IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 138 documents. Displaying 25 entries per page.


Effects of exposure time on detection of the behavior of white-rot fungi on Oriental beech wood properties
2017 - IRG/WP 17-10902
The comparison of fungal degradation of Orientalis beechwood by two white-rot fungi was evaluated in this study. Biological, mechanical, and chemical assessments of beech wood were carried out at 30 day interval for 120 days. The results demonstrated that both fungi have greater effects on beech wood during each exposure time. However, Trametes versicolor degraded beech wood more effectively than ...
E Bari, D D Nicholas, K M Ohno


Molecular identification of marine borers causing wood deterioration on marine facilities in Korea
2019 - IRG/WP 19-10955
The deterioration factors of wood which was used in the marine environment, Tongyeong (South Coast) and Incheon (West Coast) in Korea, were investigated in order to develop technologies for safe and long-term use of timber in ocean facilities. The marine microorganisms isolated by damaged wood were identified as morphological Chelura sp. and Teredo sp. As a result of DNA sequencing, it was confir...
Sae-Min Yoon, Min-Ji Kim, Won-Joung Hwang, Yong-Seok Choi, Dong-Won Son


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Assessing the risk of marine borer attack of the timber trestles and decay of timber above the intertidal zone of the Barmouth Viaduct
2021 - IRG/WP 21-10974
The Barmouth Viaduct is a Grade II* listed structure which carries the single track of the Dovey Junction to Pwllheli line and footway over the Mawddach estuary. It is in a marine environment where timber below the high tide mark is at most risk in Use Class 5 and all timber above in Use Class 3.2, permanently exposed to the risk of wetting. The structure consists of a timber trestle viaduct of ...
J R Williams


Comparison of AE-apparatus for detection of activity of Old house borer larvae, including reality check
2021 - IRG/WP 21-10981
As part of the German funded project ‘InsectDetect’ comparative measurements were done with three different Acoustic-Emission-(AE)-apparatus on 14 pine beams in order to assess presence of active attack by the Old house borer (Hylotrupes bajulus (L.)). In all beams active attack was measured, though in varying intensity. This was corroborated by completely dissecting 10 of the beams. All thre...
J Creemers, B Plinke, U Noldt


Evaluation of decay and energy properties from thermally modified biomasses during fungal deterioration by NIR-spectrometry
2021 - IRG/WP 21-40922
This study is focused on the prediction of fungal weight loss (WL) and high heating value (HHV) from raw and torrefied waste lignocellulosic feedstocks, according to their exposure duration to wood-destroying fungi, using near infrared spectroscopy (NIR) and chemometrics models. Sugarcane bagasse, coffee husk, eucalyptus and pine shavings were torrefied at 290 °C in a screw reactor, during 5, 7...
B de Freitas Homem de Faria, P Santana Barbosa, J Valente Roque, A de Cassia Oliveira Carneiro, P Rousset, K Candelier, R F Teofilo


Introduction to the project ‘Deterioration and decay of wooden cultural heritage in Arctic and Alpine environments’ (ArcticAlpineDecay)
2022 - IRG/WP 22-10997
The Arctic is already affected by climate change, and this is expected to accelerate over the coming decades. Alpine regions in Norway are projected to face similar challenges. Current knowledge on Norwegian wooden cultural heritage in Arctic and Alpine regions is scattered and contains significant knowledge gaps. Historically, - scientists, sectorial governance, tourist trade and commerce have ma...
G Alfredsen, L Ross, A W Hegnes, M S Austigard, J Mattsson, N B Pedersen, A Sinitsyn, V V Martens, A-C Flyen


How the biochemical activities of polyphenols may be effective for the protection of wood deterioration by termites?
2023 - IRG/WP 23-30789
In spite of the remarkable mechanical characteristics of wood for building construction and furniture industry, this material is prone to biodeterioration by xylophagous organisms. This compromises its durability and performances during storage and services, and results in considerable economical losses estimated by the billions. Protection against fungi, termites and other wood biodegrading organ...
J-P Joseleau, D Messaoudi, K Ruel


What products are architects using? Relationships between deterioration part and structural performance in wooden houses
2023 - IRG/WP 23-50374
Architects work in the development of ideas around buildings and all the nuclei where human activity is generated. It is a work of organization of matter, in time and space, where the conceptual world of ideas and the aspirations of inventions, the interior world interact with the exterior in many kinds of realities. But as architects, we have always been interested in why and how things have bee...
I de las Casas


Relationships between deterioration part and structural performance in wooden houses
2023 - IRG/WP 23-50376
Based on the survey examples, there are four patterns of deterioration that tend to occur in plywood bearing walls of wooden houses in Japan. The first is a pattern in which wall is in a whole deterioration. It is a no damage wall or test specimen. The second is a pattern in which only the sill is deteriorating. It is caused by moisture or termites from ground to the base. In addition, there is a ...
Y Ota, H Ishiyama, S Okamoto


Evaluation of decay detection drill data – a semi-quantitative approach
2025 - IRG/WP 25-11067
Decay detection drilling and pick testing are common methods for evaluating decay in structural timber. In this study 63 poles in snow fence trusses at Finse in Norway, where climate change is expected to increase decay hazard, were evaluated by both drilling and pick testing. The aim of this study was to 1: assess a novel method to translate qualitative evaluation of drilling data into quantitati...
M S Austigard, J Mattsson, G Alfredsen, L Ross, N Bjerregaard Pedersen


Detecting wood-decay fungi in walls: a non-destructive approach with an electronic nose
2025 - IRG/WP 25-11070
Wood-decay fungi degrade the structural integrity and safety of wooden buildings, leading to potential hazards and reduced durability. Conventional detection methods, such as visual inspection and destructive sampling, are often impractical for concealed spaces, such as those within walls or beneath floors. These methods often require specialised training and costly equipment, making non-destructi...
M Suzuki, T Miyauchi, S Isaji, R Naganawa


Screening of fungi capable of degradation of β-aryl ether bond from lignin model compounds by using highly fluorescent-emitting detection
2025 - IRG/WP 25-11081
Lignin is an aromatic polymer and composed of phenylpropane units polymerized by dehydrogenases in cell walls. Lignin has a complex chemical structure with C-C and C-O-C bonds, and it is difficult to decompose lignin structure by microorganisms in natural conditions. For the microbial degradation of lignin structure, wood decay fungi can non-specifically degrade the lignin polymeric structure by o...
A Ishikawa, Y Mori, Y Ota, M Kiguchi