Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Alternatives to CCA-treated Pinus radiata as vineyard posts
2004 - IRG/WP 04-50212
An estimated 10 million trellis posts per year are used in Australian vineyards and about 75% of these are CCA-treated Pinus radiata. CCA-treated Pinus radiata posts are brittle and at times in short supply. Use of some products containing CCA is being restricted in Australia. Recently, plantation forestry has expanded rapidly for disposal of industrial and irrigation wastewater. Thinnings from th...
M Mollah, J Smith, K McCarthy, L J Cookson


Characterization of Poria indoor brown-rot fungi
1995 - IRG/WP 95-10094
The heterogeneous group of "Poria" fungi causing brown rot in buildings and also of wood in ground contact comprises Antrodia vaillantii, Antrodia serialis, Antrodia sinuosa, Antrodia xantha and Tyromyces placenta. These fungi have similar morphological appearance and biology. Their nomenclature has a confusing history and is still not uniform. As a consequence, misinterpretations may occur. SDS p...
O Schmidt


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


Surface characteristics of wood treated with various AAC, ACQ and CCA formulations after weathering
1991 - IRG/WP 2369
Wood samples treated with various alkylammonium compounds (AACs) as well as ammoniacal copper quat (ACQ) and chromated copper arsenate (CCA) have been studied in accelerated weathering experiments. Microscopic examination of the surfaces of these samples after exposure in a weatherometer revealed several different changes. Samples treated with didecyldimethyl ammonium chloride (DDAC) show consider...
L Jin, K J Archer, A F Preston


Moisture distribution in coated wooden panels. Studies of moisture dynamics by computerized axial tomography
1992 - IRG/WP 92-2413
Certain modern coatings have been held responsible for the rot damages in wood sidings, which have, during the past few years, appeared at an increasing extent in Scandinavia and which have occurred rather soon after the application of the coating. In this study, the moisture excluding effect of different coating systems intended for sidings have been studied with the help of an X-ray technique, c...
J Ekstedt, L O Lindgren, S Grundberg


FTIR characterization of copper ethanolamine - wood interaction
1999 - IRG/WP 99-20154
The interaction of copper ethanolamine (Cu-EA) and wood components was studied by using Fourier transform infrared spectroscopy (FTIR). In Cu-EA treated wood, significant reduction was noticed on the band attributed to carbonyl vibration from carboxylic groups at 1735±5 cm-1 and an increase in band intensity was obtained from carbonyl in carboxylate at 1595±5 cm-1. The same observation was made ...
Jun Zhang, D P Kamdem


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Characterization and differentiation of wood rotting fungi by protein and enzyme patterns
1999 - IRG/WP 99-20177
Standardized tests for wood preservatives are performed with defined fungal strains to ensure comparability between laboratories. However, changes of virulence and variation of results are well known events. Suitable and reliable measures to control the stability of the test organisms are necessary.Comparison of protein patterns produced by SDS-electrophoresis was already described by several auth...
U Schoknecht


Isolation and characterization of hydroxyl-radical-producing glycopeptide genes from the white-rot basidiomycete Phanerochaete chrysosporium
2006 - IRG/WP 06-10588
During wood decay, the white-rot basidiomycete Phanerochaete chrysosporium secretes low-molecular-weight glycopeptides that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radical. This reaction accounts for most of the hydroxyl radical produced in wood-degrading cultures of P. chrysosporium. In combination with phenol oxidases, hydroxyl radical is believed to play a r...
H Tanaka, G Yoshida, Y Baba, K Matsumura, S Itakura, A Enoki


Molecular characterization of M’jej, decaying agent of cedar forests in Morocco
2006 - IRG/WP 06-10593
Cedar wood is well appreciated since thousand years even though its economical importance is limited because of its world distribution restricted to some Mediterranean countries and Himalaya. The most important species, Cedrus atlantica have its biggest population in Morocco (130 000 ha) where it is submitted to fungal diseases. Among them, the locally named “M’jej” reduced notably saw mile ...
A Zaremski, S Bakkali-Yakhlef, C Chaintreuil, Y Abbas, Y Prin, M Abourouh, M Ducousso