Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


Wood decay enzymatic ability of Fusarium circinatum
2012 - IRG/WP 12-10777
There exists pathogens that attack standing trees of forests, and do not usually thrive once the tree is felled. However, occasionally they can be present in a latent state in the wood and can spread and affect new areas with economic, ecological and social consequences. Fusarium circinatum is a fungus that causes “pitch canker” in pine species, and is considered a quarantine organism within t...
M T Troya, F Llinares, Y Serrano, M Conde


Variation in two Postia placenta strains, MAD-698-R and FPRL 280 – mass loss, DNA content and gene
2012 - IRG/WP 12-10781
Brown-rot fungi such as Postia placenta are common inhabitants of forest ecosystems and brown rot fungi are also largely responsible for the destructive decay of wooden structures. The aim of this study was to compare two commonly used strains of Postia placenta – MAD-698-R and FPRL 280. Scots pine sapwood samples were exposed for two and eight weeks to both fungal strains. The following was inv...
N Thaler, G Alfredsen, C G Fossdal


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Effects of Nano-Wollastonite on Ignition Time Reduction in MDF
2012 - IRG/WP 12-40576
Effects of wollastonite nano-fibers on ignition time reduction in medium density fiberboard were studied. Nanowollastonite was applied at 5, 10, 15, and 20 g/kg dry weight basis of wood fibers and compared with control specimens. Two application methods of nanowollastonite were used: surface application, and internal application. Specimens of 150×130×9 mm were prepared and the ignition times wer...
H Reza Taghiyari, H Rangavar, P Noori, A Karimi


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the termites...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Postia placenta cellulase gene expression in modified wood during incipient decay
2013 - IRG/WP 13-40626
In optimization of modified wood, it is important to understand the mode of action of the wood modification and how the fungi response to it. The aim of this study was to investigate the expression of cellulases during the first two weeks of Postia placenta exposure in acetylated, DMDHEU-treated and thermally modified as well as in untreated wood. Using real-time PCR, the gene expression patterns ...
R Ringman, A Pilgård, K Richter


Utilization of TG-DSC to study thermal degradation of beech and silver fir
2013 - IRG/WP 13-40628
Thermal treatment of wood is, besides other wood modification system, used to improve the decay resistance and dimensional stability. However, the chemical changes that are caused by treatment process are still difficult to quantify, characterize and control. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during...
K Candelier, A Treu, J Dibdiakova, E Larnøy, A Petrissans, S Dumarçay, M Pétrissans, P Gérardin


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the term...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems