Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson
Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer
Critical moisture levels and mould resistance of five different wood treatments
2013 - IRG/WP 13-30632
Mould resistance of five different treatments were tested using two methods, a recently
developed method for the determination of critical moisture levels of building materials (RHcrit),
and ASTM D3273-94. The critical moisture level method exposed samples at 22 °C and 98, 92,
86 and 82% relative humidity (RH) for 12 weeks. ASTM D3273-94 was performed at 29 °C and
about 95% RH.
Treatments c...
G Bok, P Johansson, A Ekstrand Tobin, S Bardage
Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products.
In this study the efficacy of wood treated with micronized copper, zinc oxide and their
mixture was compared to that of wood treated with soluble amine copper oxide with
subterranean termites in a laboratory test. All of the formulations tested were effective in
controlling wood degradation by the term...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani
Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker
Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour
Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson
Is there a role for termite alates in colony expansion in Wisconsin?
2014 - IRG/WP 14-10820
Termite colonies in Wisconsin tend to be large and widely spread out geographically, and separated by distances up to 1342km. We recently completed a study to determine the genetic diversity and population substructure of thirteen existing colonies of Reticulitermes flavipes using amplified fragment length polymorphism to determine patterns of termite dispersal in Wisconsin. Measures of inbreedin...
F Green III, R A Arango, G R Esenther, T G Shelton
Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow
A comparison of the resistance of pyrethroid-treated wood to damage by Coptotermes acinaciformis in Australia and C. formosanus in China and the USA
2014 - IRG/WP 14-10830
Field trials, using a single aboveground method of exposure, were used to assess a range of retentions of two pyrethroids (bifenthrin and permethrin) in Pinus radiata D. Don sapwood against two species of Coptotermes in three countries to provide directly comparable results. Coptotermes acinaciformis (Froggatt) in Australia, C. formosanus Shiraki in China and C. formosanus in the USA consumed simi...
J Creffield, M Lenz, D Scown, T Evans, Junhong Zhong, B Kard, J Hague, K Brown, E Freytag, J Curole, R Smith, T Shupe
Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene
Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack).
In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi
Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz
Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo
Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann
Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram
The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals
Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar
Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers
Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker
Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke
Field trials results of preservative treated ground contact stake conducted in Korea
2014 - IRG/WP 14-30640
The field trials results from Korea preservative treated ground contact stake are reported. There was two site which was in southern area(Anmeon) and east area (Jungsun) of Korea. The CUAZ, CCA and CBHDO preservatives were use in this study. The sapwood of Japanese red pine stake was treated with these preservatives according to Korea standard method and then installed in 2003. Every year the insp...
Dong Won Son, Won Jung Hwang, Hyun-mi Lee, Dong-heub Lee, Sang-bum Park
Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture.
In this ...
G Köse, A Temiz, S Demirel, O E Özkan
Fire resistance of wood treated with potassium carbonate and silanes
2014 - IRG/WP 14-30657
This paper reports on the effect that organosilicon compounds and potassium carbonate and urea (PCU) have on wood flammability. The study focus on reducing wood flammability by promoting char formation through manipulation of the condensed phase decomposition chemistry. Potassium carbonate is known as an effective fire retardant, however it is easily leached out from wood and increases its hygrosc...
B Mazela, M Broda, W Perdoch
Resistance of fungal derived pigments to ultraviolet light exposure
2014 - IRG/WP 14-30642
The potential for using fungal derived pigments as surface treatments for limiting photodegradation of wood was investigated. Extracts from Chlorociboria aeruginosa and Scytalidium cuboideum were compared with a traditional aniline dye and chromic acid treatment. Hybrid poplar sapwood samples treated with these solutions were exposed to 86.4 kj/m2 of UV radiation and assessed for lignin degradatio...
H G Beck, S Freitas, G Weber, S C Robinson, J J Morrell