IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 181 documents. Displaying 25 entries per page.


Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


Improvement of wood properties by impregnation with liquefied spruce bark based resins
2016 - IRG/WP 16-40761
In this paper, biobased phenolic thermosetting resins are designed to be used as wood stabilization treatment. The originality of the study stands in substituting part of phenol by spruce (picea abies) bark: this is achieved by a liquefaction process in phenol in the presence of sulfuric acid as catalyst. Next, thermosetting resins are synthetized from liquefied bark by condensation on formaldehy...
X Duret, E Fredon, E Masson, P Gérardin


Status of the research and development of a new preservative system (EFPL) for pressure treatment of spruce in Canada
1975 - IRG/WP 348
Our work has been to develop a system which would have the stability of the ACA system and the formulation flexibility of the CCA system enabling properties such as fixation of arsenic, water repellency, appearance and cost to be controlled. Our permeability studies of spruce using a method previously developed indicated that an ammoniacal solution of copper arsenate is an excellent candidate for ...
J Rak, M R Clarke


Comparison of cubic and plug samples for preparation and data assembly in permeability study
2000 - IRG/WP 00-20197
In order to determine if plug experimental samples (PES: 30 x 15 mm2 diameter) could be used for inspection of wood permeability characteristics, radial and longitudinal flow directions were prepared according to either PES or cubic experimental samples (CES: 100 x 20 x 20 mm3) from the sapwood zone of Sitka spruce and treated by tanalith-C according to full-cell process. Results from the two prep...
I Usta


Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter


Spruce lumber treatments with ammoniacal solutions of inorganic preservatives
1977 - IRG/WP 391
As a part of our work in the Wood Preservation group at the Eastern Forest Products Laboratory in Ottawa to facilitate exploitation of spruce, which is a large timber resource in Canada, we have been studying the treatability of spruce roundwood. A report on this subject was presented to this group last year. More recently, another commodity - spruce timber - has been rapidly gaining the interest ...
R Rak


Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


The influence of formulation on the behaviour of LOSP's during industrial impregnation of spruce
1986 - IRG/WP 3387
Evidence is presented that the comparative behaviour of two LOSP formulations during impregnation treatment of spruce cannot be predicted purely on the basis of their physical characteristics (viscosity, surface tension and contact angle) nor on the extent of their 'passive' penetration into pine sapwood....
L D A Saunders, D M Zuvencko


Evaluation of Barrier Wrap Systems after 71 Months of Exposure
2013 - IRG/WP 13-40631
A 71 month study of the performance of booted samples in ground contact was conducted in AWPA hazard zone 4. Data indicated that excellent performance of wrapped systems, even over untreated wood, could be obtained. Instances of decay colonization or termite attack could all be attributed to some breaking of the integrity of the barrier system. Good performance for treatment below ground contact...
H M Barnes, M G Sanders, G B Lindsey, C McIntyre


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


Above ground performance of CCA-treated fingerjointed lumbe
1993 - IRG/WP 93-40003
Studs made from short lengths by finger jointing are becoming more commonly used in North America. Recently Forintek has received enquiries about the performance of such material in a treated form. Treated and untreated nominal 2x4 inch² spruce-pine-fir (SPF) studs exposed above ground for 12 years in southwestern British Columbia were evaluated for evidence of decay. Despite shallow preservative...
P I Morris, G E Troughton


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 5. Treatment of Sitka spruce and Scots pine
1999 - IRG/WP 99-40136
The suitability of the MPP Process for CCA treatment and accelerated fixation of species other than Radiata pine was assessed by pilot plant trials on UK-grown Sitka spruce (Picea sitchensis) and Scots pine (Pinus sylvestris). Pressure and vacuum kickbacks of spruce (14 l/m3) and Scots' pine (122 l/m3) were both substantially lower than that generated during treatment of radiata pine (369...
M E Hedley, K Nasheri, G Durbin


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Antifungal activity of a stilbene glucoside from the bark of Picea glehnii
2001 - IRG/WP 01-10402
Stilbene glucosides are widely distributed as phenolic extractives in the bark of Picea glehnii, a commercially species planted in the northern area of Japan, and its content reaches to more than 10% by the dried weight of the bark. Although antifungal activities of these compounds have been reported, the mechanism of growth inhibition is still unclear. Isorhapontin (5,4'-dihydroxy-3&...
S Shibutani, M Samejima


The effects of density on vertical variation of permeability of Sitka spruce within tree
2000 - IRG/WP 00-40156
Tree improvement of Sitka spruce is a combination of silviculture and tree breeding aimed at producing higher quality products including increased growth rate and timber yield, and wood density. It is useful to know annual ring structure and density distribution when studying the quality of wood, grading it, or determining how the wood structure affects residual flow in softwoods. Since density is...
I Usta.


Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates


In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie


CCA component distribution in the heartwood of treated lodgepole pine and white spruce
1998 - IRG/WP 98-30173
As part of a comprehensive study on the influence of drying on heartwood permeability, the distribution of copper, chromium and arsenic (CCA) in lodgepole pine (Pinus contorta Dougl.) and white spruce (Picea glauca (Moench) Voss.) heartwood was examined with light microscopy. Stained microtomed sections were examined to determine the penetration pathway for the CCA. The microscopic observations re...
Y An, J N R Ruddick, P I Morris


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Next Page