Your search resulted in 3254 documents. Displaying 25 entries per page.
How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent.
The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen
Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States.
The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...
J Habicht, D Häntzschel, J Wittenzellner
Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez
Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt
Effect of water repellents on leaching from CCA treated wood
1995 - IRG/WP 95-50044
CCA treated fence boards brushed with a water repellent finish had consistently lower leaching losses of all CCA components compared to the rate for matched samples without the water repellent. These results are after 12 cycles of simulated rainfall in the laboratory (1800 mm rainfall total) and four months of natural rain exposure in Toronto....
P A Cooper, R MacVicar
Studies on accelerated ageing procedures with TBTO-treated wood
1985 - IRG/WP 2244
The efficacy of various procedures for accelerated ageing of organotin based wood preservatives in treated wood has been investigated. It was found that leaching of the treated wood samples in water according to the European Standard EN 84 was not satisfactory for organotin based preservatives and is probably also unsuitable even for other types of organic solvent preservatives. Keeping tributylti...
J Jermer, M-L Edlund, B Henningsson, W Hintze
Use of vermiculite as substrate in assays on phytotoxicity of treated wood
1989 - IRG/WP 3547
It is considered the possibility of using vermiculite instead of soil as substrate in assays on phytotoxicity of wood treated with preservatives for agricultural use. Three organic preservatives were used. It had been tested the behaviour of both, vermiculite and soil in case of preservative leaking due to a leach. So that, assays of germination with cucurbitaceous were carried out, mixing a dose ...
M V Baonza Merino, D Franco
Accelerated ageing of preservatives in treated wood
1988 - IRG/WP 3476
New preservatives are tested in the laboratory and often in field tests before they are used commercially. Some preservatives, however, tested in the laboratory do not show the expected stability when used in service. The differences between laboratory tests and practical use can never be completely eliminated but must be minimized as far as possible by relevant testing methods. Studies of the eff...
M-L Edlund, B Henningsson, B Jensen, C-E Sundman
Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland
Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina
Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman
Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent
Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk
Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda
Wood preservation and the environment: A Canadian perspective
1990 - IRG/WP 3577
The non-pressure (surface) and pressure treatment of wood impacts on the environment in four ways. These are: through the production of treated wood at sawmills and pressure treating facilities; during the storage of treated wood prior to use; when the pressure treated wood is placed in service; and finally, when the treated product reaches the end of its useful life and must be disposed. By refer...
J N R Ruddick
How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek
Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric
The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel
EPR investigations of interactions between ammoniacal Cu(II) octanoate and wood
1996 - IRG/WP 96-30110
Ammoniacal solutions of copper(II) octanoate [ C u . h l f . 2 . r h l f.(O2CC7H15)4], interactions of these solutions with wood and wood components, and leaching of copper(II) octanoate from impregnated wood samples, have been studied by electron paramagnetic resonance (EPR) method. It is still not clear if in the Cu(II) octanoate - water - ammonia system, Cu(II) remains in a (copper(II) octanoat...
F Dagarin, M Petric, F Pohleven, M Sentjurc
Leaching of chromium and other cca components from wood-cement composites made with spent CCA treated wood
2000 - IRG/WP 00-50153
Wood cement composites are an attractive option for recycling spent treated wood, since the CCA treatment enhances the physical, mechanical and biological resistance properties of the composite. However, we have noted a higher than normal leaching of chromium from these products and this appears to result from conversion of some of the trivalent chromium to the more leachable and toxic hexavalent ...
D Qi, P A Cooper
Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek
Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper
The effect of treatment temperature on the biological performance of CCA treated wood
1990 - IRG/WP 3624
Birch and Scots pine sapwood blocks were treated with several concentrations of CCA at three different temperatures: 5, 20 and 35°C. The treated wood was maintained at the appropriate temperature for the fixation period. Leached and unleached samples were then exposed in a soft rot monoculture test using Chaetomium globosum and a brown rot monoculture test using Coniophora puteana. The treatment ...
S M Gray
Laboratory simulation of leaching from creosote treated wood in aquatic exposures
2000 - IRG/WP 00-50157
Creosote has a long history of use as a preservative particularly in industrial wood products, but its use has come under increasing scrutiny as a result of concerns about its potential effects on aquatic and terrestrial non-target organisms. Despite its long use, there is relatively little data on the rates of creosote loss in many exposures. In this report, we describe small scale leaching tank ...
Ying Xiao, J Simonsen, J J Morrell
Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey