Your search resulted in 1429 documents. Displaying 25 entries per page.
The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet
Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling
Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik
Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman
Multicomponent biocide systems protect wood from decay fungi, mold fungi, and termites for interior applications
2004 - IRG/WP 04-30333
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of proper moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under condit...
C A Clausen,V W Yang
Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens
Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel
An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong
Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden
Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke
Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh
European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use
are waited to valid the progra...
Anonymous
Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher
Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn
Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods
Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong
Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka
Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner
Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial
Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce
Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross
Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner
Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy
Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig
Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...