IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 177 documents. Displaying 25 entries per page.


Efficacies of an insecticide and a fungicide for preventing blue-stain of Japanese red pine logs
2006 - IRG/WP 06-20329
We examined blue-stain fungi on Japanese red pine at 3 forests and 2 saw mills in Iwate Prefecture, Japan. The isolated ophiostomatoid fungi were Leptographium sp and Ophiostoma sp. There were 3 routes of the blue-stain; fungal growth from the spore or hypha stuck on the cross cut surfaces, fungal spread through the inner bark by bark beetles and fungal invasion around whorled knot. The larger ext...
H Taniuchi, T Koiwa, H Masuya, S Doi


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


The efficacy of commercial silicones against blue stain and mould fungi in wood
2008 - IRG/WP 08-30471
Scots pine (Pinus sylvestris L.) wood samples were vacuum pressure impregnated with quatsilicone micro emulsion (<40 nm particle size), aminosilicone macro emulsion (110 nm) and silicone macro emulsion with alkyl modified side groups (740 nm) and the resulting material properties were studied. Quatsilicone micro emulsion resulted in maximum bulking (4.8%) and anti-swelling efficiency (21.8%) in...
S C Ghosh, C Mai, H Militz


Control biológico de la mancha azul en madera aserrada de Pinus radiata D. Don.
2008 - IRG/WP 08-10681
Radiata pine wood is highly susceptible to the attack of sapstaining fungi promoting a discoloration which results in important economical losses. The use of chemicals, a customary procedure to prevent its occurrence is becoming nowadays, due to environmental concern, a more questionable practice. The biological control of blue stain fungi with albino isolates of the Ophiostoma genera appear to ...
J Navarrete, A Segura, P Martínez, R Vera, C Segovia, P Herrera, L Reyes, D McNew, T C Harrington, R L Farrell, J M Thwaites, B Held, R A Blanchette


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Use of wax emulsions for upgrading of wood properties
2009 - IRG/WP 09-40451
Waxes are used for treatment of wood surfaces for several decades, predominately as surface treatments, because they did not penetrate into the wood. In order to overcome this issue, water emulsions were applied in present experiment. Five water emulsions of various concentration was used namely; two emulsions of montan wax (LGE, MW1), emulsion of polyethylene (WE1), emulsion of ethylene copolymer...
B Lesar, F Pohleven, M Humar


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Plasma-assisted bleaching of blue-stain from lodgepole pine wood
2017 - IRG/WP 17-40799
We hypothesize that plasma will etch wood and fungal hyphae in blue-stained lodgepole pine, and increase the ability of hypochlorite bleach to remove discolouration from blue-stained wood. Blue-stained lodgepole pine wood was exposed to a glow-discharge plasma derived from water, and the surface wettability, permeability and colour of the treated wood was measured. Plasma-treated wood was dipped i...
A Jamali, P D Evans