Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Molecular analysis of the basidiomycete Coniophora puteana
1992 - IRG/WP 92-1534
Sodium dodecylsulphate polyacrylamide gel electrophoresis and Western Blotting, using a polyclonal antiserum produced against a whole cell extract of Coniophora puteana, were used to analyse the major proteins and antigens of the wet rot organism Coniophora puteana. The macromolecule profiles of this organism were different from other members of the Coniophora genus and from a set of unrelated org...
H E McDowell, D Button, J W Palfreyman


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Evaluation of natural durability of solid wood and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywood against Basidiomycete fungi
2008 - IRG/WP 08-10645
The aim of this research was to study the response of mixed plywoods composed of durable heartwood and non-durable sapwood to fungal attack. For this purpose, the species of Cupressus sempervirens (cypress) was chosen for its well-known durable heartwood. The evaluation of durability of plywood panels against fungi was done according to ENV 12038 and the fungi used were Coriolus versicolor (CV) an...
F Faraji, M F Thévenon, N Lemenager, B Thibaut


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Laboratory study of toxicity or tolerance of CCA preservative and heavy metal constituents copper, chromium and arsenic to Malaysian tropical fungi
2011 - IRG/WP 11-30579
CCA preservative and its constituent heavy metal tolerance and toxicity to 3 Malaysian isolates Phialophora fastigiata (soft rot fungus), Paecilomyces variotii (mould fungus) and an unidentified white rot Basidiomycete, was investigated by the modified ‘Strange-Smith’ agar-well-plate technique with 1.6% CCA concentration and the malt-agar-plate bioassay technique with a range of CCA and consti...
A H H Wong, T Mark Venås, N Morsing, C C L Tan, P K F Chong


Biodiversity of wood-decaying fungi in French Guiana sequences of the small subunit (SSU) of ribosomal (r) DNA and the two primer pairs SR6/SR10R and SR7/SR1R
2019 - IRG/WP 19-10936
Fungi from tropical regions are currently under-represented in the classification system. Indeed, difficult access to tropical forests makes it complicated to study fungus species in such environments, unlike in European zones where fungal diversity and taxonomy are much better known. The purposes of this work were: a) to enhance classification by integrating new data that would bring out the impo...
C Zaremski, A Ducousso-Detrez, N Amusant, A Zaremski


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


Which fungi cause sapstain in Canadian softwoods?
1998 - IRG/WP 98-10285
The Canadian forest products industry suffers considerable losses in revenue due to fungal stains. There is an increased awareness that more complete knowledge about the causal organisms might help solve the problem. A first step was to initiate a thorough survey of bluestain fungi in Canada. Systematic sampling was done at seven selected sawmills in six Canadian provinces. In summer 1997 fresh lo...
A Uzunovic, Dian-Qing Yang, P Gagné, C Breuil, L Bernier, A Byrne


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Preliminary study of the fungicidal and structural variability in copper naphthenates and naphthenic acids
1996 - IRG/WP 96-30114
Copper naphthenates, an oil-borne wood preservative listed by the American Wood-Preservers' Association (AWPA), is manufactured by complexing copper(II) with naphthenic acids. Prior to AWPA listing as a wood preservative, field experiments showed that copper naphthenates generally had good stability and were active against wood-destroying organisms. Recently, however, there have been reports ...
T Schultz, D D Nicholas, L L Ingram Jr, T H Fisher


The effect of certain wood extractives on the growth of marine micro-organisms
1977 - IRG/WP 438
S E J Furtado, E B G Jones, J D Bultman


Inhibition of wood-inhabiting fungi by actinomycetes
1981 - IRG/WP 1137
Actinomycetes of the genera Streptomyces, Micromonospora, Microtetraspora, Nocardia and Rhodococcus, isolated from wood, were laboratory tested for their inhibitory effects against the Basidiomycete fungi Polystictus sanguineus and Sistrotrema brinkmannii. One-third of the representatives of the genus Streptomyces which were tested produced significant inhibitory zones whereas actinomycetes belong...
M S Cavalcante, R A Eaton


Comité International Permanent pour la Recherche sur la Préservation des Matériaux en Milieu Marin. Information from the Wood Group
1980 - IRG/WP 460
E G B Jones


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


The restricted distribution of Serpula lacrymans in Australian buildings
1989 - IRG/WP 1382
Temperature data has been gathered over a number of years, not only for flooring regions of various buildings in Melbourne, but also within roof spaces and external to the buildings. Findings are discussed in relation to the distribution of Serpula lacrymans within Australia, its restriction to certain types of building construction and its restriction to flooring regions. The subfloor spaces of b...
J D Thornton


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....