Your search resulted in 166 documents. Displaying 25 entries per page.
Functionalization of wood with nano-sized titanium dioxide – Efficacy against mould growth and effect on cell wall integrity
2025 - IRG/WP 25-20740
Nano-sized titanium dioxide (nano TiO2) is a photocatalytic compound that generates reactive radicals under UV radiation, which can inhibit microbial growth and impart self-cleaning properties. This effect has been widely utilised on materials such as glass or tiles. This study investigates the potential of nano TiO2 treatments to prevent mould growth on wood and their impact on cell wall integrit...
U Hundhausen, S Bollmus, L Ross
Citric acid/urea derivatives as an anti-discolouration treatment for wood surfaces
2025 - IRG/WP 25-20741
The exterior-use wood faces raining and sunlight exposure, which can cause property changes of the wood, such as the discolouration, dimensional instability, and biological attack. This article explores the use of citric acid and urea as surface protection of wood. The heating of citric acid and urea can result in the fluorescent carbon dots. These carbon dots can absorb UV light with the emission...
C-F Lin, O Myronycheva, D Jones, O Karlsson
Are we barking up the right tree? - the use of bark residues in wood protection
2025 - IRG/WP 25-20742
Tree bark, a lignocellulosic side-stream, is typically underutilised, often combusted or landfilled, thus contributing to greenhouse gas emissions. This communication paper explores the potential of bark residues, particularly suberinic acid, tannins and other polyphenols, in wood protection applications, including coatings, adhesives, and fire retardants. Several European projects have been initi...
A Treu, M Altgen, M Sipponen, M Borrega
CIOL Wood - Scientific Innovations in Wood Modification for Enhanced Performance and Usage
2025 - IRG/WP 25-20743
CIOL® is a wood modification technology designed as an environmentally friendly alternative to traditional wood preservatives. Utilising a biobased formulation based on sorbitol and citric acid, CIOL® enhances wood's chemical structure, improving its durability, stability, and resistance to decay. This paper provides an overview of the advancements made in CIOL® technology, including its improv...
E Larnøy, A Treu, M Diraison, M Smith, A Audouin, P T Lewandowski, J Biørnstad
A novel anti-fungal wood crack repairing agent based on CQDs/PVA
2025 - IRG/WP 25-20744
Wood is a sustainable material, but its tendency to crack and decay poses a challenge for its applications. In this study, we developed a combination system of nitrogen-doping carbon quantum dots (N-CQDs) and polyvinyl alcohol (PVA) to repair wood cracks. Rather than employing the conventional repairing methods such as filling cracks with sawdust and petroleum based-adhesives, this technique can m...
X Zhao, Z Zhang, Y Peng, W Wang, J Cao
Transmission poles - Analysis of causes of premature failure in Slovenia
2025 - IRG/WP 25-20745
The study focuses on analysing the causes of the premature collapse of wooden transmission poles in Slovenia, where there have been several cases of rapid fungal decomposition of poles despite the planned lifespan of 30 to 50 years. The poles were made of Scots pine wood and impregnated with a copper-ethanolamine wood preservative. The research aimed to assess the condition of standing poles and e...
M Humar, B Lesar, N Kregar, S Drnovšek
Evaluation of 'Deep Penetration Treatment' for wood preservation
2025 - IRG/WP 25-20746
‘Deep Penetration Treatment’ (DPT) is a recently developed wood preservation technique in Japan designed to meet the preservation standards required for residential foundations. This method involves spraying a specially formulated solvent-borne wood preservative onto properly incised dried lumber. Despite being a non-pressure treatment, DPT achieves penetration levels comparable to conventiona...
M Ikeda, T Shigeyama, Y Sugai
Hot and cold treatment with ACQ
2025 - IRG/WP 25-20747
Wood deterioration poses a significant challenge in tropical and sub-tropical developing countries, leading to premature structural failure and economic losses. While preservative treatment offers a solution, the high cost of commercial vacuum pressure systems often hinders its widespread adoption. Lower-technology alternatives, like the hot and cold bath method, present a more affordable option f...
J Norton
Wood phytosanitation: which Standard should be applied?
2025 - IRG/WP 25-20748
The international Standards ISPM 15 and ISPM 39 are both essential tools for safeguarding global plant health, but they serve different purposes, and apply to different aspects of international trade. ISPM 15 focuses on wood packaging material and mandates Standardised treatments and marking, while ISPM 39 addresses international movement of wood and emphasises risk assessment and tailored phytosa...
L Robertson, S Santos, M T Troya
Influence of incising methods and wood moisture content on ‘deep penetration treatment’ in Japanese cedar and larch
2025 - IRG/WP 25-20749
To expand applicability of ‘deep penetration treatment’, a solvent-borne and non-pressure treatment that is commonly coupled with roller-type incising using a flat blade, we investigated drill and laser machining as alternative incising methods and examined the influence of wood moisture content on the preservative penetration. Various incising methods were applied to heartwood of Japanese ced...
S Taira, T Miyauchi, S Isaji, H Matsunaga
NTR classified preservative-treated laminated wood
2025 - IRG/WP 25-20750
NTR is a trusted quality labelling system used for the classification and quality control of wood products that have been treated with preservatives or modified. These labels are issued by the Nordic Wood Preservation Council (NWPC) and in recent years, producers of glued laminated timber as well as building material suppliers have shown increasing interest in NTR classification for glued laminate...
J Jermer, F Westin, R Digaitis
The iTrussT project – Advancements in timber bridge design, preservation, and monitoring
2025 - IRG/WP 25-20751
The Norwegian research project iTrussT (2025–2028) aims to advance timber bridge design and unlock wood’s full potential as a sustainable solution for modern infrastructure. It addresses three critical challenges: First, fatigue testing of glued laminated timber lamellae will provide deeper insights into shear failure mechanisms, supporting the development of safer, more efficient structures a...
K-C Mahnert, U Hundhausen
Durability Analysis of Bio-based Phenol-Formaldehyde Resin-Treated Wood
2025 - IRG/WP 25-20753
The aim of this study is to explore the application of bio-based materials in outdoor construction. Enhancing the durability of wood products effectively extends their carbon storage lifespan, making it essential to investigate their long-term durability. The study used commercial resin (CPF) and laboratory-synthesised petro-based phenolic resin (LPF) as control groups. Japanese cedar specimens we...
T-H Lin, P-Y Kuo
Carbon quantum dots as a fungicide and its applications in wood
2025 - IRG/WP 25-20754
In this work, we synthesised nitrogen-doped carbon quantum dots (CQDs) via a microwave assisted method. CQDs with proper structure showed excellent anti-fungal effects against both brown (Postia placenta, Pp) and white rot decay fungi (Trametes versicolor, Tv) on wood. The underlying anti-fungal mechanisms of CQDs on wood were further elucidated. We found that positively charged nano-sized CQDs pr...
X Zhao, Z Zhang, M Zhou, J Cao
Investigation of a commercial fire-retardant additive on particleboard properties
2025 - IRG/WP 25-20755
Fire resistance of wood-based panels is in addition to mechanical and sorption properties, an important property when considering its usability for construction applications. Increased fire resistance is achieved through fire retardant addition during panel production or by spraying fire-retardant on already finished panel. A potential downside of fire-retardant addition during panel production ca...
D Jones, S Medved, M Lawther
Sustainable and environmentally friendly bio-based protection against fire
2025 - IRG/WP 25-20756
Flame-retardant agents are used to confer fire resistant properties with effects strongly dependent on their ability to form char during the thermal degradation. The char coats the polymeric materials and provides a good barrier against heat and oxygen diffusion, thus reducing the combustion rate of the polymeric materials. Halogenated agents that are used today are toxic and may cause severe heal...
M Tanase-Opedal, A Larsson, P O Flaete
Predicting weather resistance of Recoated Outdoor Wood by Near Infrared Diffuse Reflectance Spectroscopy
2025 - IRG/WP 25-20757
Wood exposed to the outdoors causes slow degradation. One wood treatment to retain this degradation is paints and stains, and recoating is essential process for these coated wood products to achieve a long service life. We investigated that possibility of using near infrared spectroscopy to estimate repair condition and weather resistance of recoated outdoor wood. The specimens used for recoating ...
M Murai, M Itani, K Isoda
Curing Behaviour of Bio-based Phenol Formaldehyde Resin and the Durability Performance of Treated Wood
2025 - IRG/WP 25-20758
The aim of the study is to investigate the curing behaviours of bio-based PF resins treated Japanese Cedar (Cryptomeria japonica). Compared to conventional wood preservatives such as metal-based ACQ, bio-based PF resin was more environmentally-friendly and can store more plant-based carbon inside treated wood. However, all these preservatives have the risk of being leached out. This study conducte...
Y-S Lee, P-Y Kuo
Enhancing the Effectiveness of Penflufen by using a Plant Booster
2025 - IRG/WP 25-20759
Penflufen (Preventol® A 800) is a modern pyrazole fungicide which has been approved by the US EPA for the use in wood protection in 2018. Penflufen is an inhibitor of the succinate dehydrogenase (SDHI). It is highly efficient against wood decaying basidiomycetes fungi. In the European standard efficacy test EN 113/ EN 84, penflufen is controlling both brown rot and white rot fungi at the low rete...
D Messaoudi, A Robert, P Meckler, T Jaetsch
The Impact of Drying Techniques on the Quality of Thermally Modified Wood
2025 - IRG/WP 25-30813
The wood drying technique applied before loading the dry wood into the ThermoWood® kiln may affect its properties. For this purpose, Scots pine (Pinus sylvestris) boards were first dried through three drying methods, including radio-frequency/vacuum (RF/V), mild, and moderate conventional drying, and then loaded into a ThermoWood® kiln for thermal modification at 212 °C for 3 hours according to...
M Ghorbanian Far, N Sharifi, A Nikoutadbir, A Tarmian, M Humar
The non-energy utilization of low-quality wood from the invasive species Prunus serotina
2025 - IRG/WP 25-30814
Alien invasive species in Europe, such as Prunus serotina, can significantly impact ecosystem structure and function. This species provides low-quality timber, which is most often used for energy purposes in the form of biomass. In the era of policies focused on a circular economy, seeking methods to extend the life cycle of raw materials and wood products is necessary. For this purpose, the wood ...
W Perdoch, P Kołwzan
Decay resistance of thermally modified Eucalyptus grandis in closed and open systems
2025 - IRG/WP 25-30815
Thermal modification has been successfully used to improve the durability of Eucalyptus wood from fast-growing forests. Although it is the most common type of modification process, there are some fields for studies on thermally modified wood, particularly about the comparison between processes in closed and open systems. This work aimed to analyse the effect of thermal modification in closed and o...
D C Batista, A C Oliveira Rupf, M Wentzel, C Brischke, H Militz
Chestnut tannin-furfurylic resins for wood preservation: influence of the proportion of tannins as a copolymer
2025 - IRG/WP 25-30816
Tannin, which is present in all plants, is the most abundant polyphenol globally and can be extracted using water or organic solvents such as acetone, ethanol and methanol. Tannins are classified into two categories: condensed tannins (catechin-based polymers) and hydrolysable tannins (sugar esters with galloyl units). Previous studies have demonstrated its potential as a raw material for modifyin...
J V Dorini-Falavinha, C Gerardin-Charbonnier, P Cademartori
Novel treatments of solid wood - studies into the use of imidazole and succinimide
2025 - IRG/WP 25-30817
Recent activities have focussed on the use of ionic liquids (ILs) in wood treatments and bioprocessing. Most ILs are based on imidazolium systems, so it was decided to investigate the potential of imidazole as a treatment, along with another heterocyclic compound, namely succinimide. Thus, modification of Scots pine sapwood (Pinus sylvestris L.) with heterocyclic compounds, imidazole and succinimi...
D Jones, A Scharf, H Dernegård, J Oja, S Duarte, J Levanić, M Humar
Enhanced Termite Resistance of Low Durability Fast Growing Teak Wood by Non-Biocide Treatments Based on Chemical and Thermal Modification
2025 - IRG/WP 25-30818
Short rotation teak as a fast-growing tree can be considered as a renewable material resource for the future green economy. However, short rotation teak wood is susceptible to biodeterioration, particularly to termite attack. The objective of this work was to investigate the effect of chemical and thermal treatment on resistance of sapwood, transition wood, and heartwood of short rotation teak aga...
R Martha, K Candelier, M-F Thévenon, B George, I S Rahayu, W Darmawan, P Gérardin