Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders


Methodology challenges in developing a transfer of natural durability from sawmill residues, illustrated by experiences with white cypress (Callitris glaucophylla)
2000 - IRG/WP 00-20203
The transfer of durability-conferring extractives from durable to non-durable wood has been accomplished often, but usually as an educational exercise rather than as a commercially oriented process. In the latter environment, many factors previously overlooked become vitally important. How to study them, in the absence of well-developed methodology and given the shorter timeframes being demanded b...
M J Kennedy, M A Powell


European standardization for wood preservation
1990 - IRG/WP 2359
G Castan


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


A survey to assess the current and future usage of timber in British port structures
1998 - IRG/WP 98-10247
Port engineers responsible for 30 British ports were surveyed by questionnaire or interview to establish current and prospective usage of timber in those ports. The ports surveyed account for about 25% of total cargo handled annually in Britain and being located all around the British mainland, were considered to form a representative sample. The survey identified the hardwoods and softwoods in us...
G S Sawyer, S E M Plaster


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Ultrastructure of the attack of a naturally durable timber by tunnelling bacteria
1990 - IRG/WP 1462
The attack of the wood of Eusideroxylon zwageri, a naturally durable species, by tunnelling bacteria (TB) was examined by light microscopy and transmission electron microscopy. Observations were made primarily on fibres. Parenchyma were included in some cases. Both fibres and parenchyma are rich in extractives. In fibres, extractives are primarily present in the lumen. The amber colouration of fib...
A P Singh, T Nilsson, G F Daniel


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Study of the natural durability and impregnability of a metropolitan species of tree
1986 - IRG/WP 2261
The current and predictable evolution of construction timber supply conditions is motivating research for a more efficient utilization of native woods. It is now important to determine statistically reliable impregnability values on a national scale, and to evaluate the natural durability of woods recently introduced in France, or economically important native woods....
M E Mathieu


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Heat treatment of bamboo
2001 - IRG/WP 01-40216
Bamboo is a fast growing material with remarkable mechanical properties. In many tropical and subtropical countries bamboo is available in suitable dimensions for a reasonable price. Therefore it is used for many purposes which range from the basket production up to the industrial production of parquet or paper. However, bamboo is known as susceptible to fungal or insect attack and it is difficult...
H Leithoff, R-D Peek


Experimental real building evaluation of termite attack - Effect of the space between the mat foundation and the thermal insulation
2000 - IRG/WP 00-10374
For evaluating the termite resistance of the real house foundation, specially in the case of thermal insulation systems for foundation walls, thermal insulation which can be attacked by termite, must be evaluate. Because of the difficulty of the water penetration of thermal insulation, the water barrier systems can be protected against termite attacks, in our opinions. The observation on the proce...
K Suzuki, K Hagio, Y Tanaka


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Bibliography of organic solvent based wood preservatives
1971 - IRG/WP 38 E
This publication has as its objective the collection of the more important and more recent references dealing with solvent-based timber preservatives; these are often termed - sometimes wrongly - oil-borne preservatives or even organic wood preservatives. It is hoped that this review will stimulate more fundamental studies in the future in this field or on some of its aspects....
H Alliot


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Maintaining the adoption of the equilibrium moisture content in timber by bifluorides under outdoor circumstance
1989 - IRG/WP 3541
A description is given of the practical application of bifluorides, f. ex. Diffusec in maintaining the adaption of the equilibrium moisture content in timber, as a result of a many years observation of treated timber under outdoor circumstances....
H F M Nijman


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...