Surface accumulation of copper on CCA-impregnated Pinus patula stakes during marine preservative trials in the southern hemisphere
1992 - IRG/WP 92-4181
Pinus patula stakes treated with CCA to target retentions of 30 kg/m³ salts were exposed to sea water in marine and estuarine ecosystems off the coast of Southern Africa for two years. Samples were then analysed for copper and arsenic. Analysis of samples from the marine ecosystem showed (IRG/WP/4167) that arsenic was longitudinally and transversely leached from the wood, whereas the copper was r...
G D Shelver, C D McQuaid, M Tarin, A A W Baecker


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Wood surface pretreatments with metal tannates
1989 - IRG/WP 3552
The sequential application of aqueous solutions of tannins derived from radiata pine bark and water-soluble metal salts was examined as a means of improving the water repellency of wood surfaces. Nine metal salts were screened in combination with tannin solutions and, based on water repellency of pretreated filter paper, four were selected for further study. The two-step application of tannin solu...
D V Plackett, D R Cronshaw


Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Alternatives to CCA-treated Pinus radiata as vineyard posts
2004 - IRG/WP 04-50212
An estimated 10 million trellis posts per year are used in Australian vineyards and about 75% of these are CCA-treated Pinus radiata. CCA-treated Pinus radiata posts are brittle and at times in short supply. Use of some products containing CCA is being restricted in Australia. Recently, plantation forestry has expanded rapidly for disposal of industrial and irrigation wastewater. Thinnings from th...
M Mollah, J Smith, K McCarthy, L J Cookson


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


Surface characteristics of wood treated with various AAC, ACQ and CCA formulations after weathering
1991 - IRG/WP 2369
Wood samples treated with various alkylammonium compounds (AACs) as well as ammoniacal copper quat (ACQ) and chromated copper arsenate (CCA) have been studied in accelerated weathering experiments. Microscopic examination of the surfaces of these samples after exposure in a weatherometer revealed several different changes. Samples treated with didecyldimethyl ammonium chloride (DDAC) show consider...
L Jin, K J Archer, A F Preston


Moisture distribution in coated wooden panels. Studies of moisture dynamics by computerized axial tomography
1992 - IRG/WP 92-2413
Certain modern coatings have been held responsible for the rot damages in wood sidings, which have, during the past few years, appeared at an increasing extent in Scandinavia and which have occurred rather soon after the application of the coating. In this study, the moisture excluding effect of different coating systems intended for sidings have been studied with the help of an X-ray technique, c...
J Ekstedt, L O Lindgren, S Grundberg


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


CCA-treated Wood Disposed in Landfills and Life-cycle Trade-Offs With Waste-to-Energy and MSW Landfill Disposal
2005 - IRG/WP 05-50231
CCA-treated wood as a solid waste is managed in various ways throughout the world. Although some wood is combusted for the production of energy in the U.S., more often than not, CCA-treated wood is disposed in landfills. In other countries, wood, often including CCA-treated wood, is combusted for the production of energy. This paper is presented in two parts. Part I evaluates the impact of CCA-tre...
J Jambeck, K Weitz, T G Townsend, H M Solo-Gabriele


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek