Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


Water-repellent additive for CCA
1991 - IRG/WP 3655
Hickson have developed a water repellent additive for incorporation into copper-chromium-arsenate timber treatment solutions. The water repellent emulsion shows good stability in the treatment solution, is easily incorporated and applied in a single stage treatment. No modifications to the additive is safe to treatment schedule are usually needed and use. Weathering of the treated wood is substant...
P Warburton, R F Fox, J A Cornfield


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


A comparative field test of the effectiveness of anti-sapstain treatments on radiata pine roundwood
1986 - IRG/WP 3376
Peeled radiata pine posts were sprayed with one of six antisapstain formulations, with and without a wax water-repellent additive, to evaluate the protection given by each treatment. After 3 months' outside storage the best treatments tested were 4% product Busan 30, 2% product Busan 1009, and 2% active sodium pentachlorophenoxide (NaPCP) with 1.5% borax. After 6 months' storage ...
J A Drysdale, R M Keirle


Studies on the biological improvement of permeability in New Zealand grown Douglas fir
1983 - IRG/WP 3231
This report outlines progress towards optimizing conditions for water storage of New Zealand grown Douglas fir with the aim of improving permeability to water-borne preservatives, in particular CCA. Small scale laboratory tests are in progress but the need to scale up to potential commercial applications is being considered. Mixed populations of bacteria isolated from 10 week water sprinkled Dougl...
K J Archer


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


Computerised data acquisitioning, handling and processing in wood preservation studies
1984 - IRG/WP 2218
The computerisation of data acquisitioning, handling and processing in weathering studies on wood treated with protective coatings is discussed. An integrated system comprising a data base, statistical package and a custom written graphical processor is explained. Two treatments are compared and the correctness of a mathematical weathering model is evaluated....
T Rypstra, K Vos


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan