IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3511 documents. Displaying 25 entries per page.


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Depletion of wood preservatives after four years' marine exposure in Mt. Maunganui harbour, NZ
1994 - IRG/WP 94-50036
This paper reports on chemical analysis of marine test samples exposed in Mt. Maunganui harbour, New Zealand from 1977 to 1981. Depletion data for a Class II CCA, a CCA-A formulation, acid copper chromate and ammoniacal copper arsenate are presented. The results suggest differences in the rate of loss of individual preservative components among the four formulations and redistribution of individua...
K J Archer, A F Preston, C M Chittenden, D R Page


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


Comparative evaluation of the barrier effect against Hylotrupes bajulus L. of different types of wood preservative
1986 - IRG/WP 1307
This paper settles the difference of contact action against females of Hylotrupes bajulus the likelihood of egg-laying, the ovicide effect and the hazards of development of newly hatched larvae between some preservatives belonging to three differents types: mineral waterborne products, organic products and emulsions. The results show that against females, the action is fast with organic products, ...
M-M Serment


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


Report of field test results for dichloro-n-octyl-isothiazolone: A potential new wood preservative
1988 - IRG/WP 3495
In a previous report (IRG/WP/3306) we presented preliminary laboratory test results on 4,5-dichloro-2-n-octyl-4-isothiazolone (RH 287). Laboratory data indicated toxic threshold values for RH 287 ranging from 0.37 to 0.50 kg/m³. In this report we present field test results on an IRG L-joint test and an in-ground stake test for RH 287, pentachlorophenol and biocide free test units. (a) L-joint tes...
D E Greenley, B M Hegarty


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


The formation of organotin carboxylates in bis(tributyltin) oxide - treated Pinus sylvestris sapwood
1990 - IRG/WP 3618
Tributyltin compounds have been successfully used for many years as wood preservatives, although their chemical nature in timber have not been fully elucidated. This study by 119Sn and 13C NMR spectroscopy has shown that, on impregnation into Pinus sylvestris sapwood, bis(tributyltin) oxide, (Bu3Sn)2O, is rapidly converted to tributyltin carboxylates, Bu3SnOCO·R, via reaction with components of t...
S J Blunden, R Hill


Oxygen index levels and thermal analysis of wood treated with melamine-formaldehyde-boron combinations
1997 - IRG/WP 97-30135
Melamine formaldehyde (MF) resin was impregnated into scots pine (Pinus sylvestris L.) specimens with aqueous solutions of 5, 10 and 20% concs. Boric acid (BA) and borax (BX) was added to MF resin at the concentration levels of 0.25, 1.00 and 4.70% to each level of resin concs. BA and BX mixture was prepared at the 5:1 (w/w) ratio considering resultant pH of solutions and better fire resistance. U...
M K Yalinkilic, W-Y Su, Z Demirci, E Baysal, M Takahashi, S Ishihara


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


Laboratory fumigations to determine the minimum temperature for methyl bromide eradication of the oak wilt fungus in red oak
1983 - IRG/WP 3243
Laboratory chamber fumigations of naturally-infected ret oak log sections exterminatet the oak wilt fungus in sapwood at temperatures down to 0°C. Only low, sporadic fungus survival was observed when log sections were gassed with methyl bromide at -5°C and aired for 4 da. at 0°C. Lower temperature treatments were not effective even if gas levels or exposure times were increased by 50%....
E L Schmidt


Kinetic modelling of adsorption of quaternary ammonium compounds by Scots pine wood sawdust (Pinus sylvestris L.)
2005 - IRG/WP 05-30369
The adsorption of new quaternary ammonium compounds from aqueous solutions onto Scots pine wood (Pinus sylvestris L.) sawdust was studied. The pseudo first- and second- order kinetic models were used for the mathematical description of the sorption dynamic process of QACs onto wood. The highest correlation coefficients were obtained for the pseudo-second order kinetic model, those suggest that che...
J Zabielska-Matejuk


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1977 - IRG/WP 288
G Castan


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Differences in feeding activity among colonies of Formosan subterranean termite Coptotermes formosanus Shiraki
1983 - IRG/WP 1202
Feeding activities of 7 colonies of the Formosan subterranean termite, Coptotermes formosanus Shiraki, were examined. Wood-consumption rates among colonies differed significantly, ranging from 23.80-78.48 mg/g/day. This large intraspecific variation raised a question of whether differences in feeding activity reported for other termite species were due to interspecific differences. When rates were...
N-Y Su, J P La Fage


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz