Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


Durable fibre for durable MDF – testing Tricoya®
2015 - IRG/WP 15-40704
The chemical modification of wood has been a commercial reality for a decade on release of technologies for the modification of solid wood including Accoya®. A challenge and an opportunity for the modification technologies which typically impart dimensional stability, water stability and enhanced biological durability was the adaptation of the technology to wood based panels. This paper presents ...
E Suttie, J Alexander, M Maes


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Natural durability of eight tropical hardwoods species from Africa
2005 - IRG/WP 05-10563
Current forest inventory results reveal that there are more than 700 hundred-hardwood species in tropical forests, of which less than 10 percent are harvested and used for commercial purposes. The increased use of lesser-known species can decrease the pressure on current commercial species, increase the value of the forest and lead to better management practices. However basic information on physi...
P Nzokou, K Wehner, D P Kamdem


Performance of treated and untreated sawn fence posts of Scots pine and Norway spruce
2000 - IRG/WP 00-30247
Sawn fence posts are a rather important product and the objective of this trial was to assess their durability. In 1985 a field trial with treated and untreated fence posts of Scots pine (Pinus sylvestris L.) and Norway spruce (Picea abies (L.) Karst.) was set out at the test field in Ultuna, Uppsala, Sweden. The posts had a dimension of 75 x 100 x 1400 mm3. The preservatives applied were a CCA, a...
Ö Bergman


Exterior wood stains
1980 - IRG/WP 3135
Experience has shown that conventional paints cannot now be relied upon to provide a complete seal against water entry, that in practice water can often circumvent the film and that the paint, far from serving to keep water out will seal it in. Moreover present-day paints are often subject to localised and premature failure out of doors and consequently entail high maintenance costs. Problems of w...
E R Miller


Preservative requirements for exterior particleboard as predicted from accelerated laboratory evaluations
1976 - IRG/WP 265
Arguments for and against preservative treatment of exterior particleboard were considered; it was concluded that preservative treatment is desirable. Laboratory decay tests were conducted to determine levels of sodium pentachlorophenoxide required to protect exterior particleboard from decay fungi. The decay resistance of treated board was compared with that of timber (both naturally durable and ...
M E Hedley


Fungal resistance of smoke-dried Cryptomeria japonica wood
1998 - IRG/WP 98-40118
Performance of smoke dried wood on fungal resistance was studied. The maximum temperature of the smoke seasoning was 80-90°C in the drying room and 70-80°C within the wood for 6 days during the treatment for 15 days. Decay resistance of smoke-dried Cryptomeria japonica wood was evaluated using a brown rot fungus, Tyromyces palustris. Weight losses of untreated wood, smoke-dried wood, and smoke-d...
K Yamamoto, I Momohara, T Nishimura


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Wood preservation in Thailand
1983 - IRG/WP 3265
The report gives a background to Thailand and its timber resources, production and consumption. The history of wood preservation in the country and its modern industrial development are described. Its 19 preservation plants are listed and the production figures of the two major ones given. The wood preservatives in use are noted and the costs of treating a railway sleeper in three different ways c...
A Rananand, R Cockcroft


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


Stability and performance of tributyltin compounds
1984 - IRG/WP 3275
Based on the critical examinations of the disputable permanence of tributyltin compounds in wood, this paper deals with a number of examinations of the relative evaporation, thermal stability and oxidation stability of some TBT-compounds. While thermal and oxidative stability is high for all TBT-species, the relative evaporation at elevated temperature is highly variable, and lowest for the TBT-es...
F Imsgard, B Jensen, H A B Landsiedel, H Plum


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


A study of wood quality of Juglans nigra and hybrid walnut (MJ 209xRA) : durability against Coriolus versicolor, density and MOR
2004 - IRG/WP 04-10522
The study investigated possible effects of harvesting season on some wood properties of Juglan nigra (JN) and a hybrid walnut (MJ209xRA). The samples were taken from trees which were harvested in June July, August, November of the same year, and March in the year after to determine whether there were any significant differences in wood properties as regards the harvesting seasons. In order to test...
B Charrier, F Charrier, D P Kamdem, J B Aurel, G Janin


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Previous Page | Next Page