Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Adsorption of ACQ components in wood
2010 - IRG/WP 10-30522
To investigate the chemical adsorption capacity of copper-monoethanolamine (Cu-Mea) components on wood, the Na+ cation exchange capacity (CEC) of red pine (Pinus resinosa Ait.) was determined and compared to the adsorption capacity of free Mea and Cu-Mea complexes. The CEC increased with increasing pH. Free Mea adsorption as a function of pH followed the sodium adsorption curve except at pH over 9...
Myung Jae Lee, P Cooper


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


Eastern redcedar included sapwood: Resistance to mold and termites under laboratory conditions
2012 - IRG/WP 12-10765
The heartwood of eastern redcedar (Juniperus virginiana) frequently contains areas of light-colored wood. This “included sapwood” is considered to be a defect by some manufacturers. In this study, sapwood, included sapwood and heartwood samples from five eastern redcedar trees were exposed to mold fungi or to subterranean termites in a no-choice feeding test. Extractives content was also measu...
C Köse, A M Taylor


In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copper Azole, and borates with and without inclusion of mold inhibitors are presented. The data suggest that the different preservative treatme...
L Jin, P Walcheski, A Preston


The influence of microclimate on the moisture conditions in a Norway spruce (Picea abies (L.) Karst.) joint exposed to artificial rain
2013 - IRG/WP 13-20505
Wood structures outdoors are susceptible to decay if they are exposed to high moisture contents during long periods of time. Structures with joints that act as water traps are especially exposed since high moisture contents are reached in such positions. This paper presents a part of a laboratory study that concerns the relationship between the microclimate and the material climate, i.e. the moist...
M Fredriksson, L Wadsö, P Johansson


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Characterization of wood modification prepared by in situ polymerization with pre-polymer and the mechanism of modification
2013 - IRG/WP 13-40633
Chemical modification of wood is a potential way to obtain high quality wood. In this study, the fast-growing poplar was impregnated with modifier using a pulse-dipping machine by in situ polymerization. Fungal decay analysis, mechanical properties and dimension stability of the natural and modified woods were investigated. The wood samples were also characterized by X-ray diffraction (XRD) Therma...
Qian Lang, Zeng Bi, Junwen Pu


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Critical moisture levels and mould resistance of five different wood treatments
2013 - IRG/WP 13-30632
Mould resistance of five different treatments were tested using two methods, a recently developed method for the determination of critical moisture levels of building materials (RHcrit), and ASTM D3273-94. The critical moisture level method exposed samples at 22 °C and 98, 92, 86 and 82% relative humidity (RH) for 12 weeks. ASTM D3273-94 was performed at 29 °C and about 95% RH. Treatments c...
G Bok, P Johansson, A Ekstrand Tobin, S Bardage


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Study of in-situ gel polymerization established by Si-O-Si framework within wood micropores
2014 - IRG/WP 14-40672
Sodium silicate was used to form Si–O–Si framework by gel process and optimize the effect of the methylolurea impregnation on poplar wood. The modifier cured within the wood micropores by in-situ gel polymerization during the kiln drying. The results showed that treated wood acquired higher mechanical strength, but lower hygroscopicity. New positions of the XRD peaks appeared which caused by s...
Zeng Bi, Qian Lang, Heyu Chen, Junwen Pu


Polyamidoamines (PAA) functionalized with siloxane fragments as potential wood preservatives
2015 - IRG/WP 15-40708
Polyamidoamines (PAAs) utilized in this research were obtained by the reaction between N,N-methyl-bis-acrylamide (MBA) and Ethanolalmine (EtA) and/or aminopropytriethoxysilane (APTES). Different combinations between them were tested as wood preservatives against fungal decay. First, in situ impregnations of PAAs, with the reagents above described in different ratio, were performed and the effectiv...
S Palanti, G Predieri, E Feci, L Bergamonti


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker