IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 91 documents. Displaying 25 entries per page.


Pole yield of some softwood and hardwood species grown in Bangladesh
1999 - IRG/WP 99-40143
Growth study on 9 timber species planted in Bangladesh soils revealed that 6 species fall under wooden electric pole yield group-A, produce 33% poles within 10 years, another 33% within 15 years and additional 33% within 20 years of rotation. Two species under yield group-B produce 33% poles within 15 years and another 33% within 20 years. One species under yield group-C produce at best 25% poles ...
A K Lahiry


The susceptibility of acetylated Pinus radiata to mould and stain fungi
1992 - IRG/WP 92-1548
The aim of this investigation was to determine the effect of 5, 10, 15 and 20 percent acetylation weight gains on the susceptibility of Pinus radiata sapwood to mould and stain fungi, and to establish if an acrylic paint, an oil-based stain and a water repellant gave superior protection from fungal growth on wood treated to 20% acetylation weight gain, compared to untreated wood. One treatment set...
R N Wakeling, D V Plackett, D R Cronshaw


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


Standardization of CCA treated 45 hardwood species grown in Bangladesh for REB crossarms
1995 - IRG/WP 95-20059
Researches on 45 hardwood species grown in Bangladesh regarding density, moduli of rupture (MOR), colour and treatability of sapwood and heartwood, seasoning property and natural durability of heartwood revealed that both sapwood and heartwood of 17 species could be full cell pressure treated with CCA at impregnation pressure of 14-18 kg/cm² and only sapwood of rest 28 species could be pressure t...
A K Lahiry


Principles behind the laboratory assessment of materials with subterranean termites - Recent perspectives and shifts in emphasis
1986 - IRG/WP 1291
Laboratory assessments of materials against termites aim to give an indication of the likely performance of materials in the field. To meet this objective, test procedures have to provide the conditions that promote the most vigorous activity of the insects. Implications of recent findings on inter- and intracolony variability in vigour, the need to monitor termite activity with differing types of...
M Lenz


Hardwood Field Experiment: Progress Report 1977-1986
1986 - IRG/WP 3391
The international hardwood field experiment was planned in l976 and set up in same 30 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance. It was hoped that a picture of performance of a range of economically important species would be built up and at the same time provide vital background inform...
D J Dickinson, S M Gray


The influence of drilling patterns on the distribution of toxicants from Polesaver Rods in hardwood poles
1994 - IRG/WP 94-30051
Polesaver Rods are solid rods of wood preservative that are used as a groundline maintenance treatment to control biodeterioration in hardwood transmission poles in Australia. The rods are inserted in holes that are drilled in a prescribed manner to distribute the toxicants into the critical groundline region of the poles. To determine the influence of drilling patterns on the distribution of toxi...
W D Gardner, C N McEvoy


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


Effects of chemicals used for ground-line protection of hardwood poles on termite attack
1988 - IRG/WP 1356
The majority of chemicals formulatet to protect the groundline of hardwood poles in Australia have been fungicides. Nine products were tested against Coptotermes lacteus attack to determine their value in preventing attack by subterranean termites. Results indicated that Busan, high temperature creosote, pigment emulsified creosote, copper naphthenate gel and "Blue 7" had a repellent effect on Cop...
R S Johnstone, R H Eldridge


The effect of concrete embedment on CCA treated hardwood and softwood timbers
1985 - IRG/WP 3340
Small size stakes of Eucalyptus maculata and Pinus elliottii were treated with CCA to various retentions and embedded in concrete collars containing varying amounts of a fungicide additive. During the 30 month trial period stakes were removed after 12, 18, 24 and 30 months and assessed for residual strength. Stakes which showed significant strength reductions were microscopically examined for the ...
L E Leightley, G A Willoughby


Micromorphology of oak wood degraded by brown rot fungus Coniophora puteana
2000 - IRG/WP 00-10356
To characterize the degradation of hardwood by brown rot fungus, Coniophora puteana was incubated on the wood blocks of Quercus accutissima. For comparison, the same fungus was also incubated on the pine wood blocks of Pinus densiflora. In softwood, the shape of the wood cells and thickness of the cell appeared unchanged even the loss of birefringence in the affected areas. In contrast, oak wood d...
Yoon Soo Kim, Seung-Gon Wi, Kwang-Ho Lee


A field test on susceptibility of wood-based board materials to moulds
1989 - IRG/WP 3545
A field test on susceptibility of wood-based board materials to mould growth was carried out under practical, but severe, service-conditions. A total of 19 commercially available composite boards were investigated. It was found that all board materials tested were not completely immune to mould attack. Test results revealed that among the three main categories of wood-based boards involved, partic...
Qiao Wang, B Henningsson


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


Neem leaves, a potential source for protection of hardwood against wood decaying fungus
2005 - IRG/WP 05-30370
Neem leaves are widely recognized for their insecticidal, pesticidal, fungistatic and fungitoxic ability. The present study is to investigate the efficacy of neem leaves extractives against wood destroying microbes, a brown and a white rot. Neem leaves extractives prepared in various solvents such as petroleum ether, acetone, ethanol, methanol and hot water were tested at a concentration levels of...
S Dhyani, S Tripathi, V K Jain


Extracellular laccase production in brown-rot fungus Coniophora puteana
2001 - IRG/WP 01-10391
Coniophora puteana, one of representing brown-rot fungus, was investigated in terms of extracellular ligninolytic enzyme production. Three fungal strains of C. puteana were inoculated in liquid culture medium with sawdust of pine and oak wood. Extracellular laccase production was observed in some strains of C. puteana in the culture medium with sawdust of oak wood. The highest activity occurred at...
Kwang-Ho Lee, Seung-Gon Wi, Yoon Soo Kim


Susceptibility of heartwood of three Pinus species to attack by the subterranean termite Coptotermes acinaciformis (Froggatt)
1994 - IRG/WP 94-20026
Heartwood of plantation-grown Pinus elliottii (slash pine), Pinus caribaea (Caribbean pine) and Pinus radiata (radiata pine) was obtained from a range of locations throughout Australia and New Zealand for use in a field bioassey with subterranean termites. Timber stock was analysed for a number of stilbene and flavonoid heartwood extractive components which could contribute to variation in suscept...
M J Kennedy, L L Dixon, B C Peters


The susceptibility to sludging of sulfate and oxide CCA
1990 - IRG/WP 3599
Radiata pine sapwood was treated separately with a sulphate CCA-C and an oxide CCA in a pilot scale pressure plant using a full cell process. CCA solutions were recovered from the final vacuum phase, placed in plastic tubes, and their susceptibility to sludging determined by examining changes in solution pH, time required for sludge to form and weight and chemical composition of sludge formed. Sul...
B T Mutandadzi, P D Evans


Re-sealing cut ends of envelope-treated softwood framing timber to protect against damage by the Australian subterranean termite Coptotermes acinaciformis: A revisitation
2006 - IRG/WP 06-20335
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate damage on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 ? 90 mm) which has a repellent Tanalith? T envelope, was further investigated. Specimens of commercial Pinus radiata D.Don framing timber (untreated) and Pinus elliottii Englem. (untrea...
B C Peters, M Lenz, J W Creffield


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Utilization of thermodesorption coupled to GC-MS to characterize volatiles formation kinetics during wood thermodegradation
2012 - IRG/WP 12-40587
Identification of volatile degradation products produced during wood mild pyrolysis is important to have better insight on thermodegradation mechanisms. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during wood thermodegradation indicating an higher susceptibility of hardwoods to thermodegradation compare to so...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Kamdem, P Gérardin


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


Previous Page | Next Page