Your search resulted in 3797 documents. Displaying 25 entries per page.
Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas
Assessing the risks from the use of wood preservatives
2001 - IRG/WP 01-50166-07
PPT-Presentation...
C B Welch
The Tenth Report of the International Research Group on Wood Preservation 1979-1980
1980 - IRG/WP 5110
R Cockcroft
Studies on the infestation behaviour of the powder-post beetle Lyctus brunneus (Steph.) and its physical control in the wood yards of the Caspian forests of Iran
1985 - IRG/WP 1271
Lyctus brunneus (Steph.) is a pest which has not been previously thoroughly studied in Iran. It severely attacks Iranian hardwoods, especially those used in wooden houses and that have not been treated. Research work was necessary to determine the natural resistance of the most important timber species in Iran against this insect....
P Niloufari
The Sixth Annual Report of the International Research Group on Wood Preservation 1974-1975
1975 - IRG/WP 541
IRG Secretariat
Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda
Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood.
Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz
Response of the Formosan Subterranean Termite (Coptotermes formosanus) to Cellulose Insulation Treated with Boric Acid in Choice and No-Choice Tests.
2004 - IRG/WP 04-10532
The tunneling ability of the Formosan subterranean termite Coptotermes formosanus Shiraki through a cellulose insulation material containing11.1% boric acid was tested in choice and no-choice bioassays. We examined tunneling behavior and mortality of termites exposed to treated and untreated insulation material in miniature simulated wall voids. In a choice test termites tunneled through untreat...
M E Mankowski, J K Grace
The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger
Recent soft-rot research in softwoods and hardwoods
1980 - IRG/WP 1108
The purpose of this paper is to describe briefly the current status of our research on soft-rot fungi. The work to be discussed is still in progress and any results described must be regarded as provisional....
J A Butcher
Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne
Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger
Wood preservation in the USA
1982 - IRG/WP 3215
This report is a comprehensive survey of the status of the wood preservation field in the U.S.A. at the start of the 1980s. The importance of wood preservation is discussed and its industry described. Various statistics and analyses regarding the use of treated wood have been compiled. Both pressure and non-pressure applications have been covered, as well as remedial treatments and pest control op...
D D Nicholas, R Cockcroft
Short-term field test method with accelerated infection of Basidiomycetes in wood
1981 - IRG/WP 2155
In the ŠIPAD - IRC Wood Protection Laboratory an attempt has been made to develop a simple short-term method for field testing out-of-ground contact wood using accelerated infections with Basidiomycetes. This method makes it possible to obtain a preliminary assessment of a preservative's quality and to estimate the possibility of achieving promising results in more expensive long-term te...
N Vidovic
Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone
Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal
Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 467
Results of a detailed study on the vertical distribution of fouling and wood-boring organisms of Trondheimsfjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15 March 1977 to 15 July 1977 (Series I) and from 22 July 1977 to 13 March 1978 (Series II). The intensity of fouling generally decreased w...
L N Santhakumaran
Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner
Comparative investigations on the influence of wood seasoning, wood properties and temperature on the toxic values of wood preservatives against Hylotrupes egg larvae
1970 - IRG/WP 28
Comparative tests carried out at three institutes indicated the influence of kiln temperature, position of wood specimens in the cross sectional area and test temperature on the toxic values determined in accordance with DIN 52165 with egg larvae of the house longhorn beetle (Hylotrupes bajulus L.). The preservatives applied were boric acid in distilled water and g-benzene-hexachloride dissolved i...
G Becker, T Hof, O Wälchli
Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea
Effectiveness and synergistic effects between copper and polymer betaine
1996 - IRG/WP 96-30097
Different formulations of "Copper Amine" and Polymer Betaine were studied. During laboratory tests a synergism between both active ingredients against soft rot and dry rot has been found. The efficacy against soft rot according to the "BAM method" and the European Standard ENV 807 depends only on the amount of copper. Long term tests in a fungus cellar for determining the relative protective effec...
H Härtner, V Barth
Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas
Reticulitermes lucifugus Rossi, and its damages in Turkey
1982 - IRG/WP 1152
The moist-wood termite, Reticulitermes lucifugus Rossi, is generally observed on the wood material which has a direct contact with the soil as trunks and fence stakes. It was reported to be found in some provinces in Turkey. The termite has been seen in these areas so far at the endemic level, but any considerable damage or epidemy has not yet been reported. Considerable damages were observed on t...
O A Sekendiz
Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem
Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods