Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


Improving the Dimensional Stability and Fire Resistance of OSB by Roller-Coating Panels with UV-Curable Finishes
2008 - IRG/WP 08-40434
Oriented strandboard was sanded and roller-coated with UV-cured finishes. The effects of these treatments on the surface roughness, dimensional stability and fire resistance of OSB were assessed. Sanding reduced the average roughness of OSB, but it had a smaller effect on maximum roughness because sanded boards still contained surface voids between some strands. Sanded boards absorbed less than ha...
P D Evans, I Cullis


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Properties of strand board bonded with ammonium pentaborate (APB) modified phenol formaldehyde resin
2009 - IRG/WP 09-40455
Ammonium pentaborate (APB) is combined with phenol formaldehyde (PF) resin in this study to develop a high-performance wood-based composite. The effect of APB and its combination with polyethylene glycol (PEG) on the physical, mechanical properties as well as formaldehyde emission of strand board were tested and compared with disodium octaborate tetrahydrateand (DOT) and zinc borate (ZB). The resu...
Wei Gao, Jinzhen Cao


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Physical and Mechanical Properties of Bamboo Oriented Strand Board Treated with Copper-based Preservatives
2009 - IRG/WP 09-40482
Oriented strand board (OSB) has been gradually accepted, used and developed in China. Bamboo is a renewable and potential non-wood fibre resource for making OSB. But the nature of bamboo makes its products including bamboo OSB (BOSB) more prone to decay and mold. Protection BOSB from biodegradation is the key both to efficiently using bamboo resource and to improving the durability of the final pr...
Juwan Jin, Daochun Qin


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Effect of 4 Preservatives on Physical, Mechanical and Mold-Resistant Properties of Bamboo Oriented Strand Boards
2010 - IRG/WP 10-40483
This study investigated the effects of 4 preservative systems on physical, mechanical and mold-resistant properties of bamboo oriented strand board (OSB) panels bonded with urea formaldehyde resin. Preservative A (Zinc Borate), B (IPBC), C (AAC+Borate) and D (carbendazim + prochloraz) were incorporated with strands during blending at three loading levels. The results showed that the mechanical and...
Juwan Jin, Daochun Qin, Wanshu Wei, Kuan Fan


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Termite Resistance of Different Wood Panels Treated with Bifex® under Laboratory and Field Trials
2011 - IRG/WP 11-10745
The effects of Biflex® on termite resistance of laminated chip Board, MDF (Medium Density Fiber), Ply Wood and Veen Board at 50 ppm were evaluated. Laboratory and field trials resistance tests showed that all woods treated with Biflex were resistant to termites as compared to untreated ones. It was concluded that as chemical loadings increased, termite mortalities increased, and at the same time...
F Manzoor, S A Malik, B M Ahmed Shiday, A Liaquat, N Naz


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Performance of Zinc Borate-Treated Oriented Structural Straw Board against Mold Fungi, Decay Fungi and Termites–A Preliminary Trial
2011 - IRG/WP 11-40571
The performance of zinc borate (ZB)-treated oriented structural straw board (OSSB) against mold fungi, decay fungi and termites was examined in standard laboratory evaluations. OSSB was fabricated with split wheat straw and diphenylmethane diisocyante (pMDI) resin. The ZB was added during panel manufacture to achieve preservative levels (wt.%) of 1.0%, 1.5%, 2.0%, and 3.0%. Untreated (0.0% ZB) OSS...
Guangping Han, M Manning, Wanli Cheng, E Pierre, W Wasylciw


Preliminary laboratory bioassay to evaluate engineered Fibre-boards against subterranean termites C. acinaciformis (Isoptera: Rhinotermitidae)
2012 - IRG/WP 12-10768
In Australia, laboratory bioassays with subterranean termites typically contain groups of workers and soldiers in a substrate of moist mound material. This termite substrate may affect termite consumption, and the test materials create a favorable termite condition for the test. The main purpose of this test is to examine the effect of a melamine formaldehyde treatment of wood panels to evaluate t...
B M Ahmed (Shiday), H Militz, B Ozarska, I Ali, L Kloeser


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Termite resistance of copper-based preservative supplemented aspen strandboards
2012 - IRG/WP 12-30594
Termite resistance of aspen strandboards treated with various copper-based preservative systems was evaluated in field exposure tests. Five copper-based chemicals or zinc borate were blended into aspen furnish at three retention levels prior to pressing. Tebuconazole or 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (DCOI) were added as co-biocides to selected copper-based treatments. Sections from...
J J Morrell, C Vidrine, A Preston, L Jin


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri