IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1082 documents. Displaying 25 entries per page.


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


Physical and biological properties of albizzia waferboards modified with cross-linking agents
1995 - IRG/WP 95-40043
Chemically-modified low-density waferboards with cross-linking agents were produced using a fast-growing species of hardwood albizzia (Paraserienthes falcata Becker) as a raw materials and isocyanate resin as a glue adhesive. For the chemical modification, the vapor-phase formalization of the boards and the pad-dry-cure treatment of wafers with cross-linking agents were employed. The vapor-phase f...
S Yusuf, Y Imamura, M Takahashi, K Minato


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


The antifungal efficacy of Guayule resin
1987 - IRG/WP 3429
The Naval Research Laboratory is evaluating the non-rubber-producing portion of guayule (Parthenium argentatum) resin as a protectant for wood in terrestrial and marine service. This study phase, in collaboration with the universities of Arizona and Mississippi State, evaluates the resin's fungicidal worth. Resin-impregnated pine sapwood was exposed to brown rot fungi (Gloeophyllum trabeu...
J D Bultman, R L Gilbertson, T L Amburgey, J E Adaskaveg, S V Parikh, C A Bailey


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Silicic acid-Boric acid complexes as wood preservatives
2001 - IRG/WP 01-30273
A silicic acid monomer aqueous solution (SAMS) or colloidal silicic acid solution (CSAS) was combined with various metal compounds or boric acid. Agents where SAMS or CSAS was combined with boric acid gave good protection against decay caused by the brown-rot fungus Fomitopsis palustris, the treated wood (Cryptomera japonica D. Don) specimens after the leaching test maintained a high resistance to...
H Yamaguchi


Antagonistic properties of Gliocladium virens against wood attacking fungi
1996 - IRG/WP 96-10162
Gliocladium virens has shown good antagonism against decay fungi in agar medium and in wood blocks. Gliotoxin produced by Gliocladium virens is associated with biocontrol of some plant diseases, but its importance to biocontrol of wood-attacking fungi is unknown. We investigated the ability of gliotoxin-producing (GLT+) isolates of Gliocladium virens and gliotoxin-deficient (GLT-) mutants of Glioc...
T L Highley, H S Ananthapadmanabha, C R Howell


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


Collaborative soft rot tests. Names and addresses of collaborators
1973 - IRG/WP 231
IRG Secretariat


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


Current techniques for screening initial formulations against Basidiomycetes and soft rot
1978 - IRG/WP 2103
J D Thornton, H Greaves


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


The dry rot fungus and other fungi in houses. Part 2
1993 - IRG/WP 93-10001
J Bech-Andersen


Some characteristics of Pinus radiata wood from trees subjected to resin extraction
1987 - IRG/WP 3403
35 year old Pinus radiata trees growing in La Puntilla (lat. 37° south, long. 72,4° west), Chile, were subjected to resin extraction 5 years ago. After harvesting them simultaneously with control trees of the same place and age, probes were taken from the bottom of each pole, at 3.4 m, 7.8 m and 11.4 m height. Analysis of ethanol/benzene extract, CCA salt penetration tests and sapstain and brown-rot development rate were performed. The extract content differed in both groups. In the ascendent sense it decreases in unextracted trees and increases in extracted. CCA salt penetration was deeper in treated trees than in untreated. Wood subjectect to resin extraction was less susceptible to sapstain development. No significant difference was detected in both groups in relation to the development of brown-rot.
M C Rose, J Navarrete, G Sandoval, A Bedoya, L Ortega, R Zurita