The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields


Bending properties of wood after its decay with Coniophora puteana and subsequent modification with selected chemicals
1999 - IRG/WP 99-40146
Mechanical properties of wood are often decreased due to decay processes caused by biotic and/or abiotic factors. Damaged wooden elements (e.g. historical structures) can be reinforced by more methods, including their modification with convenient chemicals. This paper presents influences of selected chemicals on basic bending properties (modulus of elasticity - MOE, modulus of rupture - MOR) of so...
L Reinprecht, S Varinska


Fungal decay of acrylate treated wood
2004 - IRG/WP 04-30357
Natural durability of wood species is variable. Chemical wood preservatives, such as biocides are necessary for extension of their service life. Many methods have been developed to increase the resistance of wood and wood products against wood-destroying organisms during the last years. The most frequently used methods are chemical and thermal modification of wood. In wood modification the basic c...
Z Tiralova, L Reinprecht


Influence of the decay of spruce chips by the selected fungi on their chemical structure and the pulp properties
2004 - IRG/WP 04-10510
The paper focuses on changes in the weight and in the molecular structure of spruce chips submitted to long-term storing as well as to medium- and long-term model rotting degradation caused by some chosen fungi identified at storing processes on the pile. For the model decay of chips under laboratory conditions during 3 or 6 weeks the white-rot fungi: Phanerochaete chrysosporium, Heterobasidion an...
R Solár, L Reinprecht, A Geffert, F Kacík


Proposal for a method aiming at the quantification of the impact of wood extraction in Life Cycle Assessment
1998 - IRG/WP 98-50113
Life Cycle Assessment has been accepted as an instrument for the assessment of the environmental impact of products. Characterisation factors for impact assessment of emissions from products have been established. To date no characterisation factor exists for the extraction of biotic resources, for example wood. Since the main disadvantage of using wood as a material lies in the extraction of reso...
P Esser, E Van der Voet


The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


Amenability of radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) as affected by aspects of cell ends in uniseriate ray parenchyma tissue
2003 - IRG/WP 03-40252
The principal objective of this article was to recognise and understand the amenability of ray parenchyma cell ends (end platform) in uniseriate ray tissue to influence the radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) by examination of most (Queen Charlotte Islands in Rhondda, South Wales) and the least (South Oregon in Dalby, North-East England) seed origins that grown in ...
I Usta, M D C Hale


Correlation between modulus of elasticity, mass losses and FTIR spectra of copper treated decayed wood
2006 - IRG/WP 06-10580
The composition of copper-based preservatives will change from copper-chromium to copper-ethanolamine, due to environmental demands. The most important drawback of copper-impregnated wood is the presence of tolerant fungal organisms that have developed an ability to degrade such preserved wood. In order to elucidate these processes, specimens (0.5×1.0×15 cm) made of Norway spruce (Picea abies) w...
M Humar, B Bucar, F Pohleven


Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso


Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


Wood furfurylation process development. Part 1: Oscillating Pressure Method
2007 - IRG/WP 07-40376
Furfurylated wood (wood modified by furfuryl alcohol) has over the last years gained marked shares from both tropical wood and conventional preservative treated wood and this has, in turn, generated several research projects concerning process development. The impregnation of spruce is well known from literature to be a difficult task. Furthermore, the sapwood of Scandinavian-grown Scots pine is a...
E Larnøy, M Westin, B Källander, S Lande