Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


CCA-treated Wood Disposed in Landfills and Life-cycle Trade-Offs With Waste-to-Energy and MSW Landfill Disposal
2005 - IRG/WP 05-50231
CCA-treated wood as a solid waste is managed in various ways throughout the world. Although some wood is combusted for the production of energy in the U.S., more often than not, CCA-treated wood is disposed in landfills. In other countries, wood, often including CCA-treated wood, is combusted for the production of energy. This paper is presented in two parts. Part I evaluates the impact of CCA-tre...
J Jambeck, K Weitz, T G Townsend, H M Solo-Gabriele


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Characterization and differentiation of wood rotting fungi by protein and enzyme patterns
1999 - IRG/WP 99-20177
Standardized tests for wood preservatives are performed with defined fungal strains to ensure comparability between laboratories. However, changes of virulence and variation of results are well known events. Suitable and reliable measures to control the stability of the test organisms are necessary.Comparison of protein patterns produced by SDS-electrophoresis was already described by several auth...
U Schoknecht


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Isolation and characterization of hydroxyl-radical-producing glycopeptide genes from the white-rot basidiomycete Phanerochaete chrysosporium
2006 - IRG/WP 06-10588
During wood decay, the white-rot basidiomycete Phanerochaete chrysosporium secretes low-molecular-weight glycopeptides that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radical. This reaction accounts for most of the hydroxyl radical produced in wood-degrading cultures of P. chrysosporium. In combination with phenol oxidases, hydroxyl radical is believed to play a r...
H Tanaka, G Yoshida, Y Baba, K Matsumura, S Itakura, A Enoki


Molecular characterization of M’jej, decaying agent of cedar forests in Morocco
2006 - IRG/WP 06-10593
Cedar wood is well appreciated since thousand years even though its economical importance is limited because of its world distribution restricted to some Mediterranean countries and Himalaya. The most important species, Cedrus atlantica have its biggest population in Morocco (130 000 ha) where it is submitted to fungal diseases. Among them, the locally named “M’jej” reduced notably saw mile ...
A Zaremski, S Bakkali-Yakhlef, C Chaintreuil, Y Abbas, Y Prin, M Abourouh, M Ducousso


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


Preliminary Observations of the Effect of Kerfing on the Surface Checking and Warping of Flat Sawn Southern Pine Decking
2007 - IRG/WP 07-20360
Checking and warping of decking timber are serious defects and methods of reducing their severity are required to ensure that wooden decking can compete with alternative decking materials. Kerfing is effective at reducing the checking and distortion of square cross-section lumber, and the checking of roundwood. In the past it has also been applied to preservative treated decking boards, however, t...
R Ratu, J Weizenegger, P Evans


Electrokinetic Accelerated Ingress of Boron After Surface Treatment of Wood
2007 - IRG/WP 07-40372
In this work electrokinetic acceleration of boron penetration after surface treatment is proposed in order to offer an alternative to the often low penetration rates based on diffusion. Electrodialytic experiments showed that boric acid could be transported as negatively charged complexes with tartaric acid in aqueous solutions at pH 4-5. Boric acid could not be transported when tartaric acid was ...
I V Christensen


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


The Effect of Solar Radiation on the Surface Checking of Wood
2007 - IRG/WP 07-40356
The aim of this research was to investigate whether exposure to solar radiation increases the checking of wood exposed to the weather, and examine the causes and spectral dependency of such an effect. Lodgepole pine samples were exposed outdoors under filters which transmitted selected regions of the solar spectrum while allowing other weathering factors to act on samples. Surface checking in samp...
P Evans, K Urban