Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


International standardisation: a hypothetical case study with stand-alone borate wood preservatives
1998 - IRG/WP 98-20147
The possibility of developing wood preservation standards with a global remit has a number of obvious advantages as well as far reaching ramifications, many of which are undefined as yet. The commercial implications of adopting international standards are clearly considerable, but equally, such a development is likely to focus attention on the conceptual differences in the way that different regio...
M W Schoeman, J D Lloyd


Comparison of laboratory tests and field experiments for the estimation of emissions from treated wood
2005 - IRG/WP 05-50224-6
The authorisation procedure for biocidal products according to the European Biocides Direc¬tive in¬cludes the assessment of possible environmental risks by the emission of ac¬tive ingre¬dients. This needs an input of data on the expected emissions of biocides into environmental com¬part¬ments. The procedures for the estimation of these emissions should be harmonised. La¬boratory test proceÂ...
U Schoknecht


Screening test methods with termites as first laboratory evaluation of new active substances for wood preservation
1995 - IRG/WP 95-10135
European test methods (EN) with termites have been compared with long-standing experience from screening test methods in the laboratory of Eberswalde. The results are discussed in terms on the possibility of using screening test methods as the first laboratory evaluation of new active substances in wood preservatives. The advantages and disadvantages of these methods are considered. Only a small a...
W Unger


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Laboratory evaluation of AC 217,300 as a termiticidal dust
1983 - IRG/WP 3247
Laboratory bioassays are described with the amidinohydrazone, AC217,300, a candidate termiticide to replace arsenic trioxide in termite control. When used as a dust and topically applied, AC217,300 was toxic to Coptotermes acinaciformis and Mastotermes darwiniensis. Although arsenic trioxide dust causes faster mortality in Coptotermes acinaciformis than AC217,300 dust, the latter has lower mammali...
J R J French, P J Robinson


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Laboratory tests on the residual effects of pyrethroids against termites thirteen years after application
1994 - IRG/WP 94-30056
This paper is in continuation to a series of articles published on the work being developed in Brazil regarding the feasibility of using photostabl synthetic pyrethroids against termites. Tests were carried out to compare the efficacy of five synthetic pyrethroids with the traditional organo-chlorinated pesticide, chlordane. Wooden blocks were impregnated with alcohol-based solutions of the above-...
A M F Oliveira


Efficacy of a novel copper-based organic solvent preservative in laboratory and fungus cellar tests
1995 - IRG/WP 95-30071
The efficacy of Chemicca 4, a novel copper-based organic solvent preservative, was compared with that of other LOSP in pure culture laboratory decay tests and with that of CCA and TBTO in a fungus cellar exposure. It was markedly superior to copper and zinc naphthenates at equivalent metal retentions in laboratory decay tests, and similar in activity to TBTO. After 60 months' fungus cella...
M E Hedley, P N Maynard


Laboratory evaluation of disodium octaborate tetrahydrate (TIM-BORÃ’ ) as a wood preservative or a bait-toxicant against the Formosan and eastern subterranean termites (Isoptera: Rhinotermitidae)
1991 - IRG/WP 1513
A no-choice bioassay indicated that termite feeding was significantly reduced when wood was treated with TIM-BORÃ’ at retentions of >3600 ppm and >900 ppm (w/w) for Coptotermes formosanus and Reticulitermes flavipes, respectively, and thus these wood preservative retention rates may be considered for these termite species. Results of a choice bioassay suggested retention rates of 450-1800 pp...
N-Y Su, R H Scheffrahn


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


Wood plastic composites from modified wood. Part 2 - Durability in laboratory decay tests
2006 - IRG/WP 06-40353
The decay resistance of wood plastic composites, WPCs, was tested according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils, terrestrial microcosms, TMCs). The WPC materials were conically extruded profiles with 30% polypropylene content. The 70% wood content was untreated Scots pine sapwood, acetylated pine and heat treated Norway spruce, respective...
M Westin, P Larsson Brelid, M L Edlund, G Alfredsen


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase chain reaction (PCR) with primer pairs ITS1-F and ITS4 were performed followed by sequencing of the internal transcribed spacer (ITS) region. ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis