Temperature influence on the growing velocity and cellulolytic activities of Poria placenta strains from several locations
1986 - IRG/WP 2263
The differences observed on the FPRL 280 Poria Placenta strain at several Research European Laboratories for determining up the fungicide effectiveness of wood preservative has carry us to do a comparative study about the cellulolytic activity and growth velocity of each of this strains at different temperatures (22, 24 and 28°C). The results show significative differences when the temperature is...
A M Navarrete, M T De Troya


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


What can DNA fingerprinting, aggression tests and morphometry contribute to the identification of colonies of the Formosan subterranean termite
2000 - IRG/WP 00-10371
Multilocus DNA fingerprinting, aggression tests and morphometry were compared to evaluate their potential for the identification of colonies of the Formosan subterranean termite, Coptotermes formosanus (Isoptera: Rhinotermitidae) in Hawaii. DNA fingerprinting separates the termites from all studied collection sites. Since the genetic similarity between termites from different collection sites lies...
C Husseneder, J K Grace


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Molecular studies on isolates of Serpula lacrymans
1989 - IRG/WP 1421
The major protein species present in detergent extracts of 14 different Serpula lacrymans isolates have been compared, by sodium dodecyl sulphate polyacrylamide gel electrophoresis (SDS-PAGE), with a standard strain, viz. Serpula lacrymans FPRL 12C. Following silver staining of SDS gels the major protein species identified in 12 isolates were similar to those found in the standard strain. However ...
A Vigrow, D Button, J W Palfreyman, B King, B M Hegarty


Virulence testing of cultures of different origins of the test fungus Coriolus versicolor strain CTB 863 A
1986 - IRG/WP 2267
The virulence of cultures of different origins of Coriolus versicolor CTB 863 A - a strain which is mentioned in EN 113 - was tested. Standard blocks of beech wood were used at temperatures of 20-22°C and 26-28°C and particleboard was tested at 26-28°C. The decay capacity of the different inoculations varied widely, as could be expected it was greatest at the higher temperature level....
W Kerner


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Results from soft rot tests in vermiculite jars
1976 - IRG/WP 272
T Vihavainen


About the relations between the natural durability of some tropical species and their extractives content
1983 - IRG/WP 1208
G R Y Déon


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


Virulence tests with fungal strains used in EN 113 CEN ring test. Results with Coniophora puteana (Schum.ex Fr.) Karst
1986 - IRG/WP 2249
D Dirol


Collaborative soft rot experiments 1974. Preliminary analysis of results
1975 - IRG/WP 251
J K Carey, J G Savory


Molecular Microbiology and Wood Protection
2009 - IRG/WP 09-20416
During the last decade, the development of molecular tools has allowed significant advances in environmental microbiology. Such techniques have proved to be invaluable tools for the qualitative and quantitative description of environmental microbial communities. The aim of this paper, written for non-specialized readers, is to discuss the possible applications of such tools in wood preservation fi...
E Gelhaye, M Morel


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals