Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


A report of the Technical Recommendations documents for the Canadian Wood Protection and Preservation Facilities and an environmental study of storm water runoff from anti-sapstain treatment plants
1988 - IRG/WP 3478
With the completion of the Final draft of the Technical Recommendations (TR) documents for the Wood Preservation and Wood Protection Industry, there are naturally questions on what is expected from these documents and how Environment Canada and Provincial regulatory agencies may interact with the wood preservation industry. In general, it is expected that the Canadian Wood Preservation and Protect...
G Das, V N P Mathur


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


An appraisal of anti-sapstain chemicals in Queensland, Australia
1985 - IRG/WP 3331
Eleven formulations were tested in the field for effectiveness against sapstain, mould and fungi on Pinus elliottii in Queensland. The commercially used sodium pentachlorophenoxide (0.5% a.i.) and Captafol (0.2% a.i.) performed well. Busan 1009 (0.3% a.i.), Protek T (5.0% a.i.), Woodgard E.S. and E.C. (0.8% a.i.), together with sodium tetrachlorophenoxide (0.5% a.i.) offer potential as anti-sapsta...
L E Leightley


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


The effect of stack height on the performance of preservatives used for the prevention of sapstain on seasoning wood
1997 - IRG/WP 97-10192
The performance of three anti-sapstain preservatives was investigated under field conditions in south east England. The preservatives under test were: copper-8-quinolinolate (Mitrol PQ8) trimethylalkylammoniumchloride and sodium hexanoate (Sinesto B) and chlorothalonil (Tuff Brite). The preservatives were tested on Corsican Pine grown in south east England. The field trial was set up to investigat...
J R Williams, D J Dickinson, J F Webber


Protection of pine sawtimber and sawn timber against blue stain in Poland
1983 - IRG/WP 3193
The purpose of this paper is the synthesis of more important results of basic and applied research that have been grouped in the following problems: 1.: Fungi causing blue stain in the pine wood, occurring in Poland. 2.: Moisture content changes of pine sawtimber and sawn timber as the factor of blue stain producing fungi development. 3.: Effect of sapwood moisture content on the degree of wood st...
E Tarocinski, M H Zielinski


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Effect of the Storage Time of Logs in Anti-Stain Treatment Effectiveness
2016 - IRG/WP 16-30683
Storage of green lumber, for 7 months, operationally treated with anti-stain products, depending on the storage time of the logs (10, 20 and 30 days) post harvesting allows to affirm that with increasing storage time of the logs, occurs a progressive increase in intensity, severity and types of fungi present in the logs. It is further noted, a significant increase in the percentage of sawn lumber ...
M A Peredo, C Barria


Which fungi cause sapstain in Canadian softwoods?
1998 - IRG/WP 98-10285
The Canadian forest products industry suffers considerable losses in revenue due to fungal stains. There is an increased awareness that more complete knowledge about the causal organisms might help solve the problem. A first step was to initiate a thorough survey of bluestain fungi in Canada. Systematic sampling was done at seven selected sawmills in six Canadian provinces. In summer 1997 fresh lo...
A Uzunovic, Dian-Qing Yang, P Gagné, C Breuil, L Bernier, A Byrne


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli