SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy
UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch
An illustrated comment on the soft rot problem in Australia and Papua New Guinea
1977 - IRG/WP 296
A brief survey of soft rot is presented, with particular reference to attack of preservative treated hardwood transmission poles in Australia. Possible explanations of why the preservatives are failing to protect the poles are discussed, together with current efforts to produce control measures. Examples of soft rot in variously treated eucalypt or pine specimens are shown to illustrate the morpho...
H Greaves
Remediation of pentachlorophenol- and creosote-contaminated soils using wood-degrading fungi
1994 - IRG/WP 94-50021
Microbiological treatment of hazardous wastes has generally been associated with the use of bacteria. During the past decade a significant body of evidence has accumulated that demonstrates that fungi, in particular white-rot fungi, have the ability to degrade a wide range of hazardous organic compounds (xenobiotics) and thus might also be useful for treatment of materials contaminated with these ...
R T Lamar, T K Kirk
The colonization of selected naturally durable timbers by marine fungi and borers
1977 - IRG/WP 439
In recent years, concrete and metal have been widely substituted for wood in contact with sea water, but wood products have not lost their usefulness under such conditions. In many cases, wood if sound and durable, may prove to be the most practical and economical of materials used in sea water exposure. Timber when immersed in the sea may be attacked by micro-organisms (bacteria and fungi) and ma...
S E J Furtado, E B G Jones
Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano
Valid names for some common decay fungi and their synonyms
1992 - IRG/WP 92-1522
The taxonomy of wood destroying fungi has changed noticeably within the last ten years. New genera and more well defined generic concepts have emerged with concomitant and necessary changes in nomenclature. The following is a revision of a list originally prepared by Kaarik (1979) in collaboration with Professor Dr. C. Jacquiot (France), Mr. J. G. Savory (United Kingdom) and Dr. G. Seehann (Federa...
M J Larsen, R M Rentmeester
Supplementary experiment to the main trial (IRG/WP/367, 384) to determine the performance of preservative treated hardwoods with particular reference to soft rot
1977 - IRG/WP 3101
The field experiment being carried out by the IRG (described in document IRG/WP/367) is designed to obtain information on the performance of a preservative in different hardwoods in ground contact. A total of 57 timber species is being examined and 36 different field sites are involved representing a complete range of climatic conditions. IRG document WP/384 describes the treatment details of the ...
F W Brooks, C R Coggins, D J Dickinson
The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established.
´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry
Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny
Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson
Collaborative soft rot tests: Paper for discussion in Working Group II
1970 - IRG/WP II 5A
An account of the major part of the collaborative work on laboratory tests of toxicity of preservatives to soft rot fungi initiated by the European Homologation Committee at Delft in 1966 has been published in ‘Material und Organismen’ (1970) as a report of progress. The main objective of these collaborative tests, namely to establish a reliable and acceptable standard test method was not acco...
J G Savory, A F Bravery
Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver
Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch
Reaction of osmium tetroxide with a diphenolic compound as a model substance for demethylated lignin
1986 - IRG/WP 1303
By using caffeic acid as a model substance for diphenolic moieties of demethylated lignin it was found that electron dense particles called by the authors "osmiophilic particles" in former papers are reaction products of OsO4 with the model substance. By these products it is possible to indicate the enzymatic demethylation of lignin taking place during wood decay. The appearance of the electron de...
K Messner, E Srebotnik
Susceptibility of CCB treated wood to fungal colonization
2003 - IRG/WP 03-10492
CCB treated wood is generally resistant to all wood decay fungi. However, like CCA impregnated wood, susceptibility of CCB treated wood to copper tolerant fungi have been observed. The ability of various brown rot fungal hyphae to penetrate and overgrow the wood samples was investigated. Samples made of Norway spruce (Picea abies) were impregnated with 5 % CCB solution according to the EN 113 proc...
F Pohleven, U Andoljsek, P Karabegovic, C Tavzes, S A Amartey, M Humar
Final proposals for a field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot
1976 - IRG/WP 367
A series of hardwood stakes have been prepared and treated in the UK from samples (mainly sapwood) supplied from participants around the world. The stakes include 4 reference species common to each site and, in most cases, at least 2 local species of importance. The treated stakes will be despatched to the co-operating scientists and installed under local conditions. It is hoped that with periodic...
D J Dickinson
Preventive effectiveness of petroleum derivatives against blue-stain fungi. Part 2
1993 - IRG/WP 93-30001
Solvex-Tar, a product derived from the distillation of petroleum could be suitable for the treatment against blue-stain fungi in wood used in exterior carpentry, due to its effectiveness as a fungicide. The aim of this work has been to optimize the application of this product, modifying it as necessary, so as to improve its physical characteristics without interfering with its preventive effective...
E Sanchez, M T De Troya, A M Navarrete, A Guijarro
Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel
Laboratory tests on light organic solvent preservatives for use in Australia. - Part 6: Soft rot resistance of three fully formulated preservatives on different timber substrates
2000 - IRG/WP 00-30245
The above-ground soft rot resistance of substrates treated with three fully formulated light organic solvent preservatives (Cuprivac Green WR, Impresol WR 205 and Vacsol) was studied using a modified vermiculite burial method. The substrates were sapwood of Pinus elliottii and P. radiata and heartwood of Eucalyptus regnans, Pseudotsuga menziesii, Shorea sp. (a lower and a higher density source) an...
G C Johnson, M A Tighe, J D Thornton
Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy
The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling
Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz
Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown
Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil