Your search resulted in 3468 documents. Displaying 25 entries per page.
Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel
Respiration measurement of dry-rot
1995 - IRG/WP 95-10095
Methods for measuring the production of carbondioxide from wood infected with the dry-rot fungus were evaluated. By enclosing whole wood blocks and measuring the concentration of gas in the headspace by gas chromatography, an exponential increase in the concentration of CO2 was observed for at least 2 months. This technique could therefore present a method for evaluating various treatments of dry-...
L Toft
Targeted inhibition of wood decay (Using everything but the kitchen sink)
1997 - IRG/WP 97-10203
Low molecular weight oxidative decay agents have been implicated in the degradation of wood by brown-rot decay as evidenced by chemical analysis of brown-rotted wood and detection of oxalic acid and hydroxy radicals. Fenton chemistry (H2O2 / Fe++) is often proposed as the mechanism for generating hydroxy radicals. Previous authors have shown iron to enhance the brown-rot hydrolysis of wood, while ...
F Green III, T A Kuster, T L Highley
The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams
Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki
Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki
Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz
Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven
Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz
The role of oxidation in wood degradation by brown-rot fung
1992 - IRG/WP 92-1562
Brown-rot fungi are suggested to degrade cellulose by oxidation with hydrogen radicalsformed eg. in the conversion of hydrogen peroxide in the Fenton type reactions. The stuctural changes in the holocellulose in wood induced by Fenton's reaction on wood components are very similar to those caused by brown-rot fungi. In this work the effect of the Fenton reaction on wood components was stu...
A-C Ritschkoff, J Pere, J Buchert, L Viikari
Identification of brown rot fungi on wood in above ground conditions by PCR, T-RFLP and sequencing
2004 - IRG/WP 04-10512
Fungi selected in test fields in Germany and Estonia and fungi (Coniophora puteana) cultivated on medium have been identified by the molecular methods PCR (Polymerase Chain Reaction), T-RFLP (Terminal Restricted Fragment Length Polymorphism) and sequenced to species level. The samples from the German field test showed that the fruit body sample was a different fungus than from the mycelium sample....
U Råberg, N Högberg, C J Land
Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell
Preliminary studies of the performance of iron chelators as inhibitors of brown rot (Coniophora puteana) attack
1996 - IRG/WP 96-10185
This paper describes experiments to examine the proposal that the presence of iron is essential for brown rot fungi to utilize hydroxyl radicals remote from the hyphae as a means of converting the wood into a food source. reliminary test results are presented from trials using three different iron chelators impregnated into Scots pine (Pinus sylvestris) sapwood blocks. Their relative effects on th...
E D Suttie, R J Orsler, P M Wood
Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky
European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use
are waited to valid the progra...
Anonymous
Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher
The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh
The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached
for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee
Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner
Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner
Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster
Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson
Soft-rot in Tabebuia sp. wood used in water cooling tower:
identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius
Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler
Decay resistance of Siberian larch wood against brown rot fungus. - Part 3. The variation between plus trees and their grafted clones
2000 - IRG/WP 00-10350
The aim of the study was to estimate the variation in the decay resistance of Siberian larch (Larix sibirica Ledeb.) wood using mature plus trees and their grafted clones. Samples were collected with an increment core borer from 11 original plus trees and their 25-year-old grafted seed orchard clones. A typical brown rot fungus, Coniophora puteana (Schum. ex Fr.) Karst. (BAM Ebw. 15), was used as ...
H Viitanen, L Paajanen, M Venäläinen, A Harju, P Velling