IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 653 documents. Displaying 25 entries per page.


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Overview of the treated wood quality control program in the United States with the recent challenges and advances
2017 - IRG/WP 17-20616
In the past two decades, there have been significant and rapid changes in wood protection technologies for residential applications which have moved away from long established heavy duty metal oxide based products such as chromated copper arsenate (CCA). The successor generation of wood protection systems usually contain copper as the primary biocide, in combination with carbon-based co-biocides s...
L Jin


Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Status of the research and development of a new preservative system (EFPL) for pressure treatment of spruce in Canada
1975 - IRG/WP 348
Our work has been to develop a system which would have the stability of the ACA system and the formulation flexibility of the CCA system enabling properties such as fixation of arsenic, water repellency, appearance and cost to be controlled. Our permeability studies of spruce using a method previously developed indicated that an ammoniacal solution of copper arsenate is an excellent candidate for ...
J Rak, M R Clarke


Manual of a mini treating plant for waterborne preservative treatment of timber and bamboo
1999 - IRG/WP 99-40130
This contributional article includes machinaries and equipments necessary for a small wood treating plant for the pressure treatment of tim bers with waterborne preservatives along with the cost and design. The preservative treatment limitations, treatment schedules and specifications for different products have been described. The cost of a mini treating plant will be 6,00,000 Tk. (13,000 US$), s...
A K Lahiry


Registration and approval of wood preservatives in Australia and New Zealand
2001 - IRG/WP 01-50166-06
Wood preservatives are treated as agricultural chemicals in Australia and, at the time of writing, as pesticides in New Zealand. Antisapstain products are currently considered to be agricultural chemicals in New Zealand while wood preservatives in the future will be considered as hazardous substances under the Hazardous Substances and New Organisms Act when this Act is fully implemented. They are ...
H Greaves


Field performance of wood preservative systems in secondary timber species
1997 - IRG/WP 97-30152
The objective of this ongoing study is to evaluate the performance of new, potential, and standard wood preservative systems in secondary North American timber species. Eleven preservative systems were evaluated in this study - ACQ Type B, Copper Citrate 2: l, CDDC, chlorothalonil/chlorpyrifos, copper-8-quinolinolate, tebuconazole/chlorpyrifos, RH287, propiconazole/chlorpyrifos, copper naphthenate...
P E Laks, K W Gutting, R C De Groot


Fire resistance of preservative treated fence posts
1994 - IRG/WP 94-30033
Pine fence posts were pressure treated separately with CCA-C, CCA-wax, CCA-oil and creosote. Treated posts and untreated controls were planted in the ground in a randomised block design, weathered for six months and then subjected to a controlled burning test using two fuel loads. Creosote treatment increased the time that posts were alight whereas CCA treatment had no such effect. However, CCA tr...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Improved techniques designed for evaluation of fungicides in soil for control of dry rot fungus Serpula lacrymans
1985 - IRG/WP 2238
Improved techniques provide a laboratory method for the evaluation of chemicals in soil for control of dry rot fungus Serpula lacrymans. Results with their application to three chemicals were reported. These techniques are useful to eliminate chemicals lacking the necessary toxicity and weatherbility for dry rot control when the chemicals have been applied to the soil....
M Takahashi, K Nishimoto


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


Performance of preservative-treated hardwoods with particular reference to soft rot. Report of condition of specimens installed in Victoria, Australia
1980 - IRG/WP 3155
J Beesley, R McCarthy


Protocol for evaluation and approving new wood preservative
1985 - IRG/WP 2159
M E Hedley, J A Butcher


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Insect resistance of preservative treated tropical plywood against Lyctus
1990 - IRG/WP 1453
Seven plywood types composed of tropical wood species, vulnerable to Lyctus, were treated with various commercial water-borne and oil-borne preservatives. A wide range of preservative retentions was obtained by treating boards with dip treatment, steeping, double-vacuum and vacuum-pressure impregnations. Selected samples were subsequently tested for their insect resistance against Lyctus africanus...
J Van Acker, M Stevens, M Pallaske


Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


CEN Draft (38 N 460E) Standard: Test method for determining the protective effectiveness of a preservative in the marine environment
1986 - IRG/WP 4132
This European Standard describes a marine test method which provides a basis for asseasing the effectiveness of a wood preservative used to prevent attack of timber in sea-water by marine borers. The method is only suitable for testing preservatives which are intended to prevent attack by marine wood boring organisms of treated timber for use in more or less permanent contact with sea-water. It is...
G Castan


A novel method for delivering fluids into bolted wooden components.
2004 - IRG/WP 04-40280
The paper describes the development of a washer that enables fluids such as wood preservatives and adhesive resins to be delivered to bolted wooden components in-situ. The system was developed to meet the criteria of low cost and the ability to tolerate inaccurate drilling of holes in the wooden members....
G S Sawyer, B Tole


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


Previous Page | Next Page