Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Borate thermal treatments
1992 - IRG/WP 92-3715
Green, partially seasoned (air-dried, steam conditioned), or kiln-dried southern pine timbers were treated thermally using 15% disodiumoctaborate tetrahydrate solution. After treatment, sections were stored under non-drying conditions to allow for diffusion. Results showed that effective treatment meeting the AWPA minimum retention (0.17 B203 pcf [2.72 kg/m³] in the outer inch) and penetration (2...
H M Barnes, R W Landers, L H Williams


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


Water-repellent additive for CCA
1991 - IRG/WP 3655
Hickson have developed a water repellent additive for incorporation into copper-chromium-arsenate timber treatment solutions. The water repellent emulsion shows good stability in the treatment solution, is easily incorporated and applied in a single stage treatment. No modifications to the additive is safe to treatment schedule are usually needed and use. Weathering of the treated wood is substant...
P Warburton, R F Fox, J A Cornfield


Survey of conditioning treatment practices in India
1978 - IRG/WP 3127
India has 75.3 million hectares (ie about 24% of total land area) under forests out of which the area of productive forests, from which industrial wood is available, is about 60 million ha. The Task Force on Forest Resources Survey has tentatively estimated that the total growing stock in Indian Forests is 24,000 million cubic metres (m³). The total recorded production of wood in the country is r...
M C Tewari


Fixation of CCA in Pinus sylvestris after kiln-drying
1990 - IRG/WP 3594
Tanalith C Paste is 98% fixed and Tanalith Oxide C is 99% fixed irrespective of whether treated Pinus sylvestris is kiln or air dried. A schedule suitable for kiln drying of CCA treated Pinus sylvestris is described....
P Warburton, J A Cornfield, D A Lewis, D G Anderson


Adequate preservative treatment of tropical and subtropical hardwoods for electric anchor logs
1997 - IRG/WP 97-40101
Most available 27 different hardwood species grown in Bangladesh was investigated regarding suitability as CCA-C (chromated copper arsenate type-C) impregnated anchor logs for rural electrification programme. The kiln-drying properties, sapwood thicknesses, CCA treatability grades of sapwood and heartwood, natural durability of heartwood and CCA retainability at specific assay zone separated 27 ha...
A K Lahiry


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


Kiln drying of CCA-treated wood - Some safety and environmental considerations
1987 - IRG/WP 3443
Vapours and condensate from a condenser kiln in which CCA-treated wood was being dried have been collected and analysed. The concentrations of arsenic, copper and chromium found in the vapours from the drying process were well below Swedish threshold limit values. The contents of arsenic and chromium were also low in the condensate, although the copper content was fairly high. The latter result wa...
J Jermer, B Lundberg


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


A note on te seasoning, preservative treatment and suitability of debdaru (Polyalthia longifolia Benth & Hooker.) for poles
1995 - IRG/WP 95-40056
The main work is to determining the suitability of Debdaru (Polyalthia longifolia Benth.) as poles from Government and Village forests are investigated. The poles of Debdaru are easily treatable with CCA preservative by full-cell pressure method, but difficult to dry (air & kiln). Proper quality control must be maintain from procurement to treatment, specially during physical selection & d...
G N M Ilias, M D Rokib-ul-Hafiz


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles
2001 - IRG/WP 01-40206
Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles. Fungal colonization of poles following peeling has been the subject of considerable concern among electric utilities. While the presence of fungi does not, in itself constitute a risk, the survival of these fungi through the conventional treating processes could allow them to continue to degrad...
J J Morrell, P G Forsyth, K L Levien


Standardization of CCA treated 45 hardwood species grown in Bangladesh for REB crossarms
1995 - IRG/WP 95-20059
Researches on 45 hardwood species grown in Bangladesh regarding density, moduli of rupture (MOR), colour and treatability of sapwood and heartwood, seasoning property and natural durability of heartwood revealed that both sapwood and heartwood of 17 species could be full cell pressure treated with CCA at impregnation pressure of 14-18 kg/cm² and only sapwood of rest 28 species could be pressure t...
A K Lahiry


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy


Thermotolerant moulds on timber during kiln drying
1980 - IRG/WP 1109
In recent years a special disease named the wood trimmer's disease has been observed with increasing frequency among saw mill workers. Particularly workers in the trimming department have been affected. The medical symptoms are usually high fever, ague headache, pain in muscles and joints. It was shown that the disease was of immunologic nature and caused by over-exposure to spores from m...
B Henningsson


Effect of post-treatment drying schedule on the modulus of elasticity of CCA-treated southern pine dimension stock using nondestructive methods
1987 - IRG/WP 3413
This paper describes the results from the nondestructive testing for modulus of elasticity (MOE) of southern pine (Pinus sp.) 2 x 6's treated with chromated copper arsenate and redried using three commercial kiln schedules. The data indicate that redrying CCA-treated southern pine dimension stock treated to above-ground retentions (4 kg/m³) has no deleterious effect on the MOE, regardles...
H M Barnes, S Moore


Kiln drying of LSOP treated timber: rate of solvent evaporation, overpaintability and recovery of the solvent
1992 - IRG/WP 92-3711
The rate of solvent evaporation from LOSP treated timber dried in a kiln at 35°C has been investigated. Around 50% solvent removal has been found to be consistent with good overpaintability using a water based acrylic primer. It has been demonstrated that an activated carbon solvent recovery system is capable of removing all the solvent vapour from the outlet of a commercial joinery drying kiIn, ...
P Warburton, L B Sheard


Survey of conditioning treatment practices in the Philippines
1975 - IRG/WP 349
The wood preservation industry in the Philippines is at present beset by many problems. An association of the industry similar to those existing in other countries has only been initiated last year by FORPRIDECOM. It is hoped that the formal organisation of this association will bring into focus the importance of this particular industry in the economic and industrial development of the country. L...
R F Casin


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...