IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3797 documents. Displaying 25 entries per page.


The long-term performance of boron treated joinery in service - A case study
2000 - IRG/WP 00-20208
Joinery treated with borates 23 years ago and in service in residential flats was surveyed and analysed for boron content. The levels of boron still present were sufficient to prevent decay. None of the windows surveyed showed any decay despite the fact that moisture and sapwood contents were conducive to decay....
D J Dickinson, R J Murphy


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


Results of stake tests on wood preservatives (Progress report to 1974)
1975 - IRG/WP 361
A number of field stake trials on preservative-treated wood have been carried out at Princes Risborough Laboratory from 1928 to the present day, and many of the tests still continue. This paper presents in detail the results obtained to date, covering about 15 000 individual test stakes exposed over the period....
D F Purslow


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Circular letter to all members of WG IV Marine Wood Preservation
1985 - IRG/WP 4122
IRG Secretariat


A novel method for delivering fluids into bolted wooden components.
2004 - IRG/WP 04-40280
The paper describes the development of a washer that enables fluids such as wood preservatives and adhesive resins to be delivered to bolted wooden components in-situ. The system was developed to meet the criteria of low cost and the ability to tolerate inaccurate drilling of holes in the wooden members....
G S Sawyer, B Tole


Direct measurement of fluid flow within wood
1986 - IRG/WP 2248
The problematics of fluid flow mechanism within wood using a permeability concept are highlighted, and the non-feasibility of a practical and versatile model is explained. An alternative method using a negative temperature coefficient thermistor to measure flow velocity directly is presented. The method has been verified in living trees and shows extreme sensitivity for flow above 1 meter/hour. Fo...
J P Hösli


Field trials of groundline remedial treatments on soft rot attacked CCA treated Eucalyptus poles
1983 - IRG/WP 3222
A total of 17 CCA treated Eucalyptus poles, which were found to contain 2-5 mm of soft rot in October, 1980, were reinspected in October, 1982. In 1980, 11 of the poles were given a supplemental groundline bandage treatment of either Osmoplastic or Patox, while 6 of the poles were designated as untreated controls. Two years after remedial treatment, samples were removed from the poles for microsco...
W S McNamara, R J Ziobro, J F Triana


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma


Successive collections of Basidiospores from wood decay fungi (in vitro) show variation in germination levels on common media
1978 - IRG/WP 191
In the course of various preliminary experiments in which spore germination levels of 6 decay fungi on malt and water agar were recorded as controls, it was noted that one could not reliably obtain an expected level of spore germination for any particular fungus. Inconsistent 'control' spore germination levels of a fungus greatly complicates large scale experiments in which compa...
E L Schmidt, D W French


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Discussion of diiodomethyl p-tolyl sulfone (Amical® 48) as a fungicide for wood preservatio
1987 - IRG/WP 3425
The effectiveness of diiodomethyl-p-tolyl sulfone (Amical® 48) as a fungicide for preservation of wood is supported by a discussion of results from the literature and current research programs....
J M Stamm, K J Littel, F M H Casati, M B Friedman


Wood furfurylation process and properties of furfurylated wood
2004 - IRG/WP 04-40289
The first processes for “furfurylation” of wood (wood modification with furfuryl alcohol) were developed several decades ago. Furfuryl alcohol is a renewable chemical since it is derived from furfural, which is produced from hydrolysed biomass waste. Over the last decade modernised processes for furfurylation of wood have been developed. These new processes are based on new catalytic systems a...
M Westin, S Lande, M Schneider


Field Testing of Copper Carboxylate Preservatives
2003 - IRG/WP 03-30322
This paper details our ongoing experience with field testing of copper naphthenate and other copper carboxylate preservative systems. Results from field stake tests at an AWPA Hazard Zone 4 test site are presented. In general, copper carboxylates made with ‘synthetics’ yielded results equivalent to or only slightly lower than systems with straight nap acids or nap acids amended with syntheti...
H M Barnes, M G Sanders, T L Amburgey


The registration of wood preservatives under the Pesticides Act of 1962 in the Netherlands
1976 - IRG/WP 364
J Van der Kolk


Aspects of the biology of the wood-boring weevil Pselactus spadix herbst
1997 - IRG/WP 97-10221
The external morphology of the adult and larval digestive tract of the wood boring weevil Pselactus spadix has been reported for the first time. An examination of adult gut ultrastructure showed that the foregut was adapted for the wood boring habit with the presence of chitinous setae, grinding plates and sieve plates. The adult midgut bore eight caecae and numerous palpii. Spherical yeast-like m...
G Cooper, A J Pitman, G S Sawyer


Respiration methods used to follow the decay of wood and the toximetric evaluation of wood preservatives
1975 - IRG/WP 249
When wood is attacked and decayed by fungi, wood substance and oxygen (02) are consumed, while carbon dioxide (CO2), water and heat are liberated. Early in the 1960's workers from England, Canada and Sweden began studying CO2 evolution, with respect to decay and its control using chemical preservatives, while in Germany and the USA O2 utilization was being similarly examined. Oxygen consu...
R S Smith


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


Biological control with Trichoderma harzianum in relation to the formation for spores the production of soluble metabolites
1994 - IRG/WP 94-10073
The amount of spores produced by three strains of Trichoderma harzianum on the aerial mycelium of agar cultures and in shake cultures, respectively, correlated with the inhibition zones exerted against Phanerochaete chrysosporium in an agar diffusion test. The amount of soluble antifungal metabolites as well as the protein content also correlated with the inhibition zones and the amount of spores ...
J Bürgel, E Horvath, J Haschka, K Messner


Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara


Spore germination of Gloeophyllum trabeum on wood is related to the mass of the wood sample
1978 - IRG/WP 2118
E L Schmidt, D W French


Mould resistance of lignocellulosic material treated with some protective chemicals
1984 - IRG/WP 3294
Effectiveness of preserving lignocellulosic material against moulding by treatement with water solutions of commercial wood preservatives and mixtures of various inorganic salts was investigated and compared with the effectivenes of sodium pentachlorophenoxide and boric acid....
K Lutomski


Chemical compounds from Eperua falcata and Eperua grandiflora heartwood and their biological activities against wood destroying fungus (Coriolus versicolor)
2005 - IRG/WP 05-30373
The chemistry analysis of the compounds present in dichloromethane and ethanolic fraction as well as bioassays enables to understand the durability differences of Eperua falcata and Eperua grandiflora. The principal distinction between these two species is the acidic subfraction of diterpenoic extract, which is antifungic in Eperua falcata when tested in in-vitro conditions. This study also enable...
N Amusant, C Moretti, B Richard, E Prost, J M Nuzillard, M-F Thévenon


Previous Page | Next Page