IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 22 documents.


An evaluation of the potential of ion mobility spectrometry for detection of organic wood preservative components in solutions and treated wood
1994 - IRG/WP 94-20038
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Until now, no highly sensitive rapid analytical methods are available for the detection of wood preservatives under industrial process conditions. Preliminary experiments showed that Ion Mobility Spectrometry (IMS) could be a promising method for rapid detection of organic preser...
A Voss, J N R Ruddick, W J Homan, H Militz, H Willeitner


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States. The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...
J Habicht, D Häntzschel, J Wittenzellner


Comparison of Different Methods for Assessing the Performance of Preservatives in the BAM Fungus Cellar Test
1998 - IRG/WP 98-20149
The fungus cellar test is a common means to get reliable data on the long term performance of treated wood in soil contact. A constantly high humidity and a suitable of water holding capacity for a range of micro-organisms provide high decay rates in untreated wood and produce intensive microbial pressures on wood treated with biocides. Presently a range of biocides are under test in the BAM fungu...
I Stephan, M Grinda, D Rudolph


Leaching of Active Components from Preservative Treated Timber. Stage 1: Semi-Field Testing
2004 - IRG/WP 04-20302
The project is aiming at finding realistic leaching rates from preservative-treated wood in use class 3 (above ground). The project focuses on developing a field trial method for investigating leaching. Panels are subjected to outdoor exposure under natural weather conditions at a test field at the Danish Technological Institute. The leachate is collected and monitored by chemical analysis of the...
N Morsing, B Lindegaard


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Inorganic wood preservative levels in soil near a noise barrier treated with different preservatives after 8 years in service
2005 - IRG/WP 05-50234
In March 1996 nine test sections of a noise barrier were installed near Stockholm Sweden. The test sections include untreated Scots pine, spruce and larch and Scots pine, treated with different wood preservatives. After 8 years in service, the untreated spruce, pine and larch boards in contact with the soil were significantly decayed, with an estimated service life of about 5-10 years, while the u...
P A Cooper, Y T Ung, M-L Edlund, J Jermer, O Söderström


Treatment of precut timbers
1991 - IRG/WP 3665
A serious lack of house construction technicians has produced a trend in which wooden parts of a house are processed by computer aided precut machine and the precut wood is treated with termiticides and/or fungicides at the plant site. We have developed a new system to handle these requirements of homebuilding. This system is a combination of incising machine, spray machine and proprietary oil-bor...
K Nishimoto, Y Kuwasuru


Health hazards and environmental aspects when using Cu-HDO-containing wood preservatives in vacuum pressure plants
1993 - IRG/WP 93-50001-11
Apart from the biological efficacy of wood preservatives, the health and environmental aspects concerning the utilisation of wood preservatives, the use of treated timber and the disposal of impregnated wood are of high significance today. Therefore, information on a possible aerial concentration of wood preservatives, on the mobility of active substances in soil leached from treated timber in ser...
W Hettler, S Breyne, M Maier


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS
2000 - IRG/WP 00-20201
Beside the biological effectiveness the approval of a chemical wood preservative requires also techniques for the analytical determination of active ingredients in different matrices. Fulfilling of the last requirement is particularly difficult in the case of impregnated timber treated with wood preservatives containing organic compounds. This paper describes a procedure for the determination of t...
P Jüngel, J Wittenzellner, E Melcher


The fate of salt preservatives in facility yard soils and decontamination of soils and drainage waters
1993 - IRG/WP 93-50001-25
Extensive studies during the past 10 to 15 years revealed that noticeable amounts of preservative components may be released in the environment by dripping off or by rain prior to fixation unless adequate precautions are taken. Therefore, soil and groundwater contamination especially from chromium-VI compounds but also from other inorganic and organic constituents exist in impregnation plants, pos...
R-D Peek, H Klipp, K Brandt


Formation of polychlorinated dibenzo-p-dioxins (PCDD) and polychlorinated dibenzofurans (PCDF) during the combustion of impregnated wood
1995 - IRG/WP 95-50040-19
Wood waste and industrial wood residues often contain various preservatives. The waste management for these residuals can be recycling, deposition or combustion. Among the three possibilities, combustion seems to be the most efficient way of disposal. To obtain detailed information about emissions of organic compounds with environmental impact, especially polychlorinated dibenzo-p-dioxins (PCDD) a...
T Salthammer, H Klipp, R-D Peek


The quantitative determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using TD-GC-MS
2001 - IRG/WP 01-20223
Last year we presented the paper (IRG/WP/00-20201) "Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS". Based on the intensive discussion at the meeting, the first experiences made with the calibration of the system for this application will be reported. For the quantitative determination of N-cyclohexyl-diazeniumdioxide in treated wood, milled m...
P Jüngel, J Wittenzellner, E Melcher


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


Inorganic preservative levels in soil under treated wood decks after 8 years natural exposure in Borås, Sweden
2005 - IRG/WP 05-50233
Inorganic preservative components (Cu, Cr and As) were measured to a depth of 150 mm under deck structures made with Scots pine lumber treated with several different wood preservatives and installed in Borås Sweden 8 years ago. Higher contaminant levels were observed mainly under the drip lines and in the top 50 mm of soil. Under CCA treated decks, soil arsenic concentrations increased from ba...
P A Cooper, Y T Ung, M-L Edlund, J Jermer


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Evaluación de oxinato cúprico como alternativa al tribromofenato de sodio, para uso como funguicida antimancha. Ensayo final y conclusiones
2008 - IRG/WP 08-30481
This study evaluated the efficacy of oxine-copper (Cas Nº 10380-28-6. Synonyms: copper oxyquinolate, cupric-8-hydroxyquinolate, copper-8-quinolinolate) for the control of stain fungi in lumber. Three field tests were established and sodium tribromophenate was used as a reference preservative. Boards of Pinus elliotis and P. taeda were treated by dipping for 15, 30 or 60 seconds in two different f...
M Alba Valle


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Measurement of copper concentration in Cu-HDO treating solutions by handheld XRF
2022 - IRG/WP 22-20685
Copper based preservatives diluted in water dominate the wood preservative industry around the world. Periodically measurements and adjustments of the concentration of treating solutions must be performed as a part of the quality control at the treatment plant to achieve desired quality of the preservative treated wood. Many analytical methods are time consuming and must be performed under laborat...
P O Flaete