranean termite, Reticulitermes speratus
2002 - IRG/WP 02-10447
Stilbenic components, one of polyphenolic groups, widely distributed in plant bodies have been known as anti-microbial agents, but not known whether to have anti-termite activities. A stilbene glucoside, isorhapontin, from the bark of Picea glehnii was examined on the anti-feedant activity against a subterranean Reticulitermes speratus. Isorhapontigenin, the aglycone of isorhapontin, induced from ...
S Shibutani, M Samejima, S Doi


The Protective Effect of Different Tree Bark Extractives against Decay Fungi
2017 - IRG/WP 17-30707
There are various modification methods which increase the resistance of wooden materials. Due to recent environmental regulations, there is a need for new and environmentally-friendly wood preservatives. In this study, six different tree bark extractives were evaluated for their wood resistance against fungal degradation. For this purpose, the white rot fungi (Tramates versicolour) and brown rot f...
Ö Özgenç, S Durmaz


Gleditsia triacanthos tannins for wood coatings
2023 - IRG/WP 23-40995
When used outdoors or in high humidity interiors, wood highly is susceptible to decay by biotic and abiotic agents. Applying coating systems that contain compounds able to control decay is a way to increase the useful life of the wood. Gleditsia triachantos is regarded as a plague in many countries due to its resistance to extreme environmental conditions and its displacement of native forests. In...
C M Ibañez, E Fernandez


The effect of certain wood extractives on the growth of marine micro-organisms
1977 - IRG/WP 438
S E J Furtado, E B G Jones, J D Bultman


Chemical compounds from Eperua falcata and Eperua grandiflora heartwood and their biological activities against wood destroying fungus (Coriolus versicolor)
2005 - IRG/WP 05-30373
The chemistry analysis of the compounds present in dichloromethane and ethanolic fraction as well as bioassays enables to understand the durability differences of Eperua falcata and Eperua grandiflora. The principal distinction between these two species is the acidic subfraction of diterpenoic extract, which is antifungic in Eperua falcata when tested in in-vitro conditions. This study also enable...
N Amusant, C Moretti, B Richard, E Prost, J M Nuzillard, M-F Thévenon


Methodology challenges in developing a transfer of natural durability from sawmill residues, illustrated by experiences with white cypress (Callitris glaucophylla)
2000 - IRG/WP 00-20203
The transfer of durability-conferring extractives from durable to non-durable wood has been accomplished often, but usually as an educational exercise rather than as a commercially oriented process. In the latter environment, many factors previously overlooked become vitally important. How to study them, in the absence of well-developed methodology and given the shorter timeframes being demanded b...
M J Kennedy, M A Powell


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Antifungal activity of a stilbene glucoside from the bark of Picea glehnii
2001 - IRG/WP 01-10402
Stilbene glucosides are widely distributed as phenolic extractives in the bark of Picea glehnii, a commercially species planted in the northern area of Japan, and its content reaches to more than 10% by the dried weight of the bark. Although antifungal activities of these compounds have been reported, the mechanism of growth inhibition is still unclear. Isorhapontin (5,4'-dihydroxy-3&...
S Shibutani, M Samejima


About the relations between the natural durability of some tropical species and their extractives content
1983 - IRG/WP 1208
G R Y Déon


Co-operative research at the Naval Research Laboratory on wood extractives and related compounds as antiborer agents
1977 - IRG/WP 429
J D Bultman, K K Parrish


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Influence of bark damage on bluestain development in pine logs
1997 - IRG/WP 97-10197
Mechanized harvesting of conifers can lead to extensive bark damage, with the resulting wounds providing suitable entry points for bluestain fungi that are not associated with bark beetle vectors. However, the amount of bluestain colonisation can vary greatly between the different types of wound. To evaluate the effect of wound type seven different types of wounds were artificially created on fres...
A Uzunovic, J F Webber, D J Dickinson


Autoxidation of beech condensate
2003 - IRG/WP 03-40261
Liquid effluent from steaming beech wood was studied. The effluent contains many phenolic compounds which can present a significant toxicity. The effluent was treated by oxidation was carried out at 250 rpm for 30 min with NaOH. This was followed flocculation with CaCl2 for 30 min. The influence of parameters such as pH, time of autoxidation were studied. Experimental results reveal the electrosta...
M Irmouli, J P Haluk


Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen


Feasibility of AE (Acoustic Emission) monitoring for the detection of the activities of wood-destroying insects
1992 - IRG/WP 92-2416
The feasibility of acoustic emission (AE) as a nondestructive testing method for the detection of the wood destroying insects was investigated. AEs were detected from the wood specimens under feeding attack of sugi bark borers or powder-post beetles. However, the feasible monitoring area of an AE sensor is influenced by the attenuation of AE amplitude, so that this could be a problem in the practi...
Y Fujii, Y Imamura, E Shibata, M Noguchi


Effect of permeability and extractives on the decay rate of southern pine sapwood in above grund exposure
2005 - IRG/WP 05-20310
The effects of wood permeability and hydrophilic and hydrophobic extractives on the decay rate of southern pine sapwood in above ground exposure were investigated. Permeability was determined by water sorption measurements, and the effect of extractives was studied by pre-extracting the test samples prior to outdoor exposure using water to extract hydrophilic extractives or sequential methanol/cy...
D D Nicholas, T Schultz, L Sites, D Buckner


Influence of the peeling on the absorption in the sap displacement method
1990 - IRG/WP 3626
Results of tests on the Eucalyptus and pine fenceposts treated by sap displacement method are presented. Freshly cut post 2 m in length and 8 to 16 cm in diameter were placed for 6 days with their butt ends down in water soluble preservative solution (CCF) to a depth of about 65 cm, and these were inverted and kept in the same way for 3 days more. The treatment began a few hours after felling. The...
M V Baonza Merino


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Bioassays of extracts from scaly ash (Ganophyllum falcatum B1) against the subterranean termite Coptotermes acinaciformis (Froggatt)
1983 - IRG/WP 1206
Scaly ash, Ganophyllum falcatum B1. wood shavings were extracted by methanol, and fractionated with ethyl acetate, diethyl ether and water, and the anti-termitic properties of these materials bioassayed against the subterranean termite Coptotermes acinaciformis (Froggatt). Laboratory techniques were developed to overcome the problem of limited extractive materials. The results of the various bioas...
J R J French, J P Robinson, J W Creffield


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


The influence of the natural extractives of opepe (Nauclea diderrichii) and African padauk (Pterocarpus soyauxii) timbers on their durability
1996 - IRG/WP 96-30098
Many timbers contain chemical extractives that undoubtedly play a key role in the timber's natural durability. Opepe (Nauclea diderrichii) and padauk (Pterocarpus sp.) are both very durable timbers (class 1), yet they are described as being moderately permeable. This suggests the presence of biocidal chemicals within these timbers, rather than simple blocking agents. Initial trials on the...
E D Suttie, R J Orsler


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...