Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Immunogold labelling of size marker proteins in brown rot-degraded pine wood
1990 - IRG/WP 1428
Pine wood degraded by Fomitopsis pinicola was infiltrated with a mixture of ovalbumin (45 kDa) and myoglobin (16.7 kDa). After crosslinking of the proteins with glutaraldehyde and preparation for electron microscopy ultrathin sections were labeled with gold-conjugated antibodies. Simultaneous labeling of both proteins on the same section showed that at 50-70% weight loss ovalbumin did not penetrat...
E Srebotnik, K Messner


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Defining fungal decay types - Final proposal
1988 - IRG/WP 1355
The term soft rot is proposed for all forms of decay caused by Ascomycetes and non-basidiomyceteous Fungi imperfecti. The terms brown rot and white rot should be used only for decay caused by Basidiomycetes. Brown rot is characterized by extensive depolymerization of the cellulose and limited lignin degradation. White rot is characterised by significant degradation of the lignin component in wood....
T Nilsson


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Microbial breakdown mechanisms. Mini-Symposium at the 18th IRG meeting, Honey Harbour, Ontario, Canada
1987 - IRG/WP 1327
An understanding of how micro-organisms cause chemical alternation to wood is essential for effective wood preservation. Investigation of the Microbial Breakdown of wood is a very dynamic research field and is increasing in importance as several biocides are being examined as alternativesw to classic wood preservatives. These biocides often do not possess broad spectrum activity. It is esential th...
L E Leightley


Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki


Micromorphology of oak wood degraded by brown rot fungus Coniophora puteana
2000 - IRG/WP 00-10356
To characterize the degradation of hardwood by brown rot fungus, Coniophora puteana was incubated on the wood blocks of Quercus accutissima. For comparison, the same fungus was also incubated on the pine wood blocks of Pinus densiflora. In softwood, the shape of the wood cells and thickness of the cell appeared unchanged even the loss of birefringence in the affected areas. In contrast, oak wood d...
Yoon Soo Kim, Seung-Gon Wi, Kwang-Ho Lee


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


Extracellular laccase production in brown-rot fungus Coniophora puteana
2001 - IRG/WP 01-10391
Coniophora puteana, one of representing brown-rot fungus, was investigated in terms of extracellular ligninolytic enzyme production. Three fungal strains of C. puteana were inoculated in liquid culture medium with sawdust of pine and oak wood. Extracellular laccase production was observed in some strains of C. puteana in the culture medium with sawdust of oak wood. The highest activity occurred at...
Kwang-Ho Lee, Seung-Gon Wi, Yoon Soo Kim


Fungal Attack on Lignin and Cellulose: Elucidation of Brown- and White-Rot Mechanisms Comparing Biomimetic and In-Vivo Degradation Patterns
2010 - IRG/WP 10-10714
This paper examines research and hypotheses that have been developed over several years on wood degradation mechanisms. This information is combined with new data and analyses to explain why wood decay patterns caused by brown-rot fungi and specific types of white-rot fungi are different. New data, including work with both biomimetic studies on low molecular weight compounds, degradative enzymes, ...
V Arantes, B Goodell, A M F Milagres, Yuhui Qian, T Filley, J Jellison, S Kelley


Non-stochiometric oxidation and ROS generation promoted by guaiacol lignin structures and lignocelluose surfaces may be a component of brown rot fungal degradation mechanisms
2019 - IRG/WP 19-10937
Model guaiacol compounds representing lignin monomers, as well as DHP-lignin and wood flour of controlled particle size were used to assess iron reduction at the pH of the natural wood cell wall. All compounds functioned as electron donors for ferric iron, with the lignin monomers demonstrating capacity for non-stochiometric reduction of iron with multiple moles of ferric ion reduced per mole of l...
Y Tamarua, M Yoshidaa, L D Eltisb, B Goodell


FTIR analysis of wood blocks decayed by brown-rot fungi
2020 - IRG/WP 20-10959
Calibration curves of the relative lignin contents in Cryptomeria japonica decayed by brown-rot fungi were developed with Infrared Spectroscopy and Klason technique. First, wood decay test was conducted using brown-rot fungi (Fomitopsis palusris, F. pinicola, Wolfiporia cocos, Gloeophyllum trabeum, and Neolentinus suffrutescens) and white-rot fungus (Trametes versicolor) was used as a comparison. ...
R Kondo, Y Horikawa, R Kose, M Yoshida


The iron reduction by chemical components of wood blocks decayed by wood rotting fungi
2021 - IRG/WP 21-10979
Brown-rot fungi, a group of wood rotting fungi, is well known to be one of major microorganisms that cause the deterioration of wooden buildings in Japan and have been considered to use chelator-mediated Fenton (CMF) reaction in concert with hydrolytic and redox enzymes for degradation of wood cell wall. CMF can be described as a non-enzymatic degradation system that utilizes hydroxyl radicals pro...
R R Kondo, Y Horikawa, K Ando, B Goodell, M Yoshida


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


Effect of medium-term degradation of beech wood by erosive (Phanerochaete chrysosporium) and lignin-selective (Ceriporiopsis subvermispora) strains of white rot fungi on its selected physical properties
2004 - IRG/WP 04-40292
At the Faculty of Wood Sciences and Technology a fungal delignification of normal and tension beech wood by erosive and lignin-selective strains white-rot fungi has been studied. The pre-treatment of both kind of wood samples was accompanied by partial delignification and apparent changes of their physical properties influencing the polar liquids penetration....
R Solár, S Kurjatko, M Mamonová, J Hudec


A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


Next Page