IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1546 documents. Displaying 25 entries per page.


Bioremediation of surfactant contaminated waste
1996 - IRG/WP 96-50070
The objective of this work was to determine the potential of fungi as agents for the bioremediation of wastes (particularly wood and soil) contaminated with quaternary ammonium compounds (QACs). Until now only bacteria have been investigated for this purpose. Tolerant strains of Gliocladium roseum and Verticillium bulbillosum were studied for their ability to degrade the following QACs: didecyldim...
J L Bürgel, J Dubois, J N R Ruddick


Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Failure of overhead power transmission and telecommunication poles in Tanzania: Causes, preventive and remedial measures
1988 - IRG/WP 3465
Unless measures are considered urgently to combat massive pole failures occuring in service, it is likely that wooden poles may soon become unpopular. Consequently, pole users may be forced to use costlier alternatives such as underground cables and concrete or steel poles. In trying to countercheck this trend, this paper names the main agents of pole failure, discusses different models of pole fa...
K K Murira


Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Effect of nutrient regimes, temperature, pH, and wood sterilization method on performance of selected bioprotectants against wood staining fungi
1992 - IRG/WP 92-1551
The effect of nutrient regimes, incubation temperature, media pH, and wood sterilization method on performance of four potential bioprotectants (Pseudomonas putida, Pseudomonas cepacia, Bacillus subtilis, and Trichoderma harzianum) against wood staining fungi were evaluated using small ponderosa pine samples over a four week period. Incubation at 32°C resulted in slight increases in the degree of...
J J Morrell, C M Secton


Efficacy of copper:propiconazole and copper:citrate systems in ground contact exposure at a site with copper tolerant fungi
2003 - IRG/WP 03-30305
Southern yellow pine (SYP) sapwood field stakes were treated with copper alone (ammoniacal copper carbonate, ACC) at four levels, or three levels of copper (1.6, 3.2, or 6.4 kgm-3, as CuO), air-dried, then re-treated with propiconazole in a light organic solvent at 0.07, 0.3, or 0.7 kgm-3 retentions. In a separate study, SYP field stakes were treated with three levels of ACC to give 6.7, 13.4 or ...
D D Nicholas, T Schultz


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


The identification of organic compounds in wood using thermal desorption GC-MS - possibilities and limitations
2001 - IRG/WP 01-20224
There is a clear need for the analytical characterisation and identification of organic compounds and their derivatives in different phases especially in timber. In this context the paper describes a rapid and powerful gas chromatographic method for the determination of insecticides, biocides and "other" organic substances in treated and/or modified wood. The main advantage of this procedure is th...
P Jüngel, E Melcher


A bioassay to determine preservative retention in hardwoods and southern pines
1982 - IRG/WP 2183
In this paper the author discusses and suggests a new method of evaluating preservative retention in treated woods by means of bioassays. Twelve North American species were tested with different retention levels of pentachlorophenol (PCP) and copper/chrome/arsenic (CCA) preservatives. The results observed in this work show that among other fungi, Aspergillus niger responds to both preservatives, w...
J C Moreschi


Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden


Preservation of wood-based panels against fungi and insects and and testing its efficiency
1976 - IRG/WP 270
Wood-based panel products which are made of susceptible wood species may be destroyed by fungi under wet conditions and by termites. The glues do not provide sufficient protection unless very high concentrations are applied. Particle boards and fibre boards are not susceptible to beetle infestation, although some species may attack plywood. Various types of preservatives provide sufficient protect...
G Becker, M Gersonde


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Current status of AAC preservatives in New Zealand
1980 - IRG/WP 3141
Two types of alkylammonium compounds (AAC) have been approved as commercially acceptable wood preservatives by the NZ Timber Preservation Authority (TPA). They are alkyldimethylbenzyl ammonium chloride and alkyldimethylamine acetate, both of which must contain either (a) 70% alkyl chains of C12 + C14 and less than 10% of any other individual chain length, or (b) 85% alkyl chains of C12 + C14 with ...
J A Butcher


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


The Copper Tolerance of Mycelium vs. Spores for Two Brown Rot Fungi
2002 - IRG/WP 02-10422
The copper tolerance of two brown rot fungi, Gloeophyllum sepiarium and Oligoporus placentus, has been tested using both mycelia and basidiospores as inoculum sources. Mycelial growth of O. placentus on agar medium was shown to be much more tolerant to copper (as copper sulfate) than that of G. sepiarium. However, there was no difference in copper tolerance of basidiospores between the two specie...
S Choi, J N R Ruddick, P I Morris


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell


Previous Page | Next Page