Questionnaire for Volume 2 of the basidiomycete monographs
1985 - IRG/WP 1254
12 monographs of wood destroying basidiomycetes were published in volume 1. Volume 2 includes the following 17 basidiomycetes: Antrodia serialis, Chondrostereum purpureum, Climacocystic borealis, Fomitopsis pinicola, Hyphoderma tenue, Lentinus degener, Lentinus squarrulosus, Paxillus panuoides, Phellinus contiguus, Poria xantha, Pycnoporus sanguineus, Rigidoporus vitreus, Serpula himantoides, Sistotrema brinkmannii, Stereum sanguinolentum, Trametes corrugata
T Nilsson


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Monographic card: Coniophora puteana (Schum. ex Fr.) Karst. (Second draft)
1978 - IRG/WP 171
A Käärik


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Effect of asphyxiation on wood decay fungi treated with argon and nitrogen gas
2002 - IRG/WP 02-10452
The effects of low-oxygen conditions, achieved with either argon or nitrogen gas, on the viability of wood decay fungi Coniophora puteana, Antrodia vaillantii and Trametes versicolor, cultivated on PDA medium and infected wood samples, were examined. The fungal cultures were exposed to low oxygen concentration (below 10 ppm) for one to five weeks in hermetically sealed vessels. Anoxic treatment di...
C Tavzes, F Pohleven, M Janisek, R J Koestler


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Use of fluorescent-coupled lectins as probes for studying fungal degradation of wood
1986 - IRG/WP 1288
The ability of the fluorescent-coupled lectins wheat germ agglutin (WGA) and Concanavalin A (Con A) to react with selected Basidiomycetes, Ascomycetes, and Fungi Imperfecti was evaluated using pure cultures of 35 fungi grown on malt extract agar. WGA, which binds specifically to the n-acetylglucosamine residues found in fungal chitin, reacted with nearly all hyaline fungal structures but did not r...
J J Morrell, R L Krahmer, L C Lin


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery


Report on the status of collaborative experiments within the Sub-group on Basidiomycete tests
1983 - IRG/WP 2194
This report summarises the results of co-operative work carried out within the Sub-Group on Basidiomycete tests up to December 1982. The principle findings are recorded in the Conclusions Section. Work intended between IRG-13 in Turkey and IRG-14 in Australia is cited under Future Programme. An Annex provides a response sheet for existing and new participants to notify their contributions....
A F Bravery


A laboratory soil-block decay evaluation of plywoods edge-treated with preservatives
1982 - IRG/WP 2174
Preservative-treated plywood used under conditions or severe decay hazard frequently has its original, or cut edges, protected by the application of a field-cut preservative. This study uses a laboratory test method to compare the efficacy of four commercial preservative treatments against two commonly occurring brown-rot fungi. The results are not meant to indicate the service life of such treate...
R S Smith, A Byrne


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Previous Page | Next Page