IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 67 documents. Displaying 25 entries per page.


Termite Resistance of Different Wood Panels Treated with Bifex® under Laboratory and Field Trials
2011 - IRG/WP 11-10745
The effects of Biflex® on termite resistance of laminated chip Board, MDF (Medium Density Fiber), Ply Wood and Veen Board at 50 ppm were evaluated. Laboratory and field trials resistance tests showed that all woods treated with Biflex were resistant to termites as compared to untreated ones. It was concluded that as chemical loadings increased, termite mortalities increased, and at the same time...
F Manzoor, S A Malik, B M Ahmed Shiday, A Liaquat, N Naz


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Performance of Zinc Borate-Treated Oriented Structural Straw Board against Mold Fungi, Decay Fungi and Termites–A Preliminary Trial
2011 - IRG/WP 11-40571
The performance of zinc borate (ZB)-treated oriented structural straw board (OSSB) against mold fungi, decay fungi and termites was examined in standard laboratory evaluations. OSSB was fabricated with split wheat straw and diphenylmethane diisocyante (pMDI) resin. The ZB was added during panel manufacture to achieve preservative levels (wt.%) of 1.0%, 1.5%, 2.0%, and 3.0%. Untreated (0.0% ZB) OSS...
Guangping Han, M Manning, Wanli Cheng, E Pierre, W Wasylciw


Termite resistance of copper-based preservative supplemented aspen strandboards
2012 - IRG/WP 12-30594
Termite resistance of aspen strandboards treated with various copper-based preservative systems was evaluated in field exposure tests. Five copper-based chemicals or zinc borate were blended into aspen furnish at three retention levels prior to pressing. Tebuconazole or 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (DCOI) were added as co-biocides to selected copper-based treatments. Sections from...
J J Morrell, C Vidrine, A Preston, L Jin


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Effect of silver nanoparticles on the rate of heat transfer to the core of the medium-density fiberboard mat
2014 - IRG/WP 14-40653
Effect of silver nanoparticles on the rate of heat transferred to the core section of medium-density fiberboard (MDF) mat was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg based on the weight of dry wood fibers; the results were then compared with the control MDF panels. The size range of silver nanoparticles was 30-80 nm. Res...
H Reza Taghiyari, O Schmidt, E Bari, P M Tahir, A Karimi, P Nouri, A Jahangiri


Study of weathering Characteristics in Profiled and Treated Deck Boards
2014 - IRG/WP 14-40680
Wood exposed outdoors to repeated wetting and drying develops surface checks. Excessive checking of wooden deck boards has been a major source of dissatisfaction to consumers. In this study, Southern pine (Pinus sp.) deck boards were machined to flat (control) and ribbed surface profiles. The specimens were treated with aqueous formulations of 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (EL2) and ...
M Akhtari, D Nicholas, L Sites


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


The susceptibility of oriented structural straw board (OSSB) to damage by subterranean wood-destroying and grass-feeding termites in Australia
2014 - IRG/WP 14-40683
The field performance of untreated oriented structural straw board (OSSB) made from wheat straw was evaluated against two economically important Australian species of wood destroying subterranean termite, Coptotermes acinaciformis and Mastotermes darwiniensis, and two Australian species of grass-feeding subterranean termite, Amitermes meridionalis and Nasutitermes triodiae. Oriented strand board (...
J Hague, D Scown, J Creffield, M Neal


The resistance of composite boards protected with azole and inorganic nanoparticles to basidiomycetes and moulds
2015 - IRG/WP 15-40688
This paper presents a study on the resistance of wood composite boards, glued with silicone adhesive and obtained from chips of Scots pine Pinus silvestris L. and willow Salix viminalis L., to basidiomycetes and mould. The boards were protected in the production processes with fungicides based on metal nanoparticles, as well as on derivatives of 1,2,4-triazole, benzimidazole, and thiazole. The bio...
J Zabielska-Matejuk, I Frąckowiak, A Stangierska


Increasing the hardness of wood-composite panels by nanosilver
2016 - IRG/WP 16-40715
Effect of silver nanoparticles on hardness in medium-density fiberboard (MDF) was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg, based on the dry weight of wood fibers; the results were then compared with the control panels. The size range of silver nanoparticles was 30-80 nm. Composite mats were hot-pressed for 6, 8, and 10 m...
H R Taghiyari, J Norton, K Heidarhaee


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Moisture behaviour and biological durability of high performance flax fibre reinforced composites
2017 - IRG/WP 17-40803
For natural fibre composites in structural and load bearing applications long reinforcing fibres are required. Therefore, much research is performed on flax fibre reinforced composites to optimize them for high performance use. In most cases such research focuses on the mechanical properties, yet the assessment of moisture behaviour, dimensional stability and biological durability is an important ...
N Defoirdt, J Van den Bulcke, F Bensadoun, J Ivens, I Verpoest, J Van Acker


Long-time efficacy of some soil termiticides tested according to “Modified Ground Board Test”
2018 - IRG/WP 18-10935
Field trials of efficacy of soil termiticides available in Thailand were started back in the 1980s at four different locations representing different unique weather types of the country. The method used in the trials (Modified Ground Board Test) is the compulsory test for every soil termiticides aiming to be registered for termite control in Thailand. The ongoing record reveals that some particula...
C Vongkaluang, K Charoenkrung, N Same Rain


Fungicidal properties of black liquor from the waste MDF board digestion in terms of wood protection
2023 - IRG/WP 23-50379
The aim of the work was to determine the fungicidal properties of black liquor as a product of the chemical digestion of waste MDF board. The resistance of wood treated with black liquor from MDF waste pulping process was compared with the resistance of wood treated with black liquor from the pulping process of a by-product from agricultural production. The control material consisted of non-treate...
B Mazela, W Perdoch, A Szulc, I Sieminska


Previous Page