IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 771 documents. Displaying 25 entries per page.


Effects of the addition of polyethylene glycol to the CCA-C preservative treatment
1985 - IRG/WP 3337
A modification of the CCA-C wood preservative system for utility poles has been investigated to see if spur penetration into the poles is assisted during climbing. Addition of polyethylene glycol to the CCA system has been shown to accomplish this purpose. This paper addresses the effects of the addition of polyethylene glycol to other physical properties germane to utility poles....
W P Trumble, E E Messina


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


Electrokinetic Accelerated Ingress of Boron After Surface Treatment of Wood
2007 - IRG/WP 07-40372
In this work electrokinetic acceleration of boron penetration after surface treatment is proposed in order to offer an alternative to the often low penetration rates based on diffusion. Electrodialytic experiments showed that boric acid could be transported as negatively charged complexes with tartaric acid in aqueous solutions at pH 4-5. Boric acid could not be transported when tartaric acid was ...
I V Christensen


Thermal treatment of Nigerian-grown Albizzia zygia and Funtumia elastica wood in soy oil medium.
2008 - IRG/WP 08-40413
Thermal treatment in soy oil medium is one of the techniques used as a substitute to the chemical treatment in wood preservation. However, the effects of this technique vary from one species to another and hence the need to investigate the response of individual species to it. Thermal treatment of air-dried Nigerian-grown Albizzia zygia and Funtumia elastica wood was carried out in a vessel contai...
L Awoyemi


Changes in hygroscopic, mechanical and surface properties of Scottish-grown Sitka Spruce (Picea sitchensis) wood subjected to dry heat treatment
2008 - IRG/WP 08-40415
Heat-treatment is a wood modification method which has been used to some extent in improving timber quality. However, the main limitation in the use of this technique despite its numerous advantages is the adverse effects on the various properties associated with the use of wood as an engineering material. Dry heat treatment of Scottish-grown Sitka spruce (Picea sitchensis) wood was carried out at...
L Awoyemi, M C Jarvis, A Hapca


Differential response of wood to dry air thermal treatment (DATT) and soy oil thermal treatment (SOTT)
2009 - IRG/WP 09-40446
Thermal treatment is an alternative to chemical modification method which has been used to some extent in improving timber quality. In order to get the maximum benefits possible without compromising the various end-use quality requirements of timber, several possibilities have been and are still being investigated in relation to this technique. Clear wood samples (19 x 19 x 150mm) of kiln-dried re...
L Awoyemi


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


Formation of hydrophobic wood surface by means of thermal treatment and surface modification with alkyl ketene dimer (AKD)
2016 - IRG/WP 16-40738
One of the major shortcomings of wood-based materials compared to technical materials is attributed to their poor dimensional stability in changing climates and in contact with liquid water. Heat treatment induces chemical change with a consequent decreasing of reactivity of the material showing unwanted surface inactivation. Alkyl ketene dimer (AKD) is a widely used sizing agent in papermaking, w...
T Lovaglio, T Meints, L Todaro, W Gindl-Altmutter


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi


Plasma treatment of wood - a review of 15 years of research in Göttingen
2021 - IRG/WP 21-40913
Wood is an important renewable resource and can be found omnipresent in everyday life. Its natural properties offer numerous advantages regarding physical, mechanical but also aesthetic aspects, but also challenges that one has to address with various modification methods. Driven by the desire to promote the use of promising new technologies using plasmas, there has been a close research network ...
P Sauerbier, R Köhler, G Avramidis, W Viöl, H Militz


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Starch modified with silanes – high hydrophobic surface treatment for wood protection
2023 - IRG/WP 23-40981
The great potential of silanes for starch modification and their utility as surface wood protection is still not sufficiently assessed. The work aimed to analyze the crosslinking process's effect on starch modification with silane and tested the hydrophobic properties of surface-treated wood. The starch treatment was modified with methyltrimethoxysilane or N-octyltriethoxysilane. SEM-EDX with a cr...
W Perdoch, M Bajstok, B Mazela, I Siemińska, B Peplińska


Next Page