Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Heat treatment of bamboo
2001 - IRG/WP 01-40216
Bamboo is a fast growing material with remarkable mechanical properties. In many tropical and subtropical countries bamboo is available in suitable dimensions for a reasonable price. Therefore it is used for many purposes which range from the basket production up to the industrial production of parquet or paper. However, bamboo is known as susceptible to fungal or insect attack and it is difficult...
H Leithoff, R-D Peek


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


Information from the Wood Group of COIPM
1982 - IRG/WP 494
A Gambetta


4th Report on condition of panels at Sekondi, Ghana
1978 - IRG/WP 445
F F K Ampong


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Regulatory and Consumer Challenges Facing Timber Preservation and Durability Interests in New Zealand and Australia
2003 - IRG/WP 03-20282
Timber preservation and durability interests in Australia and New Zealand are facing many challenges and threats arising from regulation and standards changes, to direct competition from competitive materials producers. Industry can address these challenges by pro-active initiation of sound, holistic, research, that addresses the performance needs of the regulators and specifiers and the expectati...
C MacKenzie


Assessment of the natural durability of four Ghanaian hardwoods against the white-rot fungus Coriolus versicolor and soft-rot using laboratory tests
2003 - IRG/WP 03-10498
The natural durability of two lesser-utilized species (LUS) (Corynanthe pachyceras Welw. (pamprana) and Glyphaea brevis (Sprengel) Monachino) (foto) from three forest districts, and two related primary species (Nauclea diderrichii (de Wild.) Merr. (opepe) and Nesogodornia papaverifera (A. Chev.) R. Capuron.) (danta) from one district in Ghana is assessed against Coriolus versicolor Linnaeus Quelet...
C Antwi-Boasiako, A J Pitman, J R Barnett


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


Flow charts for termite and decay tests to determine the natural durability of Japanese cedar (Cryptomeria japonica D. Don)
2008 - IRG/WP 08-20385
This paper deals with the experimental flow charts that were used for determination the effects of fungal decay and termite attack on Sugi heartwood during the course of the study of “Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivate”, which was carried out by Usta et al (2006)....
I Usta, S Doi


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Adequate preservative treatment of tropical and subtropical hardwoods for electric anchor logs
1997 - IRG/WP 97-40101
Most available 27 different hardwood species grown in Bangladesh was investigated regarding suitability as CCA-C (chromated copper arsenate type-C) impregnated anchor logs for rural electrification programme. The kiln-drying properties, sapwood thicknesses, CCA treatability grades of sapwood and heartwood, natural durability of heartwood and CCA retainability at specific assay zone separated 27 ha...
A K Lahiry


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Patterns of long-term performance - How well are they predicted from accelerated tests and should evaluations consider parameters other than averages?
1998 - IRG/WP 98-20130
This paper is a discussion of whether different service-life distribution patterns of products treated with unlike preservatives can be predicted, modeled, characterized, or even anticipated from accelerated laboratory tests. Graphic displays of data from Forest Products Laboratory field plots with preservative-treated and fire-retardant-treated stakes demonstrate the importance of local environme...
R C De Groot, J W Evans


Resistance of painted pine sapwood to mould fungi. Part 1. The effect of waterborne paints and fungicides on mould growth
1997 - IRG/WP 97-10233
The efficacy of different fungicides in acrylate and alkyd paints to protect pine sapwood against mould fungi was studied. The acrylate and alkyd paint systems with and without a preservative dipping treatment prior to painting were also used. Differences in the efficacy of the fungicides to protect the paint film were found. The paint films with isothiazolon and IBPC were resistant against mould ...
H Viitanen, P Ahola


Chapter 1 - Introduction to bamboo
2007 - IRG/WP 07-10635-01
In this introductory chapter the botanical position, distribution, utilization, outlooks, production, research, importance, propagation, natural durability, preservative treatment, importance of preservative treatment, treating principles, research on preservative treatment of bamboos and the objectives of this book have been described briefly under individual caption....
A K Lahiry


A new model for wetting and drying of wood end-grain – with implications for durability and service-life
2011 - IRG/WP 11-20477
New experimental data for wetting and drying of wood end-grain, Sandberg (2009), imply that traditional models for moisture transport are not at all applicable. A new model is developed to consider the phenomenological behaviour of water transport in and out of end-grain, using the pore water pressure and sorption scanning properties. Modelling results are compared to experimental results and the ...
L-O Nilsson, K Sandberg


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


Biodeterioration and preservation of rubberwood (Hevea brasiliensis)
1994 - IRG/WP 94-10084
Plantation-grown rubber trees (Hevea brasiliensis) in the tropics is fast emerging as a significant provider of quality hardwood for a variety of non-structural products, as the aesthetics of the timber is its creamed colour resembling perhaps the priced but depleting Ramin wood or even American beechwood. However rubberwood logs and sawn materials are highly sensitive to sapstain, fungal decay an...
L T Hong, A H H Wong


Natural durability of some commercial timbers of Sarawak, Malaysia in tropical marine environment
2005 - IRG/WP 05-10561
The abundant supply of timber resources in Sarawak makes timber an ideal choice to be used for marine construction. The natural durability of the main commercial timber species of Sarawak in ground contact is well established but the same is not available for marine environment. This study was conducted to assess the natural durability of 28 commercial timber species in tropical marine environmen...
K Jenang, Wang Choon Ling