The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Developements in the EEC on the regulation of wood preservatives
1993 - IRG/WP 93-50016
There is a wide variation in the regulation of wood preservatives within the EEC, ranging from product by product authorization under persticides legislation to controls via standards, or simple compliance with basic requirements on classification packaging and labelling. During the past two years the commission of the European Communitiesn has worked on a proposal concerning the placing on the ma...
K Atkinson


Laboratory evaluation of borate formulations as wood preservatves to control the subterranean termite coptotermes acinaciformis (isoptera: Rhinotermitidae) in Australia
2001 - IRG/WP 01-30266
The termiticidal efficacy of Borocol (sodium octaborate tetrahydrate), boric acid, bore-ester-7 and tri- methyl borate was evaluated in laboratory bioassays against Coptotermes acinaciformis (Froggatt). Seasoned sapwood blocks of Pinus radiata D. Don, and Eucalyptus regnans (F. Muell) were impregnated with the various borate compounds. There were marked differences in mass loss and mortality rate ...
B M Ahmed, J R J French, P Vinden


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 2nd Interim Report
1990 - IRG/WP 4161
The results of a collaborative international test to evaluate the performance of elastomeric polyurethane coatings of wooden test samples exposed in seawater at 13 sites around the world are reported. The samples have been exposed at sites with known infestations by molluscan and/or crustacean wood borers. Performance data for up to 4 years exposure at some sites is presented providing information...
R A Eaton


Fixation and leaching of selected Malaysian tropical hardwood after treated with CCA
2001 - IRG/WP 01-40207
The objective of this study is to investigate the fixation and leaching properties of selected Malaysian tropical hardwood (sentang wood (sapwood and heartwood) and rubberwood) after being treated with copper chrome arsenate (CCA) type-C preservative. The samples were treated with retention level of 0.5%, 2.0% and 5.0%. The samples were leached and the leachate were analyzed by AAS and the amount ...
R Hashim, O Sulaiman, Tan Siew Ching, K Yamamoto


Leaching of Arsenic from Mulch Made from Recycled Construction and Demolition Wood
2005 - IRG/WP 05-50232
Mulch made from recycled construction and demolition (C&D) wood has been reported to contain chromated copper arsenate (CCA)-treated wood and potentially release arsenic in the leachate by rainfall. Such recycled wood mulch is commonly masked with iron-oxide colorant, which is known to combine with arsenic. The objective of this study was to evaluate the levels of arsenic leaching from C&...
T Shibata, H M Solo-Gabriele, T G Townsend, B Dubey


Evaluation of fungal remediation of creosote treated wood
1998 - IRG/WP 98-50101-25
Biotechnological remediation of creosote treated wood may be of interest in connection with novel recycling processes. White rot fungi and/or their ligninolytic enzyme systems are supposed to be valuable tools for such processes. This paper reports about results achieved when creosoted wood was treated in solid substrate fermentation with selected white rot fungi after different extraction procedu...
K Messner, S Böhmer


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Low-toxicity DNBP wood preservatives
1987 - IRG/WP 3408
Low and very low toxicity single compound preservatives of both excellent insecticidal and fungicidal activity for interior, extrior and ground-contact applications are presented. These are ester derivatives of alkyl dinitrophenols, in particular of 2-sec-butyl-4,6-dinitrophenol (DNBP) and 2-sec-octyl-4,6-dinitrophenol. These esters, of much lower toxicity than DNBP impart to the treated timber co...
A Pizzi, W E Conradie, A Jansen, R Vosloo


Influence of pre-swelling conditioning on swellometer results for CCA and water repellent additive treated wood
1997 - IRG/WP 97-20125
The pre-test moisture content and conditioning history of wafers cut from wood treated with CCA and an emulsion water repellent additive can dramatically influence swelling curves generated using a standard swellometer apparatus. The rate of water uptake and swelling increased significantly as wafers were dried to lower moisture contents prior to immersion swelling. The pre-swelling conditioning h...
A R Zahora


A technique for determinging the efficacy of wood preservatives for partially treated timber
1988 - IRG/WP 2322
A technique is described for determining the efficacy of wood preservatives either for certain wood species where a full penetration cannot be achieved by normal vacuum-pressure methods or for more permeable species to look at efficacy of treated zone in preventing decay of an untreated core. Both sapwood and heartwood planks of spruce (Picea abies) and pine (Pinus sylvestris) were treated by CCA ...
A J Nurmi


A comparison of inductively coupled plasma spectroscopy and neutron activity analysis for the determination of concentrations in wood
1993 - IRG/WP 93-10048
As wood decays the ionic composition changes, with increases often being seen in the concentrations of Ca, Mg, Fe, Mn and sometimes K. The concentration of eight cations in red spruce sapwood and heartwood samples was determined independently by inductively coupled plasma spectroscopy (ICP) and by neutron activation analysis (NAA) as part of an effort to standardize our analytical procedures and c...
J Jellison, J Connolly, K C Smith, W T Shortle


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Attractive factors of steam-treated larch wood to termite feeding
1998 - IRG/WP 98-10256
The hot water extractives from steam-treated Japanese larch wood were studied to understand the chemical properties of attractive factors of the treated wood to feeding behavior of a subterranean termite, Coptotermes formosanus. Hot water extractives were fractionated and analyzed using chromatography, gel filtration, and NMR methods. The stimulants yielded by the steam treatment were comprised o...
S Doi, Y Kurimoto, W Ohmura, M Aoyama, S Ohara


A new method for the study of microbiological decay of wood in a strictly anaerobic environment
1988 - IRG/WP 2319
Recent work has suggested that strictly anaerobic bacteria may play a role in the biodeterioration of wood, particularly in aqueous environments. However, no suitable test methods exist for the investigation of this hypothesis. An aqueous minimal medium in specifically adapted conical flasks was sterilised, gassed using a 5.5% H2; 31.8% C02; 62.7% N2 gas mixture to remove oxygen and transferred to...
G M Rogers, A A W Baecker


Management of treated wood waste in Canada - Technical and regulatory solutions
2001 - IRG/WP 01-50166-15
A major problem facing the wood preservation industry in Canada is the management of wastes. This refers to wastes generated during the treatment process as well as waste treated wood that is removed from service. The volume of oil borne preservative treated industrial products to be removed from service in Canada over the next 20 years is expected to be fairly constant at approximately 350,000 to...
B Munson


Effectiveness of CCA fixation to avoid hexavalent chromium leaching
2002 - IRG/WP 02-50187
It is generally assumed that hexavalent chromium in chromated copper arsenate wood preservative is substantially reduced to trivalent chromium during fixation and that the potential to leach the more toxic CrVI is minimal. However, there are occasional claims some hexavalent chromium remains in wood after fixation and that small amounts of CrVI are available for leaching. One problem is that ot...
P A Cooper, D Jeremic, Y T Ung


Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Further thoughts on standard principles of testing termiticides and/or wood preservatives
1992 - IRG/WP 92-1530
At the last annual meeting in Kyoto, Japan, there was a special session devoted to the standard principles of testing termiticides. There was definitely a perceived need by researchers and industry for some guidelines that spell out basic procedures required for any methodology in testing termiticidal formulations anywhere in the world. In the testing of new potential active ingredients, considera...
J R J French


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff