IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 504 documents. Displaying 25 entries per page.


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey


A natural exposure weathering test for the evaluation of preservative performance
1992 - IRG/WP 92-2400
Natural exposure weathering tests were carried out by externally exposing treated wood samples for varying periodes of time up to 36 months. In the laboratory these samples were assayed for residual preservative effeciveness using Coniophora puteana FPRL 11E. The results indicated a loss in efficacy over and above that determined using artificial ageing procedures such as EN73 (evaporative ageing)...
J Brown, G R Williams


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Durability of plywood made from soft- and hardwoods assessed according to ENV 12038 after artificial and natural ageing
2000 - IRG/WP 00-20191
Plywood was prepared from Norway Spruce and pure heartwood of Douglas Fir, Scots Pine, European Oak, False Acacia and Macoré using a phenol-formaldehyde glue. The panels of 38 mm in thickness were pre-conditioned according to the following procedures: a) 12 weeks storage at 20°C/65% rh, b) 2 weeks artificial weathering (with rain and UV-radiation at changing temperatures), and c) a natural weath...
H Leithoff, R-D Peek


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Biological and physical properties of phenolic-resin treated wood before and after natural weathering
1999 - IRG/WP 99-40132
Biological and physical properties of phenolic resin-treated particleboards, which were made from fast growing tress and agrowaste as raw materials, were evaluated before and after natural weathering in tropical climate. The particles were sprayed with a mixture of a low molecular weight phenol-formaldehyde resin (5.0, 7.5 and 10% loading) and the adhesive phenol resin (8% loading). Results with l...
S Yusuf, Y Sudiyani, H Kajita, Y Imamura, M Takahashi


Blue stain in timber in service. Preliminary results of the IRG collaborative tests to compare natural and artificial weathering
1978 - IRG/WP 286
The collaborative programme was initiated at IRG Meetings in Wildhaus, 1976. The six collaborators were BAM (Berlin), Cuprinol Ltd (UK), EMPA (Switzerland), GORI (Denmark), PRL (UK) and Imperial College (UK). Experimental plans were finalised in December 1976 and panels treated by Cuprinol Ltd early in 1977. Natural weathering was carried out by BAM, Cuprinol, EMPA, GORI and PRL during April-Septe...
A F Bravery, D J Dickinson


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Testing blue stain fungicides for joinery timber in combination with natural weathering
1976 - IRG/WP 268
Joinery timber in outside use becomes affected by blue-stain after a short time of exposure. This is especially the case with pine sapwood treated with unpigmented lacquer, but also with other timber species as well as different types of surface treatment. According to the basic investigations of BUTIN this is due to special types of blue-stain fungi, called "Lack-bläue" (lacquer blue-stain), in ...
H Willeitner


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp


Depletion and Redistribution of Boron in Bundles of Commercially Treated Lumber Exposed to Artificial and Natural Rainfall
2008 - IRG/WP 08-30474
The depletion and redistribution of boron from stacks of Southern Yellow Pine lumber pressure treated with disodium octaborate tetrahydrate (DOT) and exposed to artificial and natural rainfall was examined. When the lumber was exposed to periodic simulated rainfall, 5.7-8.1% of the measured boron present leached from the lumber after exposure to over 300 mm of rainfall. In tests which exposed bo...
M E Mankowski, M J Manning


Component leaching from CCA, ACQ and a micronized copper quat (MCQ) system as affected by leaching protocol
2009 - IRG/WP 09-50261
Leaching results for Cu, Cr and As (CCA) and Cu (ACQ and MCQ) from southern pine are compared for laboratory tests (AWPA E11, and draft OECD methods I and II) and natural weathering of horizontally and vertically oriented lumber samples over two seasons. This paper expands on results and comparison of results presented at the IRG regional meeting in Costa Rica in Dec 2008 (Cooper and Ung 2008) a...
P A Cooper, Y T Ung


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak