Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin


Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen


Improvements of monitoring the effects of soil organisms on wood in fungal cellar tests
1996 - IRG/WP 96-20093
Accelerated testing the durability of preservative treated timber in a so called "fungal cellar" or "soil-bed" to evaluate its performance in ground contact is widespread practice. In order to obtain a more accurate and reproducible estimate of preservative performance, several institutes, among them the BAM in Berlin, have routinely carried out static bending tests in addition to visual examinati...
I Stephan, S Göller, D Rudolph


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


E.R.C. Pole Tester
1982 - IRG/WP 2190
Operating instructions for the ECRC pole-strength tester 120kNm 'PEST'....
G Elcock


The utilisation and preservation of Eucalyptus globulus agricultural stakes from Portugal
1989 - IRG/WP 3520
This paper reviews the development and utilisation of Tanalith C treated Eucalyptus globulus stakes: particular reference is made to their use in vineyards. The treatment characteristics of commercially available stakes will be described and penetration patterns evaluated....
A Milne e Carmo, D A Lewis, A Lyman


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Heat treatment of bamboo
2001 - IRG/WP 01-40216
Bamboo is a fast growing material with remarkable mechanical properties. In many tropical and subtropical countries bamboo is available in suitable dimensions for a reasonable price. Therefore it is used for many purposes which range from the basket production up to the industrial production of parquet or paper. However, bamboo is known as susceptible to fungal or insect attack and it is difficult...
H Leithoff, R-D Peek


The leachability, biological resistance, and mechanical properties of wood (Pinus sylvestris L.) treated with CCA and CCB preservatives
1999 - IRG/WP 99-30207
Scots pine (Pinus sylvestris L.) specimens treated with CCA and CCB preservative solutions (1.0%) were subjected to several fixation processes and leached elements from the specimens were determined. In addition, the specimens exposed to different fixation temperatures were subjected to soil-block test using two brown-rot fungi and one white-rot fungus in order to investigate the effects of fixati...
S N Kartal


The performance of softwood species used as poles in Queensland
1985 - IRG/WP 1253
In Queensland, the conifer Pinus elliottii could provide material suitable for use as poles. Full size pole material has been readily treated with CCA with no significant loss in strength. Seasoning of logs prior to treatment requires particular attention in the wet tropical and sub-tropical regions of Queensland. Experimental and in service field tests have indicated excellent performance of CCA ...
L E Leightley


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Physical and mechanical properties of a suitable constructional timber of Bangladesh
1997 - IRG/WP 97-40102
The study of physical and mechanical properties of lohasirish timber (Derris robusta Roxb.) grown in Bangladesh revealed that the sapwood is whitish to yellowish white, heartwood is dark grey to blackish in colour; the texture is moderately fine, the grain in mostly straight and coarse with whitish rings of parenchyma; shrinkage is moderate; the EMC ranges from 12% to 16%; fuelwood colorific value...
A K Lahiry


Bibliography: Interactions of wood preservatives with wood, metals, glues, paints and concretes
1983 - IRG/WP 3271
H Becker


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Innovations in the treatment of Southern pine heartwood
2000 - IRG/WP 00-40172
Whereas the sapwood of southern yellow pine (Pinus spp.) is readily treatable, the heartwood is essentially impermeable to preservatives such as chromated copper arsenate (CCA). Preliminary studies at the Mississippi Forest Products Laboratory indicate that increases in penetration and retention of preservative in pine heartwood can be obtained by subjecting kiln dried dimension stock to varying m...
M G Sanders, T L Amburgey, H M Barnes


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas