Your search resulted in 761 documents. Displaying 25 entries per page.
Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh
Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson
Some tests on ES - AS 11, a novel anti-sapstain formulation, and its properties
1987 - IRG/WP 3399
The results of some tests with the formulation ES - AS 11 are given. The formulation is an attempt to improve the performance of an anti-sapstain chemical by: 1) increasing its penetrability 2) uniquely combining its active ingredients. Very short times of treatment (dipping not longer than 5 seconds), low concentrations of active ingredients, and lower toxicological and environmental risks may be...
U Straetmans
Final proposals for collaborative work on laboratory soft rot testing
1987 - IRG/WP 2292
In this paper proposals are made to scope, timbers, preservatives, leaching, drying, soil type, moisture content, soil burial (blocks and stakes), incubation and dry weight determination and the expression of results....
D J Dickinson, S M Gray
Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell
Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne
The use of image analysis to quantify soft rot decay
1992 - IRG/WP 92-2410
Image analysis techniques can provide quantitative information from visual images. As part of a wider interest in decay assessment methods we have investigated the application of image analysis techniques for quantifying soft rot decay by Chaetomium globosum in transverse sections of birch wood and bamboo. A method for reducing contamination of the section (and image) by the fungal hyphae and of s...
P J Wickens, R J Murphy
Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch
Co-operative field experiment. Performance of preservative-treated hardwoods with particular reference to soft rot: Report of condition of specimens installed in Victoria, Australia
1978 - IRG/WP 3118
J Beesley
Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth
Documentation on Merulius (Serpula) lacrimans (Wulf.) Fr. according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1972 - IRG/WP 108
J Segmüller, O Wälchli
A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton
Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen
Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability.
Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek
Proposals for a field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot
1975 - IRG/WP 342
It is proposed to treat a series of hardwood stakes in the UK and install them in different sites around the world. The stakes will include 3 reference species common to every site and 2 locally selected species. The hazard of termites should be avoided in order to limit the study to action of micro-organisms....
D J Dickinson
Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson
Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris
The dry rot and other fungi in houses. Part 4
1995 - IRG/WP 95-10124
J Bech-Andersen
The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari
Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel
The use of the Pilodyn for detecting soft-rot decay in CCA treated eucalypt poles
1986 - IRG/WP 2251
A 6 Joule Pilodyn unit with 2.5 mm diameter pin was used to inspect CCA treated eucalypt poles, suspected of suffering groundline soft-rot decay. Pole plugs were removed at the inspection region and the amount of soft-rot decay present determined microscopically. High correlation (R² = 0.73) was obtained between the amount of soft-rot and Pilodyn pin penetration. The Pilodyn is recommended as a u...
L E Leightley, G A Willoughby
The effect of treatment temperature on the biological performance of CCA treated wood
1990 - IRG/WP 3624
Birch and Scots pine sapwood blocks were treated with several concentrations of CCA at three different temperatures: 5, 20 and 35°C. The treated wood was maintained at the appropriate temperature for the fixation period. Leached and unleached samples were then exposed in a soft rot monoculture test using Chaetomium globosum and a brown rot monoculture test using Coniophora puteana. The treatment ...
S M Gray
Analysis of volatile emissions as an aid in the diagnosis of dry rot
1992 - IRG/WP 92-2393
The dry rot fungus, Serpula lacrymans was grown in pure culture on malt extract and on sapwood of pine. The volatile compounds emitted from the cultures were determined by diffusion sampling on tubes filled with Tenax TA, thermal desorption and gas-chromatography-mass-spectrometry in order to find markers for attack of the fungus....
J Bjurman, J Kristensson
Monographic information on Serpula incrassata (Berk. and Curt.) Donk
1980 - IRG/WP 1128
J G Palmer, W E Eslyn
Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel