Chemical, physical-mechanical characterization and durability of thermally modified beech and ash wood by thermo-vacuum process (Termovuoto)
2016 - IRG/WP 16-40758
The paper illustrates part of the results from the CIP Eco-innovation project “Thermo-vacuum: new process for new generation of thermally modified wood”. The project is part of the 7th Framework Programme for European Research and Technological Development, and thermo-vacuum modified wood is already on the European market. The project was selected by the European Commission, EASME Agency, as "...
M Jebrane, I Cuccui, O Allegretti, N Terziev


The effect of acetylation on physical properties of beech (Fagus orientalis) and Alder (Alnus subcordata) wood
2016 - IRG/WP 16-40759
In this study the effect of acetylation on physical properties such as water absorption, volumetric swelling and anti-shrink efficiency (ASE) of beech and alder were investigated. After 24 hours soaking in acetic anhydride, in order to achieving two surface of weight gains, acetylated samples were heated in oven at 120 0C for 90 and 360 minutes. Then water absorption and dimensional stability in...
M Akhtari, M Arefkhani


Dynamics of biofilm formation on wood impregnated with vegetable oils
2016 - IRG/WP 16-40769
Biofilms can be used as a living protective coating for wood, showing advantages compared to traditional wood-coatings regarding sustainability and self-repair. Biofilms can be formed on oil impregnated wood. Such an oil-biofilm system has the potential of protecting the wood against UV and bio degradation, creating a homogeneously black surface with self-healing properties. Results of biofilm for...
K Filippovych, H Huinink, L van der Ven, O C G Adan


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Bacterial adhesion to selected wood finishes
2017 - IRG/WP 17-40793
A new generation of furniture, including antibacterial surfaces, should adjust to the changing needs of an ageing population. Respectively, determination of bacterial adhesion on wooden surfaces, finished with various wood finishes or coating is an important topic. The main aims of our work were of a preliminary character. We wanted to state if the existing methods for testing of bacterial adhesio...
M Petrič, D Kekec, J Žigon, K Godič Torkar, K Bohinc


Penetration behaviour of different hydrophobic carrier substances for oily wood preservatives in Beech and Scots pine sapwood
2017 - IRG/WP 17-40804
The use of creosote as a wood preservative has a long history. Current areas of application are railway sleepers, transmission poles, timber bridges and marine applications. If the approval for creosote will not be prolonged, alternative wood preservatives will be needed. As the penetration behaviour after pressure impregnation of different alternative oily products in this fields of application i...
M Starck, A Gellerich, H Militz


Effects of exposure time on detection of the behavior of white-rot fungi on Oriental beech wood properties
2017 - IRG/WP 17-10902
The comparison of fungal degradation of Orientalis beechwood by two white-rot fungi was evaluated in this study. Biological, mechanical, and chemical assessments of beech wood were carried out at 30 day interval for 120 days. The results demonstrated that both fungi have greater effects on beech wood during each exposure time. However, Trametes versicolor degraded beech wood more effectively than ...
E Bari, D D Nicholas, K M Ohno


FTIR-ATR monitoring of chemical changes of thermo-chemically modified beech wood degraded by brown-rot fungus
2018 - IRG/WP 18-40823
Wood chemical modification with lactic acid oligomers (OLA) has been reported to confer promising properties for wood outdoors applications. To better understand the lactic acid interaction with wood, chemical changes following biological degradation have been characterized with a battery of tests. Fourier transform infrared (FTIR) spectroscopy has been proved to be a valuable tool for studying fu...
C Grosse, M Noël, M-F Thevenon, P Gérardin


An examination of the potential for the use of the Maillard reaction to modify wood
2018 - IRG/WP 18-40829
Finding efficient ways to decrease wood decay caused by fungi and increasing its dimensional stability is an important issue in the timber construction. A possible way to avoid wood decay by fungi is by reducing the water content of wood, since water is a primary condition for fungal growth. Bulking of the wood cell wall by chemical reagents occupies the space where water normally occurs. At the s...
K Peeters, E Larnøy, A Kutnar, Č Tavzes, C A S Hill


The use of bicine and tricine as possible Maillard reagents in a combined thermal/chemical modification of beech
2019 - IRG/WP 19-40852
The effects of thermal modification have been well established, particularly in terms of reductions in mechanical performance. In recent years, there has been an increase in studies related to the Maillard reaction. More commonly associated with food chemistry, it involves the reaction of amines and reducing sugars during cooking procedures. This paper has attempted to combine the use of amines an...
D Jones, C-M Popescu, D Krzisnik, M Hocevar, M Humar, M-C Popescu


Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Effect of Heat Treatment on Physical and Mechanical Properties of Oriental Beech Wood (Fagus orientalis L.)
2021 - IRG/WP 21-40923
The present study aims to investigate the influence of heat treatment on physical and mechanical properties of Oriental beech wood (Fagus orientalis Lipsky.). Samples were exposed to temperature levels of 130˚C, 160˚C, and 190˚C for 3, 6, and 9 h. Selected physical and mechanical properties including compression strength parallel to grain, compression strength perpendicular to grain, bending st...
M D Ghalehno, D Chu, B N Sheshkal, M Humar, M Bahmani


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Data sheet on wood-boring insects. Apate monachus Fabricius. 2. Position systématique, nomenclature, identification et distribution - Espèces végétales attaquée
1981 - IRG/WP 1105
R L A Damoiseau


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


The IRG..Chanelling information and ideas into the mainstream of wood preservation technology
1985 - IRG/WP 5241
IRG Secretariat


Wood preservation in Poland
2004 - IRG/WP 04-30362
Dynamic growth of market demand for wooden elements and articles, generated in Poland increase of interest in industrial preservation. Today, Poland is a substantial producer and exporter of wood made products. Majority of exported wood - approximately 70% - is scotch pine (Pinus silvestris L.), which, due to its natural durability, requires preservation....
A Kundzewicz


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


The effect of certain wood extractives on the growth of marine micro-organisms
1977 - IRG/WP 438
S E J Furtado, E B G Jones, J D Bultman


Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix


Biological screening assays of wood samples treated with creosote plus chemical additives exposed to Limnoria tripunctata
1980 - IRG/WP 408
Laboratory methods for exposure of treated wood coupons to Limnoria tripunctata are described. Chemical additions to creosote were screened using this method. Three pesticides, Endrin, Kepone, and Malathion proved particularly effective. The addition of varying percentages of naphthalene to creosote using several treatment methods are currently being assayed. Results to date show that the coupons ...
B R Richards, D A Webb


Sequestration of copper ions by the extracellular mucilaginous material (ECMM) of two wood rotting basidiomycetes
2004 - IRG/WP 04-10533
The radial growth rate of colonies originating from either whole or ECMM-free inocula of Coriolus versicolor was investigated. The presence of ECMM allowed colonies to maintain higher growth rates than those form ECMM-free inocula up to 2 mM CuSO4 in the medium. The ECMM of C. versicolor and G. trabeum was able to reduce the diffusion of copper ions in solution. The ‘raw’ ECMM of both fungi ha...
D Vesentini, D J Dickinson, R J Murphy