IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 93 documents. Displaying 25 entries per page.


Susceptibility testing protocol for powderpost beetles in Australia
2002 - IRG/WP 02-20242
Several species of lyctine (powderpost) beetle are able to attack a range of hardwood timbers in Australia. Powderpost beetles infest only the starch-containing sapwood of certain hardwoods and do not infest softwoods. Attack by powderpost beetles on susceptible timber in Australia is almost inevitable and may continue until the food resource is completely utilised. Prevention of powderpost beetl...
B C Peters, J W Creffield, R H Eldridge


Lyctine susceptibility testing and dealing with rarely susceptible hardwood species
2007 - IRG/WP 07-10607
This study examined the lyctine susceptibility of 16 timber species or hybrids. Several of the timbers have been placed previously in a ‘rarely susceptible’ category, but for standards and compliance purposes, such in-between ratings are not acceptable. Timber specimens were spot tested for starch content, and exposed to three species of lyctine beetles in an insectary. New criteria were devel...
L J Cookson, J Carr, N Chew, J W Creffield


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Field performance of wood preservative systems in secondary timber species
1997 - IRG/WP 97-30152
The objective of this ongoing study is to evaluate the performance of new, potential, and standard wood preservative systems in secondary North American timber species. Eleven preservative systems were evaluated in this study - ACQ Type B, Copper Citrate 2: l, CDDC, chlorothalonil/chlorpyrifos, copper-8-quinolinolate, tebuconazole/chlorpyrifos, RH287, propiconazole/chlorpyrifos, copper naphthenate...
P E Laks, K W Gutting, R C De Groot


Effectiveness of "Gang-Nail" plates in preventing splitting of Eucalyptus poles and Brazilian hardwood sleepers
1984 - IRG/WP 3262
This paper presents the results of some tests carried out with an anti-splitting device, placed on the end surfaces of Eucalyptus spp utility poles and Brazilian hardwood sleepers at the beginning of an air-drying period. The type of device used, a "Gang-Nail" plate, reduces significantly the splits at the end-surface of poles, but reduces only a little the splits occurring in sleepers....
A M F Oliveira, J A C Sodré, O B Neto


Progress towards controlling soft rot of treated hardwood poles in Australia
1977 - IRG/WP 289
H Greaves


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


Mold susceptibility of oriented strandboard made with extracted flakes
2008 - IRG/WP 08-40402
As part of a larger study on the manufacture of oriented strandboard (OSB) using hot-water-extracted flakes, the mold susceptibility of extracted-flake and un-extracted-flake OSB was assessed using the standard ‘mold box’ test. OSB made with extracted flakes was much less susceptible to mold. This suggests that the extraction of hemicelluloses and other carbohydrates from wood for the producti...
A M Taylor, O Hosseinaei, Siqun Wang


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


Susceptibility of angiosperm sapwood to white-rot fungal colonization and subsequent degradation: a hypothesis
1997 - IRG/WP 97-10211
It has long been recognized that angiosperm sapwood in nature is relatively easily and preferentially degraded by white-rot fungi. This susceptibility to white-rot fungi is generally believed to be mainly caused by the structure and concentration of angiosperm lignin. However, an explicit explanation as to why lignin structure makes a particular wood vulnerable to white-rot colonisation and subseq...
T Schultz, D D Nicholas


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Adequate preservative treatment of tropical and subtropical hardwoods for electric anchor logs
1997 - IRG/WP 97-40101
Most available 27 different hardwood species grown in Bangladesh was investigated regarding suitability as CCA-C (chromated copper arsenate type-C) impregnated anchor logs for rural electrification programme. The kiln-drying properties, sapwood thicknesses, CCA treatability grades of sapwood and heartwood, natural durability of heartwood and CCA retainability at specific assay zone separated 27 ha...
A K Lahiry


Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


A laboratory evaluation of the susceptibility to biological attack of glued laminated pine timber
1991 - IRG/WP 2387
In the scope of a research programme concerning the use of maritime pine (Pinus pinaster) to produce glued laminated timber structures in Portugal, the natural durability of this material was checked by using laboratory test methods. An European standard, EN 113, was used to test durability against basidiomycetes and a test method developed at LNEC for termites was adapted for this purpose. From t...
L Nunes, H Cruz


Envelope treatment to protect softwood timbers from damage by subterranean termites
2003 - IRG/WP 03-30313
Two aboveground field trials were conducted in Australia to determine the effectiveness of envelope treatments of deltamethrin and permethrin for the protection of softwood framing timbers against termite damage. Radiata pine Pinus radiata D.Don and slash pine Pinus elliottii Englem., were treated with Tanalithä T (a novel solvent) to achieve 5-mm-depth envelopes. Details of a field trial against...
B C Peters, J W Creffield


Susceptibility of softwood bait stakes to attack by subterranean termites (Isoptera: Rhinotermitidae)
1994 - IRG/WP 94-20037
Sapwood stakes of Australian-grown Araucaria cunninghamii (hoop pine), Pinus elliotii (slash pine), Pinus radiata (radiata pine) and North American-grown Pinus sp. (southern yellow pine) were exposed to subterranean termite attack in an in-ground bioassay. Stakes in bait containers and bare stakes were attacked by Coptotermes acinaciformis and Schedorhinotermes intermedius. Basic susceptibility of...
B C Peters, R T Murray, C J Fitzgerald


Positive dosage response of CCA in hardwood power poles to soft rot indicated from New South Wales soft rot survey dat
1983 - IRG/WP 3233
Experience and observation have shown that retentions of less than 16 kg/m³ in the sapwood of individual hardwood poles are unlikely to delay its deterioration sufficiently to ensure an economic performance in some instances. The higher retentions of current practice should do so subject to adequate inspection and maintenance. Increases in retentions requirements up to 35 kg/m³ more or less, dep...
A J Witheridge


Susceptibility of harvested softwoods to infection by sap-staining fungi
2002 - IRG/WP 02-10435
In the UK a field study programme was carried out to compare the susceptibility of softwood timber from five different commercially important tree species to infection by sap-stain fungi. Logs cut from freshly felled Scots pine (Pinus sylvestris), Lodgepole pine (P. contorta var. latifolia), Sitka spruce (Picea sitchensis), Norway spruce (P. abies) and Japanese larch (Larix leptolepis) were expo...
E J Young, R A Eaton, J F Webber


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Susceptibility of CCB treated wood to fungal colonization
2003 - IRG/WP 03-10492
CCB treated wood is generally resistant to all wood decay fungi. However, like CCA impregnated wood, susceptibility of CCB treated wood to copper tolerant fungi have been observed. The ability of various brown rot fungal hyphae to penetrate and overgrow the wood samples was investigated. Samples made of Norway spruce (Picea abies) were impregnated with 5 % CCB solution according to the EN 113 proc...
F Pohleven, U Andoljsek, P Karabegovic, C Tavzes, S A Amartey, M Humar