Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan


Proposed standard laboratory method for testing fungicides for controlling sapstain and mould on unseasoned lumber
1977 - IRG/WP 292
This laboratory method is for determining the effective concentration, or concentration for zero growth (CGo), for fungicides or preparations of fungicides which are potentially useful in protecting packaged or unseasoned lumber in storage and shipment from biodeterioration by sapstain fungi and moulds. The test is rapid and may be completed in three weeks and gives a good indication of the toxici...
A J Cserjesi


Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner


Mould resistance of lignocellulosic material treated with some protective chemicals
1984 - IRG/WP 3294
Effectiveness of preserving lignocellulosic material against moulding by treatement with water solutions of commercial wood preservatives and mixtures of various inorganic salts was investigated and compared with the effectivenes of sodium pentachlorophenoxide and boric acid....
K Lutomski


Field trials of anti-sapstain products. Part 1
1991 - IRG/WP 3675
The results obtained in two field tests of anti-sapatain products, carried out in four locations in Portugal, are presented. Boards from freshly cut logs were hand-dipped, close staked and left to dry for periods from four to six months. The results obtained seem to indicate that some of the products tested performed at least as well and sometimes better, than a 3% NaPCP solution which was used as...
L Nunes, F Peixoto, M M Pedroso, J A Santos


Evaluation of the effectiveness of three microbiocides in the control of sapstains
1982 - IRG/WP 3212
Results of field test on the effectiveness of BUSAN 30, CAPTAN, FOLPET against mould and sapstain in Pinus elliottii are presented. The viability of use of FOLPET in Brazil as an alternative to sodium pentachlorophenate is also discussed....
S Milano, J A A Vianna Neto


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Blue-stain fungi (Ceratocystis spp.) found in Spain on pine woods
1989 - IRG/WP 1410
So far, there is only a very limited reported description of the different Ceratocystis spp. present on fresh wood in Spain. So, the main goal of this work has been the identification of species of this genus causing blue-stain on Pinus pinaster A. Ait. and Pinus sylvestris L. woods. We have also investigated the relationship between the species found and their propagation vectors (insects and win...
M T De Troya, A M Navarrete


Relationship between stacking, location and antisapstain preservatives on visible degrade of Eucalyptus regnans and Pinus radiata boards
1999 - IRG/WP 99-20162
An antisapstain trial was established at a Eucalyptus hardwood sawmill in Victoria, Australia. The trial incorporated two commercial formulations of antisapstain preservatives, used at four different concentrations on both hardwood (Eucalyptus regnans F. Muell) and softwood (Pinus radiata D. Don) boards. The trial also utilised different stacking methods (block-stacked, sticker-stacked, and block-...
J Snow, P Vinden, S M Read


Tentative method of testing wood preservatives against blue staining
1977 - IRG/WP 259
The blue stain of sawn wood is still a real problem in Poland. Although a preservative based on sodium orthophenylphenoxide has been introduced into sawmill practice, and the technology of wood protection developed with it, new information has been obtained concerning blue stain in wood material destined for export. In order to select new chemicals or to improve the effectiveness of the ones in cu...
E Tarocinski, O Lewandowski, M H Zielinski


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1980 - IRG/WP 279
G Castan


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Rapport sur l'activité du CEN/TC 38
1983 - IRG/WP 2204
M Pottevin


Working Group II: Sub-group: Methods of testing anti-stain chemicals for protecting sawn lumber during storage, transit
1978 - IRG/WP 2121
R Smith


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Characterisation of growth and stain of different groups of sapstain fungi on lodgepole pine
1999 - IRG/WP 99-10326
Canada is the world's largest exporter of softwood lumber. These softwood shipments are susceptible to a variety of wood-inhabiting fungi that can lead to sapstain discolouration, which in turn decrease the product value. Furthermore, the presence of these microorganisms may be unacceptable to the importing countries. The objective of this work is to assess the sapstaining capability and ...
C Fleet, C Breuil, A Uzunovic, A Byrne


Anti-stain field trials in British Columbia
1981 - IRG/WP 3174
Four alternative anti-sap stain chemicals were subjected to a four month field evaluation during the summer of 1980. The test, established at a Vancouver Island sawmill, was designed to evaluate the potential long-term effectiveness of sodium tribromophenate (Velsicol Ltd.), Biocom XX (Bramco Industries) containing methylene bis-thiocyanate, Woodbrite NTX (Van Waters & Rogers Ltd.) containing ...
D V Plackett


Detection of semi-quantitative and qualitative enzymatic activities of blue-stain fungi
2000 - IRG/WP 00-10347
Blue-stain, produced in forests, continues to be a problem in countries of moderate climate. In forestry, in certain geographical areas of Spain, it has been observed that anti-sapstain products have not always been efficient, as their fungicidal effectiveness varies on occasion, depending on the species of wood and microbiota that exist in the region. It is not always easy to identify the species...
M T De Troya, F Llinares, D Muñoz-Mingarro, M J Pozuelo, N Acero, C Rodríguez-Borrajo, A M Navarrete


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1977 - IRG/WP 288
G Castan


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Next Page