IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 47 documents. Displaying 25 entries per page.


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Cancer incidence among CCA exposed workers in the wood preserving industry
1995 - IRG/WP 95-50040-09
CCA wood preservatives - Copper, hexavalent, Chromium and tri-or pentavalent, Arsenic - has been used in the Nordic countries since mid 1930. Trivalent arsenic and hexavalent chromium compounds are toxic and cancerogenic while pentavalent arsenate and trivalent chromium are less hazardous. In impregnation, the compounds of CCA are fixed in the wood as insoluble trivalent chromium and copper pentav...
C-G Ohlson, A Andersen, F G Evans, S Karlehagen, K Nilsson


Creosote and cancer -Cancer incidence among workers exposed to creosote
1990 - IRG/WP 3572
Creosote is a wood preservative that contains polycyclic aromatic hydrocarbons, which are known to be carcinogenic. Cancer incidence among 919 male workers in Sweden and Norway exposed to creosote in the wood preserving industry was studied. The expected numbers of cases were based on the incidence rates of cancer according to the Cancer Registries of Sweden and Norway. A total of 129 cancer cases...
S Karlehagen, A Andersen, C-G Ohlson


Sub-group on Basidiomycete tests: Experimental programme and schedule of participants
1980 - IRG/WP 2145
The objectives of this IRG COLLABORATIVE BASIDIOMYCETE TEST are to compare results and assess reproducibility of a miniaturised wood block toxicity test when undertaken by different workers in different laboratories. The co-operative scientists and institutes are: Dr K Messner from Vienna (Austria); Dr R S Smith from Forintek (Canada); Mr J Hansen from Sadolins (Denmark); Mr B Jensen from Gori (De...
A F Bravery


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Evidence for Basidiomycete Tunnelling in Pinus radiata and Fagus sylvatica
2006 - IRG/WP 06-10587
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. Sites were selected to maximise occurrence of a diverse range of decay types. Presence of clamp connections in close associated with tunnelling coupled with macroscopic features similar to whi...
R Wakeling


Isolation and characterization of hydroxyl-radical-producing glycopeptide genes from the white-rot basidiomycete Phanerochaete chrysosporium
2006 - IRG/WP 06-10588
During wood decay, the white-rot basidiomycete Phanerochaete chrysosporium secretes low-molecular-weight glycopeptides that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radical. This reaction accounts for most of the hydroxyl radical produced in wood-degrading cultures of P. chrysosporium. In combination with phenol oxidases, hydroxyl radical is believed to play a r...
H Tanaka, G Yoshida, Y Baba, K Matsumura, S Itakura, A Enoki


Evaluation of natural durability of solid wood and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywood against Basidiomycete fungi
2008 - IRG/WP 08-10645
The aim of this research was to study the response of mixed plywoods composed of durable heartwood and non-durable sapwood to fungal attack. For this purpose, the species of Cupressus sempervirens (cypress) was chosen for its well-known durable heartwood. The evaluation of durability of plywood panels against fungi was done according to ENV 12038 and the fungi used were Coriolus versicolor (CV) an...
F Faraji, M F Thévenon, N Lemenager, B Thibaut


Termites y otros insectos xiliofagos en bienes arquitectonicos monumentos nacionalos de Colombia
2009 - IRG/WP 08-10679
The incidence of termites and other wood destroying insects was surveyed in ten historical buildings in Colombia. The most common insects were termites (Kalotermes, Cryptotermes, Heterotermes), although numerous decay organisms were also detected, including beetles (Anobium, Lyctus, Cerambycids) and various wood decaying fungi. Structural wood elements were classified according to the degree of a...
M G Ramírez


Analysis on dynamics of basidiomycetes in decayed wood by a method using non-specific amplification of DNA
2009 - IRG/WP 09-20426
A combination of non-specific amplification of DNA by Phi29 DNA polymerase and specific amplification of the internal transcribed spacer (ITS) region of ribosomal DNA (rDNA) by polymerase chain reaction (PCR) was applied to elucidate the ratio of basidiomycete species inhabiting decayed wood from an outdoor bench. After more than 8 hours incubation with Phi29 DNA polymerase, concentration of DNA ...
T Wada, K Igarashi, M Samejima


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


ISPM No. 15 and the Incidence of Wood Pests: Recent Findings, Policy Changes, and Current Knowledge Gaps
2011 - IRG/WP 11-30568
Largely as a result of international trade, hundreds of species of bark- and wood-infesting insects have become established in countries outside their native range. Many of these exotic insects have caused severe economic and environmental impact to urban and forest trees in the receiving countries. Most bark- and wood-infesting insects have been transported to new countries by means of the wood...
R A Haack, E G Brockerhoff


Laboratory study of toxicity or tolerance of CCA preservative and heavy metal constituents copper, chromium and arsenic to Malaysian tropical fungi
2011 - IRG/WP 11-30579
CCA preservative and its constituent heavy metal tolerance and toxicity to 3 Malaysian isolates Phialophora fastigiata (soft rot fungus), Paecilomyces variotii (mould fungus) and an unidentified white rot Basidiomycete, was investigated by the modified ‘Strange-Smith’ agar-well-plate technique with 1.6% CCA concentration and the malt-agar-plate bioassay technique with a range of CCA and consti...
A H H Wong, T Mark Venås, N Morsing, C C L Tan, P K F Chong


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


Degradation of Eucalyptus transmission poles varies across regions in Zambia
2018 - IRG/WP 18-30727
Evidence from literature shows that Eucalyptus poles treated with creosote last over 30 years before replacement. However, in Zambia, the life span of such poles has reduced to 5-10 years. The aim of this study was to investigate factors associated with degradation of treated Eucalyptus poles and how these varied across regions in the country. A total of 1200 poles were assessed in three differen...
P Ng’andwe, D Chungu, E Ncube


Biodiversity of wood-decaying fungi in French Guiana sequences of the small subunit (SSU) of ribosomal (r) DNA and the two primer pairs SR6/SR10R and SR7/SR1R
2019 - IRG/WP 19-10936
Fungi from tropical regions are currently under-represented in the classification system. Indeed, difficult access to tropical forests makes it complicated to study fungus species in such environments, unlike in European zones where fungal diversity and taxonomy are much better known. The purposes of this work were: a) to enhance classification by integrating new data that would bring out the impo...
C Zaremski, A Ducousso-Detrez, N Amusant, A Zaremski


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


Incidence of treated wood in a wood recycling facility in Western Oregon, USA: an update
2019 - IRG/WP 19-50346
Preservative treated wood provides excellent long-term performance under a variety of adverse conditions, but it must eventually be replaced. The US Environmental Protection Agency recommends reuse in a similar application, but if that is not an option, disposal in a municipal solid waste facility equipped with a leachate management system. Concerns about diminishing landfill capacity have led m...
J J Morrell


Previous Page