IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 234 documents. Displaying 25 entries per page.


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Impact of heat treatment on physico-mechanical properties of torrefied Antholceistha djalonensis wood
2017 - IRG/WP 17-40811
Thermal modification at relatively high temperatures is an effective method to improve the dimensional stability and mechanical properties of wood. This study was carried out to investigate the impact of heat treatment on the physic-mechanical properties of torrefied Anthocleistha djalonensis wood. Thirty nine defect-free specimens of dimensions 20 mm × 20 mm × 60 were prepared for the determina...
E A Iyiola, B Olufemi, J A Fuwape, J M Owoyemi


Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen


Improvements of monitoring the effects of soil organisms on wood in fungal cellar tests
1996 - IRG/WP 96-20093
Accelerated testing the durability of preservative treated timber in a so called "fungal cellar" or "soil-bed" to evaluate its performance in ground contact is widespread practice. In order to obtain a more accurate and reproducible estimate of preservative performance, several institutes, among them the BAM in Berlin, have routinely carried out static bending tests in addition to visual examinati...
I Stephan, S Göller, D Rudolph


Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


E.R.C. Pole Tester
1982 - IRG/WP 2190
Operating instructions for the ECRC pole-strength tester 120kNm 'PEST'....
G Elcock


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


The utilisation and preservation of Eucalyptus globulus agricultural stakes from Portugal
1989 - IRG/WP 3520
This paper reviews the development and utilisation of Tanalith C treated Eucalyptus globulus stakes: particular reference is made to their use in vineyards. The treatment characteristics of commercially available stakes will be described and penetration patterns evaluated....
A Milne e Carmo, D A Lewis, A Lyman


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Nouvelles techniques de lutte anti-termites à faible impact environnemental
1995 - IRG/WP 95-50040-32
P Martinet


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Environmental impact of CCA poles in service
1997 - IRG/WP 97-50087
Soil samples from different depths and distances from CCA treated utility poles in Canada were analyzed for copper, chromium and arsenic content for a number of soil types, two wood species red pine (Pinus resinosa) and jack pine (P. banksiana) and different pole ages in service. A limited number of poles were equipped with water traps to collect rain water that dripped down the poles and where su...
P A Cooper, Y T Ung, J-P Aucoin


Next Page